# US 2026/0250812 A1 · High-strength steel sheet and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250812 A1
- Document ID: US20260250812A1
- Status: Published application
- Kind: A1
- Application number: 19/162,322
- Filed: 2024-03-05
- Published: 2026-08-27
- Earliest claimed: 2023-03-06
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Ryusuke ISHITO; Junya TOBATA; Hidekazu MINAMI; Yuki TOJI
- Web page: https://patentgrep.com/patent/US20260250812A1

## CPC

- C22C 38/04: containing manganese
- C23C 2/0224: {Two or more thermal pretreatments}
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/005: {containing Mn}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/26: with niobium or tantalum
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C23G 1/08: Iron or steel
- C25D 3/22: of zinc
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A high strength steel sheet includes a steel sheet containing, by mass, C: 0.030%-0.500%, Si: 0.50%-2.50%, Mn: 1.50%-5.00%, P: not more than 0.100%, S: not more than 0.0200%, Al: not more than 1.000%, N: not more than 0.0100%, O: not more than 0.0100%, and Nb: 0.005%-0.100%, with a balance consisting of Fe and inevitable impurities, an amount of martensite is not less than 70%, an amount of retained austenite is 3%-20%, a total amount of ferrite and bainitic ferrite is not more than 10%, an instability index k of retained austenite is less than 6.1, and an instability index d of retained austenite in an initial stage of working is less than 5.7.

## Claims

### Claim 1

A high strength steel sheet comprising a steel sheet,
wherein the steel sheet has a chemical composition including, by mass,
C in an amount of not less than 0.030% and not more than 0.500%,
Si in an amount of not less than 0.50% and not more than 2.50%,
Mn in an amount of not less than 1.50% and not more than 5.00%,
P in an amount of not more than 0.100%,
S in an amount of not more than 0.0200%,
Al in an amount of not more than 1.000%,
N in an amount of not more than 0.0100%,
O in an amount of not more than 0.0100%, and
Nb in an amount of not less than 0.005% and not more than 0.100%,
with a balance consisting of Fe and inevitable impurities,
the steel sheet has a microstructure in which an amount of martensite is not less than 70%, an amount of retained austenite is not less than 3% and not more than 20%, and a total amount of ferrite and bainitic ferrite is not more than 10%,
an instability index k of retained austenite is less than 6.1, and
an instability index d of retained austenite in an initial stage of working is less than 5.7.

### Claim 2 (depends on 1)

The high strength steel sheet according to claim 1,
wherein the chemical composition further includes at least one element selected from the group consisting of, by mass,
Ti in an amount of not more than 0.200%,
V in an amount of not more than 0.200%,
Ta in an amount of not more than 0.10%,
W in an amount of not more than 0.10%,
B in an amount of not more than 0.0100%,
Cr in an amount of not more than 1.00%,
Mo in an amount of not more than 1.00%,
Ni in an amount of not more than 1.00%,
Co in an amount of not more than 0.010%,
Cu in an amount of not more than 1.00%,
Sn in an amount of not more than 0.200%,
Sb in an amount of not more than 0.200%,
Ca in an amount of not more than 0.0100%,
Mg in an amount of not more than 0.0100%,
REM in an amount of not more than 0.0100%,
Zr in an amount of not more than 0.100%,
Te in an amount of not more than 0.100%,
Hf in an amount of not more than 0.10%, and
Bi in an amount of not more than 0.200%.

### Claim 3 (depends on 1)

The high strength steel sheet according to claim 1, further comprising a plating layer on a surface of the steel sheet.

### Claim 4 (depends on 1)

A method for manufacturing the high strength steel sheet according to claim 1, the method comprising:
retaining a steel slab having the chemical composition according to claim 1 at a slab heating temperature of not lower than 1,220° C. and then performing hot rolling to obtain a hot rolled steel sheet;
cooling the hot rolled steel sheet under a condition of an average cooling rate v1 from 800° C. to 600° C. of not lower than 30° C./s and then performing pickling and cold rolling to obtain a cold rolled steel sheet;
performing a heat treatment A in which the cold rolled steel sheet is retained at a temperature T1 of not lower than 800° C. for 10 seconds or more and then cooled to a cooling stop temperature Ta of not lower than 100° C. and not higher than (Ms point −80° C.),
where, in the heat treatment A, an average cooling rate v2 from 750° C. to 600° C. is not lower than 20° C./s, an average cooling rate v3 from the Ms point to the cooling stop temperature Ta is not higher than 150° C./s, and a tension F imparted to the cold rolled steel sheet from the Ms point to the cooling stop temperature Ta is not less than 5 MPa and not more than 100 MPa;
after the heat treatment A, performing a heat treatment B in which the cold rolled steel sheet is retained at a temperature T2 of not lower than the cooling stop temperature Ta and not higher than 450° C. for 5 seconds or more and 1,000 seconds or less and then cooled;
after the heat treatment B, performing a heat treatment C in which the cold rolled steel sheet is heated to a temperature T3 of not lower than 150° C. and not higher than 400° C. and then cooled without being retained at the temperature T3,
where, in the heat treatment C, an average cooling rate v4 from 150° C. to 50° C. is not lower than 1.0° C./s and not higher than 50.0° C./s; and
after the heat treatment A and before the heat treatment C, working the cold rolled steel sheet to impart an equivalent plastic strain of not less than 0.10% and not more than 5.00% to the cold rolled steel sheet,
wherein the Ms point is represented in a unit of ° C. and determined by Formula (a):
MS
=
519
-
474
×
[
%
⁢
C
]
-
30.4
×
[
%
⁢
Mn
]
-
12.1
×
[
%
⁢
Cr
]
-
7.5
×
[
%
⁢
Mo
]
-
17.7
×
[
%
⁢
Ni
]
(
a
)
in Formula (a), [% M] represents a content of an element M in the chemical composition, and when the element M is not contained, [% M] is 0.

### Claim 5 (depends on 4)

The method for manufacturing the high strength steel sheet according to claim 4,
wherein the cold rolled steel sheet is subjected to a plating treatment.

### Claim 6 (depends on 2)

The high strength steel sheet according to claim 2, further comprising a plating layer on a surface of the steel sheet.

### Claim 7 (depends on 2)

A method for manufacturing the high strength steel sheet according to claim 2, the method comprising:
retaining a steel slab having the chemical composition according to claim 2 at a slab heating temperature of not lower than 1,220° C. and then performing hot rolling to obtain a hot rolled steel sheet;
cooling the hot rolled steel sheet under a condition of an average cooling rate v1 from 800° C. to 600° C. of not lower than 30° C./s and then performing pickling and cold rolling to obtain a cold rolled steel sheet;
performing a heat treatment A in which the cold rolled steel sheet is retained at a temperature T1 of not lower than 800° C. for 10 seconds or more and then cooled to a cooling stop temperature Ta of not lower than 100° C. and not higher than (Ms point −80° C.),
where, in the heat treatment A, an average cooling rate v2 from 750° C. to 600° C. is not lower than 20° C./s, an average cooling rate v3 from the Ms point to the cooling stop temperature Ta is not higher than 150° C./s, and a tension F imparted to the cold rolled steel sheet from the Ms point to the cooling stop temperature Ta is not less than 5 MPa and not more than 100 MPa;
after the heat treatment A, performing a heat treatment B in which the cold rolled steel sheet is retained at a temperature T2 of not lower than the cooling stop temperature Ta and not higher than 450° C. for 5 seconds or more and 1,000 seconds or less and then cooled;
after the heat treatment B, performing a heat treatment C in which the cold rolled steel sheet is heated to a temperature T3 of not lower than 150° C. and not higher than 400° C. and then cooled without being retained at the temperature T3,
where, in the heat treatment C, an average cooling rate v4 from 150° C. to 50° C. is not lower than 1.0° C./s and not higher than 50.0° C./s; and
after the heat treatment A and before the heat treatment C, working the cold rolled steel sheet to impart an equivalent plastic strain of not less than 0.10% and not more than 5.00% to the cold rolled steel sheet,
wherein the Ms point is represented in a unit of ° C. and determined by Formula (a):
MS
=
519
-
474
×
[
%
⁢
C
]
-
30.4
×
[
%
⁢
Mn
]
-
12.1
×
[
%
⁢
Cr
]
-
7.5
×
[
%
⁢
Mo
]
-
17.7
×
[
%
⁢
Ni
]
(
a
)
in Formula (a), [% M] represents a content of an element M in the chemical composition, and when the element M is not contained, [% M] is 0.

### Claim 8 (depends on 7)

The method for manufacturing the high strength steel sheet according to claim 7,
wherein the cold rolled steel sheet is subjected to a plating treatment.