# US 2026/0245790 A1 · Method for packaging sheet metal parts made from an electrical steel strip or sheet to form a laminated core

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0245790 A1
- Document ID: US20260245790A1
- Status: Published application
- Kind: A1
- Application number: 19/161,374
- Filed: 2024-03-04
- Published: 2026-08-20
- Earliest claimed: 2023-03-02
- Assignees: voestalpine Stahl GmbH
- Applicants: voestalpine Stahl GmbH
- Inventors: Ronald Fluch
- Web page: https://patentgrep.com/patent/US20260245790A1

## CPC

- H01F 41/0233: {Manufacturing of magnetic circuits made from sheets (magnetic cores made from sheets H01F27/245; soft magnetic alloys in the form of sheets H01F1/16)}
- H02K 15/02: of stator or rotor bodies
- H01F 3/02: made from sheets
- H02K 1/20: with channels or ducts for flow of cooling medium
- H02K 1/32: with channels or ducts for flow of cooling medium
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})

## Abstract

A method is demonstrated for stacking sheet metal parts made from an electrical steel strip or sheet to form a laminated core. In order to achieve freedom from leakage, it is proposed for the stacking to be carried out in such a way that all of the sheet metal parts in the stack are positioned at a rotational angle that is offset in the circumferential direction of the stack relative to their respective adjacent sheet metal part or adjacent sheet metal parts.

## Claims

### Claim 1

A method for packaging sheet metal parts made from an electrical steel strip or sheet to form a laminated core, comprising:
stacking a plurality of the sheet metal parts, each of which has a hot-melt adhesive varnish layer over an entire surface on both flat sides, on top of one another in such a way that in a stack of the stacked sheet metal parts, each of the plurality of sheet metal parts is positioned at a rotational angle that is offset in a circumferential direction of the stack relative to an adjacent sheet metal part or adjacent sheet metal parts, and
subsequently bonding the stacked sheet metal parts to one another over the entire surface of the sheet metal parts with the hot-melt adhesive varnish layers to form the laminated core.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in order to produce the rotational angle offset in the stack, the sheet metal part to be stacked on another sheet metal part is rotated in the circumferential direction of the stack and/or the stack is rotated about its circumferential direction.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a rotational angle (φ) in a range from 20 to 160 degrees is used for the rotational angle offset.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the rotational angle (φ) is 90 degrees.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the stacked sheet metal parts are embodied as axially symmetrical in relation to a longitudinal axis extending through a middle of the stack.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the hot-melt adhesive varnish layers on the sheet metal parts to be stacked are in a B-state.

### Claim 7 (depends on 1)

The method according to claim 1, wherein on its two opposite flat sides, each of the plurality of sheet metal parts has hot-melt adhesive varnish layers with different Martens hardnesses, determined according to DIN EN ISO 14577 with a force penetration depth method at a maximum force Fmax (depth hardness).

### Claim 8 (depends on 7)

The method according to claim 7, wherein each of the plurality of sheet metal parts is stacked in such a way that the hot-melt adhesive varnish layers between two adjacent sheet metal parts have different Martens hardnesses.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the hot-melt adhesive varnish layer on a first and/or second flat side of each sheet metal part have/has a Martens hardness in a range from 50 to 700 MPa.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the Martens hardnesses of the hot-melt adhesive varnish layers on the two opposite flat sides of each sheet metal part differ by at least 20 MPa.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the Martens hardnesses are determined at a test temperature in a temperature range between a lowest glass transition temperature of the hot-melt adhesive varnish layers and a highest glass transition temperature of the hot-melt adhesive varnish layers.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the stacked sheet metal parts are subjected to pressure in a longitudinal direction of the stack.

### Claim 13 (depends on 12)

The method according to claim 12, wherein when being subjected to pressure, at least the hot-melt adhesive varnish with a lower Martens hardness has a temperature greater than its glass transition temperature.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the stacked sheet metal parts are subjected to pressure in a range from 0.5 to 10 N/mm2 in the longitudinal direction of the stack during the bonding.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the sheet metal parts each have at least one channel opening and are stacked on top of one another in such a way that the channel openings delimit a cooling channel that extends in the laminated core and is positioned eccentrically with respect to a longitudinal axis of the laminated core extending through a middle of the laminated core.

### Claim 16 (depends on 1)

The method according to claim 1, comprising providing an electrical steel strip or sheet with the hot-melt adhesive varnish layers over an entire surface on two flat sides, and separating the plurality of the sheet metal parts to be stacked on top of one another from the electrical steel strip or sheet.

### Claim 17 (depends on 9)

The method according to claim 9, wherein the hot-melt adhesive varnish layer on the first and/or second flat side of each sheet metal part have/has a Martens hardness in a range from 100 to 500 MPa.

### Claim 18 (depends on 10)

The method according to claim 10, wherein the Martens hardnesses of the hot-melt adhesive varnish layers on the two opposite flat sides of each sheet metal part differ by at least 50 MPa.

### Claim 19 (depends on 11)

The method according to claim 11, wherein the Martens hardnesses are determined at a test temperature in a temperature range from 45 to below 80 degrees Celsius.

### Claim 20 (depends on 12)

The method according to claim 12, wherein when being subjected to pressure, at least the hot-melt adhesive varnish with the lower Martens hardness has a temperature in a range from 80 to 220° C.