# US 2026/0250919 A1 · Guard rail beam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250919 A1
- Document ID: US20260250919A1
- Status: Published application
- Kind: A1
- Application number: 18/870,647
- Filed: 2023-04-06
- Published: 2026-08-27
- Earliest claimed: 2022-06-30
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Shin UENO; Hiromasa SHOJI; Akinobu KOBAYASHI; Satoru YAMASHITA
- Web page: https://patentgrep.com/patent/US20260250919A1

## CPC

- C23C 2/06: Zinc or cadmium or alloys based thereon
- E01F 15/0423: {Details of rails (E01F15/0415 takes precedence)}
- B23D 35/001: {cutting members}
- C22C 18/04: with aluminium as the next major constituent
- C23C 2/14: Removing excess of molten coatings; Controlling or regulating the coating thickness
- C23C 2/16: using fluids under pressure, e.g. air knives
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- E01F 15/04: essentially made of longitudinal beams or rigid strips {supported above ground at spaced points (E01F15/10, E01F15/12 take precedence)}
- E01F 15/0407: {Metal rails (E01F15/0446 and E01F15/0453 take precedence)}
- B23D 19/04: having rotary shearing discs arranged in co-operating pairs
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- E01F: ADDITIONAL WORK, SUCH AS EQUIPPING ROADS OR THE CONSTRUCTION OF PLATFORMS, HELICOPTER LANDING STAGES, SIGNS, SNOW FENCES, OR THE LIKE
- B23D: PLANING; SLOTTING; SHEARING; BROACHING; SAWING; FILING; SCRAPING; LIKE OPERATIONS FOR WORKING METAL BY REMOVING MATERIAL, NOT OTHERWISE PROVIDED FOR (making toothed gears or the like B23F; cutting metal by applying heat locally B23K; arrangements for copying or controlling B23Q)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a guard rail beam comprised of a coated steel material comprising a steel material and coating layer formed on both surfaces of the steel material and made of a Zn-based coating, wherein at least one edge face of the steel material is covered by the coating layer and satisfies 0.60×tc≤te<tc, We≥Wc, and Wt≥Wc (tc is an average sheet thickness (mm) of the steel material at a position inside from the edge face covered by the coating layer by 10 mm or more, the is an average sheet thickness (mm) of the steel material at a position of 1 to 10 mm from the edge face covered by the coating layer, We is an average thickness (μm) per surface of the coating layer at a position of 1 to 10 mm from the edge face covered by the coating layer, Wc is an average thickness (μm) per surface of the coating layer at a position inside from the edge face covered by the coating layer by 10 mm or more, and Wt is an average thickness (μm) of the coating layer at the edge face covered by the coating layer).

## Claims

### Claim 1

A guard rail beam comprised of a coated steel material comprising a steel material and coating layer formed on both surfaces of the steel material and made of a Zn-based coating, wherein
at least one edge face of the steel material is covered by the coating layer and satisfies following Formulas 1 to 3:
0.6
×
tc
≤
te
<
tc
Formula
⁢
1
We
≥
Wc
Formula
⁢
2
Wt
≥
Wc
Formula
⁢
3
where
tc is an average sheet thickness (mm) of the steel material at a position inside from the edge face covered by the coating layer by 10 mm or more,
te is an average sheet thickness (mm) of the steel material at a position of 1 to 10 mm from the edge face covered by the coating layer,
We is an average thickness (μm) per surface of the coating layer at a position of 1 to 10 mm from the edge face covered by the coating layer,
Wc is an average thickness (μm) per surface of the coating layer at a position inside from the edge face covered by the coating layer by 10 mm or more, and
Wt is an average thickness (μm) of the coating layer at the edge face covered by the coating layer.

### Claim 2 (depends on 1)

The guard rail beam according to claim 1, wherein the coating layer is a Zn—Al—Mg-based coating.

### Claim 3 (depends on 2)

The guard rail beam according to claim 2, wherein the coating layer has a chemical composition comprising, by mass %,
Al: more than 15.0 to 30.0%,
Mg: more than 5.0 to 15.0%,
Sn: 0 to 0.70%,
Ca: 0 to 0.60%,
Si: 0 to 0.75%,
Ti: 0 to 0.25%,
Ni: 0 to 1.00%,
Co: 0 to 0.25%,
Fe: 0 to 5.0%,
B: 0 to 0.50%, and
balance: Zn and impurities.

### Claim 4 (depends on 1)

The guard rail beam according to claim 1, arranged so that the edge face covered by the coating layer faces upward relative to a ground surface.

### Claim 5 (depends on 1)

The guard rail beam according to claim 1, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 6 (depends on 1)

The guard rail beam according to claim 1, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction and a fractured surface or has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction, a sheared surface, and a fractured surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the slanted surface and the sheared surface are a total of 50 area % or more.

### Claim 7 (depends on 1)

The guard rail beam according to claim 1, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has
a first slanted surface slanted from a first surface toward a center part of the steel material relative to a sheet thickness direction,
a second slanted surface slanted from a second surface toward a center part of the steel material relative to a sheet thickness direction, and
a fractured surface formed between the first slanted surface and the second slanted surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the first slanted surface and the second slanted surface are a total of 50 area % or more.

### Claim 8 (depends on 2)

The guard rail beam according to claim 2, arranged so that the edge face covered by the coating layer faces upward relative to a ground surface.

### Claim 9 (depends on 3)

The guard rail beam according to claim 3, arranged so that the edge face covered by the coating layer faces upward relative to a ground surface.

### Claim 10 (depends on 2)

The guard rail beam according to claim 2, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 11 (depends on 3)

The guard rail beam according to claim 3, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 12 (depends on 4)

The guard rail beam according to claim 4, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 13 (depends on 5)

The guard rail beam according to claim 5, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 14 (depends on 6)

The guard rail beam according to claim 6, wherein a coating coverage rate up to a position of 10 mm from the edge face covered by the coating layer is 90 area % or more.

### Claim 15 (depends on 2)

The guard rail beam according to claim 2, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction and a fractured surface or has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction, a sheared surface, and a fractured surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the slanted surface and the sheared surface are a total of 50 area % or more.

### Claim 16 (depends on 3)

The guard rail beam according to claim 3, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction and a fractured surface or has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction, a sheared surface, and a fractured surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the slanted surface and the sheared surface are a total of 50 area % or more.

### Claim 17 (depends on 4)

The guard rail beam according to claim 4, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction and a fractured surface or has a slanted surface slanted from a first surface toward a second surface of the steel material relative to a sheet thickness direction, a sheared surface, and a fractured surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the slanted surface and the sheared surface are a total of 50 area % or more.

### Claim 18 (depends on 2)

The guard rail beam according to claim 2, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has
a first slanted surface slanted from a first surface toward a center part of the steel material relative to a sheet thickness direction,
a second slanted surface slanted from a second surface toward a center part of the steel material relative to a sheet thickness direction, and
a fractured surface formed between the first slanted surface and the second slanted surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the first slanted surface and the second slanted surface are a total of 50 area % or more.

### Claim 19 (depends on 3)

The guard rail beam according to claim 3, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has
a first slanted surface slanted from a first surface toward a center part of the steel material relative to a sheet thickness direction,
a second slanted surface slanted from a second surface toward a center part of the steel material relative to a sheet thickness direction, and
a fractured surface formed between the first slanted surface and the second slanted surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and
coating coverage rates at the first slanted surface and the second slanted surface are a total of 50 area % or more.

### Claim 20 (depends on 4)

The guard rail beam according to claim 4, wherein at least one edge face other than the edge face covered by the coating layer is a cut edge face, the cut edge face has
a first slanted surface slanted from a first surface toward a center part of the steel material relative to a sheet thickness direction,
a second slanted surface slanted from a second surface toward a center part of the steel material relative to a sheet thickness direction, and
a fractured surface formed between the first slanted surface and the second slanted surface,
a length of the fractured surface in the sheet thickness direction is 40% or less of a sheet thickness of the steel material, and