# US 2026/0249250 A1 · Polysilsesquioxane/polyetheretherketone composite membranes and methods for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0249250 A1
- Document ID: US20260249250A1
- Status: Published application
- Kind: A1
- Application number: 19/530,433
- Filed: 2026-02-05
- Published: 2026-08-27
- Earliest claimed: 2024-08-15
- Assignees: Changzhou University
- Applicants: Changzhou University
- Inventors: Meng GUO; Jing ZHONG; Xiuxiu REN; Yang PAN; Junzhu CHEN; Rong XU; Cheng XUE
- Web page: https://patentgrep.com/patent/US20260249250A1

## CPC

- B01D 69/12: Composite membranes; Ultra-thin membranes
- B01D 67/0006: {by chemical reactions (in-situ polymerisation, polycondensation, cross-linking or reaction for manufacturing composite membranes B01D69/125)}
- B01D 67/0083: {Thermal after-treatment}
- B01D 67/0095: {Drying}
- B01D 69/107: {Organic support material}
- B01D 69/1216: {Three or more layers}
- B01D 69/1251: {by interfacial polymerisation}
- B01D 71/5222: {Polyetherketone, polyetheretherketone, or polyaryletherketone}
- B01D 71/56: Polyamides, e.g. polyester-amides
- B01D 71/70: Polymers having silicon in the main chain, with or without sulfur, nitrogen, oxygen or carbon only
- B01D 71/702: {Polysilsesquioxanes or combination of silica with bridging organosilane groups}
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

A polysilsesquioxane/polyetheretherketone composite membrane and a method for preparing the same are provided. The method includes: obtaining a polysilsesquioxane polymeric sol by mixing an ethanol solvent and a polysilsesquioxane precursor, sequentially adding deionized water and hydrochloric acid after complete dissolution, followed by constant-temperature water bath stirring for performing a polymerization reaction; and obtaining the polysilsesquioxane/polyetheretherketone composite membrane by coating the polysilsesquioxane polymeric sol on a polyetheretherketone support on which an intermediate layer is formed by knife coating.

## Claims

### Claim 1

A method for preparing a polysilsesquioxane/polyetheretherketone composite membrane, comprising:
obtaining a polysilsesquioxane polymeric sol by mixing an ethanol solvent and a polysilsesquioxane precursor, sequentially adding deionized water and hydrochloric acid after complete dissolution, followed by constant-temperature water bath stirring for performing a polymerization reaction; and
obtaining the polysilsesquioxane/polyetheretherketone composite membrane by coating the polysilsesquioxane polymeric sol on a polyetheretherketone support on which an intermediate layer is formed by knife coating, wherein
a molar ratio of the polysilsesquioxane precursor, the deionized water, and the hydrochloric acid is 1:(6-240):(0.2-1),
a mass fraction of the polysilsesquioxane polymeric sol is 5 wt %-10 wt %; and
the intermediate layer on the polyetheretherketone support is formed by a process including:
subjecting an aqueous phase piperazine solution and an organic phase 1,3,5-benzenetricarbonyl chloride solution to an interfacial polymerization reaction on the polyetheretherketone support, or
subjecting polydimethylsiloxane or amino silicone oil to an oxygen plasma modification on the polyetheretherketone support.

### Claim 2 (depends on 1)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 1, wherein the polysilsesquioxane precursor comprises one of 1,2-bis(triethoxysilyl)ethane, 1,2-bis(triethoxysilyl)ethylene, 1,2-bis(triethoxysilyl)acetylene, 1,2-bis(triethoxyalkyl) methane, or 1,8-bis(triethoxyalkyl)octane.

### Claim 3 (depends on 1)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 1, wherein a stirring temperature of the constant-temperature water bath stirring is 30° C.-80° C., and a stirring time of the constant-temperature water bath stirring is 1 h-5 h.

### Claim 4 (depends on 1)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 1, wherein the subjecting the aqueous phase piperazine solution and the organic phase 1,3,5-benzenetricarbonyl chloride solution to the interfacial polymerization reaction on the polyetheretherketone support comprises:
fixing the polyetheretherketone support, and pouring the aqueous phase piperazine solution onto a surface of the polyetheretherketone support for residence and reaction, and
removing an excess of the aqueous phase piperazine solution on the surface of the polyetheretherketone support with a roller, then pouring the organic phase 1,3,5-benzenetricarbonyl chloride solution for residence to perform the interfacial polymerization reaction to form the intermediate layer, wherein
a concentration of the aqueous phase piperazine solution is 0.5 wt %-2 wt %,
a residence time of the aqueous phase piperazine solution is 1 min-5 min,
a concentration of the organic phase 1,3,5-benzenetricarbonyl chloride solution is 0.01 wt %-0.1 wt %, and
a residence time of the organic phase 1,3,5-benzenetricarbonyl chloride solution is 1 min-5 min; and
a plasma treatment pressure of the oxygen plasma modification is 15 Pa-25 Pa, a treatment power of the oxygen plasma modification is 150 W-250 W, and a treatment time of the oxygen plasma modification is 60 s-180 s.

### Claim 5 (depends on 1)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 1, wherein the coating the polysilsesquioxane polymeric sol on the polyetheretherketone support on which the intermediate layer is formed by the knife coating comprises:
fixing the polyetheretherketone support on which the intermediate layer is formed,
dropping the polysilsesquioxane polymeric sol onto one end of the polyetheretherketone support, and
coating a layer of the polysilsesquioxane polymeric sol with a knife at a constant speed, with a thickness of 200 nm-500 nm, and after calcination and drying, forming the polysilsesquioxane/polyetheretherketone composite membrane.

### Claim 6 (depends on 5)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 5, wherein the constant speed for the coating is 0.5 cm/s-5 cm/s.

### Claim 7 (depends on 5)

The method for preparing the polysilsesquioxane/polyetheretherketone composite membrane according to claim 5, wherein a temperature of the calcination and drying is 50° C.-200° C., and a time of the calcination and drying is 15 min-60 min.

### Claim 8 (depends on 1)

A polysilsesquioxane/polyetheretherketone composite membrane, which is prepared by the method according to claim 1, wherein the polysilsesquioxane/polyetheretherketone composite membrane comprises a support, the intermediate layer, and a polymeric sol layer, wherein
a material of the support is polyetheretherketone, and a pore size of the support is 1 nm-100 nm,
a material of the polymeric sol layer is the polysilsesquioxane polymeric sol,
the intermediate layer is formed on the support, and
the polymeric sol layer is coated on a surface of the intermediate layer.

### Claim 9 (depends on 1)

A use of the polysilsesquioxane/polyetheretherketone composite membrane prepared by the method according to claim 1 in separating an organic mixed solvent, comprising:
separating the organic mixed solvent by pervaporation using the polysilsesquioxane/polyetheretherketone composite membrane, wherein
a separation system of the organic mixed solvent comprises methanol/toluene and methanol/dimethyl carbonate.