# US 2026/0250216 A1 · Process for obtaining ignition pastes in an acoustic resonance mixer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250216 A1
- Document ID: US20260250216A1
- Status: Published application
- Kind: A1
- Application number: 18/844,648
- Filed: 2023-02-14
- Published: 2026-08-27
- Earliest claimed: 2022-02-15
- Assignees: Eurenco France SAS
- Applicants: Eurenco France SAS
- Inventors: Sébastien CUVELIER; Julie PEROUEL; Nicolas MARONCELLI
- Web page: https://patentgrep.com/patent/US20260250216A1

## CPC

- C06B 21/0016: {the ingredient being nitrocellulose or oranitro cellulose based propellant; Working up; gelatinising; stabilising (stabilising of explosives in general C06B21/0091)}
- C06B 21/0025: {the ingredient being a polymer bonded explosive or thermic component}
- C06B 25/28: the compound being nitrocellulose present as less than 10% by weight of the total composition
- C06B 33/14: at least one being an inorganic nitrogen-oxygen salt
- C06C 9/00: Chemical contact igniters; Chemical lighters
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})
- C06C: DETONATING OR PRIMING DEVICES; FUSES (ammunition fuzes F42C); CHEMICAL LIGHTERS; PYROPHORIC COMPOSITIONS

## Abstract

A process for obtaining an ignition paste which includes mixing the various ingredients constituting the paste in an acoustic resonance mixer. Also, a process for obtaining an ignition charge, which includes depositing the ignition paste, obtained according to the above process, on a combustible support, and drying the combustible support.

## Claims

### Claim 1

A process for obtaining an ignition paste containing, as ingredients, a reducing charge, an oxidizing charge and a cellulose ether- or cellulose ester-based collodion, the said process comprising a step of premixing, in an acoustic resonance mixer, the reducing charge and/or the oxidizing charge with the collodion.

### Claim 2 (depends on 1)

The process of claim 1, which comprises:
a) premixing, in an acoustic resonance mixer, one of the reducing and oxidizing charges with collodion;
b) mixing, in an acoustic resonance mixer, the product obtained in step a) with the other of the reducing and oxidizing charges.

### Claim 3 (depends on 2)

The process of claim 2, comprising incrementing an increased acceleration in each of steps a) and b).

### Claim 4 (depends on 1)

The process of claim 1, which comprises:
a) premixing the reducing charge with collodion in an acoustic resonance mixer;
b) premixing the oxidizing charge with collodion in an acoustic resonance mixer;
c) mixing, in an acoustic resonance mixer, the product obtained in step a) with the product obtained in step b).

### Claim 5 (depends on 4)

The process of claim 4, wherein substantially equal amounts of collodion are used in step a) and step b).

### Claim 6 (depends on 1)

The process of claim 1, comprising:
a) introducing the reducing charge, the collodion and the oxidizing charge in superimposed layers into an acoustic resonance mixer, whereby the collodion forms an intermediate layer between the reducing charge and the oxidizing charge;
b) applying an acoustic intensity to the superimposed layers, in increments of increasing acceleration, whereby a layer of reducing charge premixed with the collodion, a residual layer of collodion inbetween, and a layer of oxidizing charge premixed with the collodion are formed in the mixer;
c) applying an acoustic intensity greater than that used in step b) to the premixes obtained in step b), in increments of increasing acceleration.

### Claim 7 (depends on 6)

The process of claim 6, comprising implementing in step b) increments of increasing acceleration over a range of values from about 10 g to about 50 g.

### Claim 8 (depends on 1)

The process of claim 1, in which the ignition paste comprises about 50% to about 70% by weight of reducing and oxidizing charges, and about 30% to about 50% by weight of collodion.

### Claim 9 (depends on 1)

The process of claim 1, in which the collodion is a cellulose ester-based collodion.

### Claim 10 (depends on 9)

The process of claim 9, in which the collodion comprises, by weight:
about 70% to about 90% of a cellulose ester;
about 1% to about 20% of at least one plasticizer;
about 0.5% to about 5% of at least one cellulose ester stabilizer;
>0% to about 1% of at least one additive.

### Claim 11 (depends on 1)

The process of claim 1, in which the collodion is a cellulose ether-based collodion.

### Claim 12 (depends on 11)

The process of claim 11, in which the collodion comprises, by weight:
about 70% to about 90% of a cellulose ether;
about 1% to about 20% of at least one plasticizer;
about 0.5% to about 5% of at least one cellulose ether stabilizer;
>0% to about 1% of at least one additive.

### Claim 13 (depends on 1)

A process of obtaining an ignition charge, which comprises preparing an ignition paste according to the process defined in claim 1, depositing the ignition paste thus prepared on a combustible support, and drying the combustible support.

### Claim 14 (depends on 10)

The process of claim 10, in which the cellulose ester is nitrocellulose.

### Claim 15 (depends on 12)

The process of claim 12, in which the cellulose ether is ethyl cellulose.