# US 2026/0250427 A1 · Method to reduce alkoxy ether release from cellulose ethers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250427 A1
- Document ID: US20260250427A1
- Status: Published application
- Kind: A1
- Application number: 18/875,907
- Filed: 2023-06-29
- Published: 2026-08-27
- Earliest claimed: 2022-06-29
- Applicants: Dow Global Technologies LLC
- Inventors: Jorg Theuerkauf; Praveenkumar Boopalachandran; Scott T. Matteucci; Daniel G. Abebe; Beata A. Kilos; Kanjakha Pal; Kefu Sun
- Web page: https://patentgrep.com/patent/US20260250427A1

## CPC

- C08B 11/02: Alkyl or cycloalkyl ethers
- C08B 11/20: Post-etherification treatments of chemical or physical type, {e.g. mixed etherification in two steps}, including purification
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)

## Abstract

The release of alkoxy ethers from a cellulose ether composition that contains alkoxy ethers can be reduced by contacting the cellulose ether composition with a zeolite having a silica to alumina molar ratio (SiO2/Al2O3) greater than 3, in a quantity sufficient to adsorb at least some alkoxy ethers that are present.

## Claims

### Claim 1

A method to reduce the release of alkoxy ethers from a cellulose ether composition that contains alkoxy ethers, comprising the step of contacting the cellulose ether composition with a zeolite having a silica to alumina molar ratio (SiO2/Al2O3) greater than 3, in a quantity sufficient to adsorb at least some alkoxy ethers that are present.

### Claim 2 (depends on 1)

The method of claim 1 wherein the weight ratio of zeolite to dry-weight of cellulose ether is more than 0.5% and no more than 10%.

### Claim 3 (depends on 2)

The method of any one of claim 2 wherein the weight ratio of zeolite to dry-weight of cellulose ether is from 1% to 5%.

### Claim 4 (depends on 3)

The method of claim 3 wherein the zeolite has a silica to alumina molar ratio (SiO2/Al2O3) greater than 4.

### Claim 5 (depends on 3)

The method of claim 3 wherein the zeolite has a silica to alumina molar ratio (SiO2/Al2O3) greater than 5.

### Claim 6 (depends on 3)

The method of claim 3 wherein the zeolite has an average pore size from 3 Å to 12 Å.

### Claim 7 (depends on 3)

The method of claim 3 wherein the zeolite has an average pore size from 4 Å to 10 Å.

### Claim 8 (depends on 3)

The method of claim 3 wherein the zeolite has a pore volume from 0.1 cm3/g to 0.6 cm3/g.

### Claim 9 (depends on 3)

The method of claim 3 wherein the zeolite contains a Y zeolite.

### Claim 10 (depends on 3)

The method of claim 3 wherein the zeolite contains an MFI zeolite.

### Claim 11 (depends on 3)

The method of claim 3 wherein the zeolite contains a ZSM-5 zeolite.

### Claim 12 (depends on 3)

The method of claim 3 wherein the cellulose ether composition contains methylcellulose, ethyl cellulose, ethyl methyl cellulose, hydroxyethyl cellulose, hydroxypropyl cellulose or hydroxypropyl methylcellulose.

### Claim 13 (depends on 3)

The method of claim 3 wherein the alkoxy ether is 2-methoxyethanol.

### Claim 14 (depends on 3)

The method of claim 3 wherein the method of this invention reduces the concentration of free alkoxy ether in the cellulose ether composition to no more than 40 weight percent of pre-treatment concentrations.

### Claim 15

A cellulose ether composition that contains from 0.5 weight percent to 5 weight percent of zeolite having a silica to alumina molar ratio (SiO2/Al2O3) greater than 3, wherein the weight percentages are based on the dry weight of the cellulose ether powder.