# US 2026/0250808 A1 · Non-oriented electrical steel plate with good magnetic performance and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250808 A1
- Document ID: US20260250808A1
- Status: Published application
- Kind: A1
- Application number: 18/726,656
- Filed: 2023-01-05
- Published: 2026-08-27
- Earliest claimed: 2022-01-07
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Guobao LI; Feng ZHANG; Xuejun LYU; Xianshi FANG; Yeqiao GU; Bo WANG
- Web page: https://patentgrep.com/patent/US20260250808A1

## CPC

- C22C 38/02: containing silicon
- C21D 1/26: Methods of annealing
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 8/1277: involving a particular surface treatment (C21D8/1294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed in the present invention is a non-oriented electrical steel plate with good magnetic performance. In addition to Fe and inevitable impurities, the non-oriented electrical steel plate further contains the following chemical elements, in percentage by mass: O<C≤0.0025%, Si: 0.2-1.6%, Mn: 0.2-0.6%, Al: 0.2-0.6%, V: 0.001-0.008%, N: 0.002-0.0045%, 0<Nb≤0.003% and 0<Ti≤0.003%. In addition, further disclosed in the present invention is a manufacturing method for the non-oriented electrical steel plate with good magnetic performance. The manufacturing method comprises the steps of: (1) smelting and casting; (2) hot rolling, wherein a steel coil is not subjected to normalizing annealing or cover annealing after hot rolling, but is directly introduced to the next step; (3) acid pickling; (4) cold rolling; and (5) finished product annealing, wherein the cold-rolled steel plate is rapidly heated from room temperature to a target soaking temperature at a heating rate of 80-1000° C./s. The non-oriented electrical steel plate of the present invention has good electromagnetic performance, low iron loss and high magnetic induction, can be effectively used for preparing an iron core, and has good popularization prospects and application value.

## Claims

### Claim 1

A non-oriented electrical steel plate, comprising, in addition to Fe and inevitable impurities, the following chemical elements in percentage by mass:
0<C≤0.0025%, Si: 0.2-1.6%, Mn: 0.2-0.6%, Al: 0.2-0.6%, V: 0.0031-0.008%, N: 0.002-0.0045%, 0<Nb≤0.003% and 0<Ti≤0.003%.

### Claim 2 (depends on 1)

The non-oriented electrical steel plate according to claim 1, wherein the non-oriented electrical steel plate comprises the following chemical elements in percentage by mass:
0<C≤0.0025%, Si: 0.2-1.6%, Mn: 0.2-0.6%, Al: 0.2-0.6%, V: 0.003-0.008%, N: 0.002-0.0045%, 0<Nb≤0.003%, 0<Ti≤0.003%, with the balance being Fe and inevitable impurities.

### Claim 3 (depends on 1)

The non-oriented electrical steel plate according to claim 1, wherein the percentage by mass of V is V: 0.0031-0.0045%.

### Claim 4 (depends on 1)

The non-oriented electrical steel plate according to claim 1, wherein the inevitable impurities include: S≤0.002%.

### Claim 5 (depends on 1)

The non-oriented electrical steel plate according to claim 1, wherein the non-oriented electrical steel plate comprises inclusions, which are inclusions containing C and/or N, mainly composed of AlN, VN, VC and V (CN).

### Claim 6 (depends on 5)

The non-oriented electrical steel plate according to claim 5, wherein the inclusions containing C and/or N have a size of 200-500 nm.

### Claim 7 (depends on 5)

The non-oriented electrical steel plate according to claim 5, wherein the inclusions satisfy the following formula: 1.5≤AlN content/(VN content+VC content+V(CN) content)≤4.0.

### Claim 8 (depends on 1)

The non-oriented electrical steel plate according to claim 1, wherein the non-oriented electrical steel plate has an iron loss P15/50 of 3.2 W/kg or less and a magnetic induction B50 of 1.75 T or more.

### Claim 9 (depends on 1)

A method of manufacturing the non-oriented electrical steel plate according to claim 1, comprising the following steps:
(1) subjecting molten steel to smelting and casting to obtain a slab;
(2) subjecting the slab to hot rolling to obtain a steel coil, wherein the steel coil is not subjected to normalizing annealing or cover annealing after hot rolling, but is directly introduced to the next step;
(3) performing acid pickling to obtain an acid-pickled steel plate;
(4) subjecting the acid-pickled steel plate to cold rolling to obtain a cold-rolled steel plate; and
(5) continuous annealing, wherein the cold-rolled steel plate is heated to a target soaking temperature at a heating rate of 80-1000° C./s.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the method satisfies at least one of the following conditions:
in step (5), the target soaking temperature is 800-1000° C.;
in the casting process of step (1), the molten steel has a superheat of 10-35° C., a time for transition between solid phase and liquid phase is 10 s-120 min, the temperature of the casting is within a range of 900-1150° C., and the slab is cooled at a rate of 10° C./min or less;
in step (2), during the hot rolling, a time for the slab to stay in a furnace is 120-360 min, an initial rolling temperature is 1050-1150° C., a final rolling temperature is 650-950° C., and a coiling temperature is 500-900° C.;
in step (2), the hot-rolled steel plate has a target thickness of 0.8-3.5 mm; and/or
in step (4), the acid-pickled steel plate is cold-rolled to a target cold rolling thickness in one time.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the non-oriented electrical steel plate comprises the following chemical elements in percentage by mass:
0<C≤0.0025%, Si: 0.2-1.6%, Mn: 0.2-0.6%, Al: 0.2-0.6%, V: 0.0031-0.008%, N: 0.002-0.0045%, 0<Nb≤0.003%, 0<Ti≤0.003%, with the balance being Fe and inevitable impurities.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the percentage by mass of Vis 0.0031-0.0045%.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the inevitable impurities include: S≤0.002%.

### Claim 14 (depends on 9)

The method according to claim 9, wherein the non-oriented electrical steel plate comprises inclusions, which are inclusions containing C and/or N, mainly composed of AlN, VN, VC and V (CN).

### Claim 15 (depends on 9)

The method according to claim 9, wherein the inclusions containing C and/or N have a size of 200-500 nm.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the inclusions satisfy the following formula: 1.5≤AlN content/(VN content+VC content+V (CN) content)≤4.0.

### Claim 17 (depends on 9)

The method according to claim 9, wherein the non-oriented electrical steel plate has an iron loss P15/50 of 3.2 W/kg or less and a magnetic induction B50 of 1.75 T or more.