# US 2026/0250138 A1 · Reverse water gas shift catalysts comprising an alkali metal and alumina

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0250138 A1
- Document ID: US20260250138A1
- Status: Published application
- Kind: A1
- Application number: 19/062,818
- Filed: 2025-02-25
- Published: 2026-08-27
- Earliest claimed: 2025-02-25
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Mohammed A. AL-DAOUS; Khaled NAFEE
- Web page: https://patentgrep.com/patent/US20260250138A1

## CPC

- C01B 32/40: Carbon monoxide
- B01J 21/04: Alumina
- B01J 23/04: Alkali metals
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01B 3/16: using catalysts
- C01B 3/50: Separation of hydrogen or hydrogen-containing gases from gaseous mixtures, e.g. purification
- C10K 1/005: {Carbon dioxide}
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- C01B 2203/1276: Mixing of different feed components
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10K: PURIFYING OR MODIFYING THE CHEMICAL COMPOSITION OF COMBUSTIBLE GASES CONTAINING CARBON MONOXIDE

## Abstract

The reverse water-gas shift reaction catalysts comprising an alkali metal supported on alumina. Embodiments generally relate to catalysts for reverse water-gas shift (RWGS), methods for making the catalysts, and methods for using the catalysts in RWGS reactions. The disclosure generally relates to catalysts comprising at least one alkali metal on alumina (Al2O3), wherein the alumina in a phase selected from the group consisting of alpha-alumina (α-Al2O3) phase, theta-alumina (θ-Al2O3) phase, gamma-alumina (γ-Al2O3) phase, and any combination thereof. The catalysts are in a form of a plurality of particles having an average particle size of about 200 micrometers to about 500 micrometers.

## Claims

### Claim 1

A catalyst comprising:
alumina in a phase selected from the group consisting of alpha-alumina (α-Al2O3) phase, theta-alumina (θ-Al2O3) phase, gamma-alumina (γ-Al2O3) phase, and any combination thereof; and
an alkali metal in an amount of about 1 weight % to about 9.5 weight % per the catalyst;
wherein the catalyst is in a form of a plurality of particles having an average particle size of about 200 micrometers to about 500 micrometers.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein the alkali metal is selected from the group consisting of lithium (Li), sodium (Na), potassium (K), cesium (caesium) (Cs), and any combination thereof.

### Claim 3 (depends on 1)

The catalyst of claim 1, wherein the alkali metal is selected from the group consisting of lithium (Li), potassium (K), cesium (caesium) (Cs), and any combination thereof.

### Claim 4 (depends on 1)

The catalyst of claim 1, wherein the amount of the alkali metal is about 1 weight % to about 6 weight % per the catalyst.

### Claim 5 (depends on 2)

The catalyst of claim 2, wherein the catalyst comprises γ-Al2O3 and about 5 weight % of the potassium (K) per the catalyst.

### Claim 6 (depends on 2)

The catalyst of claim 2, wherein the catalyst comprises θ-Al2O3 and about 1 weight % of the potassium (K) per the catalyst.

### Claim 7

A method comprising:
combining alumina (Al2O3) and a solution comprising an alkali metal compound to produce a homogeneous paste;
drying the homogeneous paste at about 120° C. for at least about 24 hours; and
calcining the homogenous paste for at least about 1 hour at a calcining temperature of at least about 550° C. to produce a catalyst comprising the alkali metal and the alumina.

### Claim 8 (depends on 7)

The method of claim 7, wherein the alumina is in a phase selected from the group consisting of alpha-alumina (α-Al2O3) phase, theta-alumina (θ-Al2O3) phase, gamma-alumina (γ-Al2O3) phase, and any combination thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the calcining temperature is about 550° C. to about 750° C.

### Claim 10 (depends on 8)

The method of claim 8, wherein the catalyst comprises γ-Al2O3 and about 5 weight % of potassium (K) per the catalyst; wherein the solution comprises a KHCO3 aqueous mixture; and wherein the calcining temperature is about 600° C. for about 5 hours under static air.

### Claim 11 (depends on 8)

The method of claim 8, wherein the catalyst comprises θ-Al2O3 and about 1 weight % of potassium (K) per the catalyst; wherein the solution comprises a KHCO3 aqueous mixture; and wherein the calcining temperature is about 600° C. for about 5 hours under static air.

### Claim 12 (depends on 7)

The method of claim 7, further comprising:
processing the catalyst to produce a plurality of particles having an average particle size of about 200 micrometers to about 500 micrometers.

### Claim 13 (depends on 7)

The method of claim 7, wherein the alkali metal compound comprises an alkali metal selected from the group consisting of lithium (Li), sodium (Na), potassium (K), cesium (caesium) (Cs), and any combination thereof; and wherein the alkali metal compound is selected from the group consisting of alkali metal nitrates, alkali metal chlorides, alkali metal carbonates, alkali metal bicarbonates (alkali metal hydrogencarbonates), alkali metal benzoates, alkali metal acetylacetonates, alkali metal acetates, and any combination thereof.

### Claim 14 (depends on 1)

A method comprising:
introducing the catalyst of claim 1 into a chemical reactor;
activating the catalyst by heating the catalyst to an activation temperature of at least about 650° C. at a rate of about 5° C./min to about 15° C./min under argon;
flowing a feed composition at a Gas Hourly Space Velocity of about 3300 mL (grams of catalyst)−1 hour 1 to about 13,200 mL (grams of catalyst)−1 hour−1 into the chemical reactor, wherein the feed composition comprises CO2 and H2;
maintaining the chemical reactor at a reaction temperature of about 550° C. to about 900° C. and at a pressure of about atmospheric pressure to about 5 bar gauge (barg); and
recovering a first mixture stream leaving the chemical reactor, wherein the first mixture stream comprises:
water (H2O) vapor, unreacted carbon dioxide (CO2) gas, unreacted hydrogen (H2) gas, and carbon monoxide (CO) gas.

### Claim 15 (depends on 14)

The method of claim 14, wherein the feed composition has a CO2:H2 ratio of about 1:1 to about 1:5.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
removing the water (H2O) vapor from the first mixture stream to generate a second mixture stream, wherein the second mixture stream comprises: the carbon monoxide (CO) gas from the first mixture stream, the unreacted carbon dioxide (CO2) gas from the first mixture stream, and the unreacted hydrogen (H2) gas from the first mixture stream.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
recovering the unreacted carbon dioxide (CO2) from the second mixture stream to form a syngas mixture stream; and then optionally,
utilizing the syngas mixture stream;
wherein the syngas mixture stream comprises the carbon monoxide (CO) gas from the second mixture stream and the unreacted hydrogen (H2) gas from the second mixture stream.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
recovering the unreacted hydrogen (H2) gas from the syngas mixture stream to produce a first stream of carbon monoxide; and then optionally,
utilizing the first stream of carbon monoxide;
wherein the first stream of carbon monoxide comprises the carbon monoxide (CO) gas from the syngas mixture stream.

### Claim 19 (depends on 16)

The method of claim 16, further comprising:
recovering the unreacted hydrogen (H2) gas from the second mixture stream to generate a third mixture stream,
wherein the third mixture stream comprises the carbon monoxide (CO) gas from the second mixture stream and the unreacted carbon dioxide (CO2) gas from the second mixture stream.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
recovering the unreacted carbon dioxide (CO2) from the third mixture stream to form a second stream of carbon monoxide; and then optionally,
utilizing the second stream of carbon monoxide;
wherein the second stream of carbon monoxide comprises the carbon monoxide (CO) gas from the third mixture stream.

### Claim 21 (depends on 14)

The method of claim 14, wherein the reaction temperature is about 700° C. to about 900° C.

### Claim 22 (depends on 14)

The method of claim 14, wherein the chemical reactor is a fixed-bed reactor.

### Claim 23 (depends on 22)

The method of claim 22, wherein the catalyst comprises γ-Al2O3 and about 5 weight % of potassium (K) per the catalyst in the fixed-bed reactor; wherein the feed composition has a CO2:H2 ratio of about 1:1 to about 1:5; wherein the reaction temperature is about 750° C. and the pressure is about atmospheric pressure; and wherein the Gas Hourly Space Velocity is about 6600 mL (grams of catalyst)−1 hour−1.

### Claim 24 (depends on 22)

The method of claim 22, wherein the catalyst comprises θ-Al2O3 and about 1 weight % of potassium (K) per the catalyst in the fixed-bed reactor; wherein the feed composition has a CO2:H2 ratio of about 1:1, wherein the reaction temperature is about 750° C. and the pressure is about atmospheric pressure; and wherein the Gas Hourly Space Velocity is about 6600 mL (grams of catalyst)−1 hour−1.