# US 2026/0245859 A1 · Manufacture of dry electrodes for batteries using a solvent free paste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0245859 A1
- Document ID: US20260245859A1
- Status: Published application
- Kind: A1
- Application number: 19/161,968
- Filed: 2024-03-07
- Published: 2026-08-20
- Earliest claimed: 2023-03-08
- Assignees: Automotive Cells Company SE
- Applicants: Automotive Cells Company SE
- Inventors: Imed Eddine BEN-ALI; Thomas DEVANNE
- Web page: https://patentgrep.com/patent/US20260245859A1

## CPC

- B29C 43/24: Calendering
- H01M 4/0435: {Rolling or calendering}
- B29C 43/003: {characterised by the choice of material}
- H01G 11/28: arranged or disposed on a current collector; Layers or phases between electrodes and current collectors, e.g. adhesives
- H01G 11/50: specially adapted for lithium-ion capacitors, e.g. for lithium-doping or for intercalation
- H01G 11/70: characterised by their structure
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/139: Processes of manufacture
- H01M 4/622: {being polymers}
- B29C 43/28: incorporating preformed parts or layers, e.g. compression moulding around inserts or for coating articles
- B29L 2031/3468: {Batteries, accumulators or fuel cells (battery cases B29L2031/7146)}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 4/667: {in the form of layers, e.g. coatings}
- Y02E 60/10: Energy storage using batteries
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for manufacturing a dry electrode for batteries, directly from an agglomerate of a dry paste of a fibrilized mixture of electrode materials comprising at least one electrode active material, optionally at least one conductive material, at least one binder and optionally at least one co-binder, by continuously calendering said agglomerates and then laminating the formed calendered film.

## Claims

### Claim 1

A method for manufacturing a dry electrode for batteries, said method comprising the following steps:
step 1) providing solvent free agglomerates of a dry paste of a fibrilized mixture of electrode materials, said mixture of electrode materials comprising at least one active electrode material, optionally at least one conductive material, at least one binder, and optionally at least one co-binder, said agglomerates having a size in the range of 10 micrometres (pm) to 2 centimetres (cm), and said solvent free agglomerates of the dry paste of a fibrilized mixture of electrode materials having a temperature between 50° C. and 100° C.;
step 2) of continuously calendaring, at a temperature ranging between 80° C. to 120° C. , said agglomerates of the dry paste of the fibrilized mixture of electrode materials provided at step 1). to form a calendered film of dry electrode materials mixture-; and
step 3) of laminating said calendered film of the dry electrode materials mixture resulting from step 2) on at least one surface of a current collector to coat said current collector on at least one of its surfaces, with said calendered film of the dry electrode materials characterized in that said solvent free agglomerates of the dry paste of the fibrilized mixture of electrode materials provided at step a) is produced by a dry one-pot method comprising the following steps:
step 1a) of providing the following powders:
powder of at least one electrode active material,
A powder of at least one binder, and
step 1b) of dry mixing together all the powders provided at step 1a), to form a primary mixture of all these powders;
step 1c) of dry mixing said primary mixture resulting from step 1b), for a sufficient time, to reach a fibrilization temperature ranging between 50° C. and 100° C., for the resulting mixture to be converted to the solvent free agglomerates of the dry paste of the fibrilized mixture of electrode materials having a size in the range of 10 micrometres (pm) to 2 centimetres (cm).

### Claim 2 (depends on 1)

The method according to claim 1, in which, the steps 1b) and 1c) are implemented in one rotative tumbler blender equipped with rotative high shear blades.

### Claim 3 (depends on 2)

The method according to claim 2, in which a speed of rotation of a blender bowl, is 5 to 20 rounds per minute (rpm), and a speed of rotation of the shearing blades is 1,000 to 3,000 rpm.

### Claim 4 (depends on 2)

The method according to claim 2, in which the temperature inside a blender bowl progressively increases during step 1c) such as to reach between 50° C. to 100° C. and to induce the fibrillization of said primary mixture resulting from step 1b).

### Claim 5 (depends on 1)

A method according to claim 1 in which step 2) comprises the following successive steps:
step 2a) of transferring, without cooling, said agglomerates of the dry paste of a fibrilized mixture of electrode materials provided at step 1). from a rotative tumbler-blender, to a buffer tank,
step 2b) of transferring, without cooling, said agglomerates of the dry paste of the fibrilized mixture of electrode materials from said buffer tank to a feeding hopper, using a pneumatic aspiration system;
step 2c) of transferring said agglomerates of the dry paste of the fibrilized mixture of electrode materials from said feeding hopper to a multiple rolls calendering system using a conveyor belt equipped with a vibrational system; and
step 2d) of calendering at a temperature ranging between 80° C. to 120° C. said agglomerates of the dry paste of the fibrilized mixture of electrode materials using said multiple rolls calendering system, to form the calendered film of the dry electrode materials mixture.

### Claim 6 (depends on 1)

The method according to claim 1, in which said film of said dry electrode materials mixture resulting from step 2) or step 2d), has a thickness from 1 mm to 5 mm.

### Claim 7 (depends on 1)

The method according to claim 1, in which said laminating step 3) is implemented on both faces of a current collector sheet.

### Claim 8 (depends on 1)

The method according to claim 1, wherein step 1a further comprises providing a powder of at least one conductive material.

### Claim 9 (depends on 1)

The method according to claim 1, wherein step la further comprises providing a powder of at least one co-binder.

### Claim 10 (depends on 3)

The method according to claim 3, in which a speed of rotation of a blender bowl is 5 to 15 rpm.

### Claim 11 (depends on 3)

The method according to claim 3, wherein a speed of rotation of the shearing blades remains constant during the steps 1b) and 1c).

### Claim 12 (depends on 1)

The method according to claim 1, in which said film of said dry electrode materials mixture resulting from step 2) or step 2d), has a thickness from 1 mm to 3 mm.