# US 2026/0243657 A1 · Method for measuring peel strength of metal-bonded ceramic substrate, method for manufacturing metal-bonded ceramic substrate, and metal bonded ceramic substrate manufactured thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0243657 A1
- Document ID: US20260243657A1
- Status: Published application
- Kind: A1
- Application number: 19/164,959
- Filed: 2024-02-29
- Published: 2026-08-20
- Earliest claimed: 2023-03-15
- Assignees: Amogreentech Co., Ltd.
- Applicants: Amogreentech Co., Ltd.
- Inventors: Jihyung LEE
- Web page: https://patentgrep.com/patent/US20260243657A1

## CPC

- G01N 19/04: Measuring adhesive force between materials, e.g. of sealing tape, of coating
- G01N 1/28: Preparing specimens for investigation {including physical details of (bio-)chemical methods covered elsewhere, e.g. G01N33/50, C12Q}(mounting specimens on microscopic slides G02B21/34; means for supporting the objects or the materials to be analysed in electron microscopes H01J37/20 {; laboratory gas handling apparatus B01L5/00})
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H05K 3/06: the conductive material being removed chemically or electrolytically, e.g. by photo-etch process {(semi-additive methods H05K3/108)}
- H05K 2203/162: Testing a finished product, e.g. heat cycle testing of solder joints
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A metal-bonded ceramic substrate according to an embodiment of the present invention has metal layers bonded to the surface thereof so as to form circuit patterns, and has a plurality of the circuit patterns arranged in columns and rows, wherein, when the circuit patterns are formed, a dummy pattern for measuring peel strength can also be formed in at least one from among a plurality of dummy areas, which encompass a circuit pattern area.

## Claims

### Claim 1

A method for measuring peel strength of a metal-bonded ceramic substrate, comprising:
providing a metal-bonded ceramic substrate including a circuit pattern area where a plurality of circuit patterns are disposed in rows and columns and a plurality of dummy areas encompassing the circuit pattern area, a dummy pattern for measuring peel strength being formed in at least one of the dummy areas;
separating at least one of the dummy areas; and
measuring peel strength of the dummy pattern formed in the separated dummy area.

### Claim 2 (depends on 1)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 1, wherein, in the measuring of the peel strength of the dummy pattern, a remaining portion of the separated dummy area except for the dummy pattern is fixed, and the dummy pattern is peeled off while being pulled with a measuring machine to measure the peel strength of the dummy pattern.

### Claim 3 (depends on 1)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 1, wherein, in the separating of the dummy areas, the dummy areas are separated along a cutting line formed around the dummy areas.

### Claim 4 (depends on 1)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 1, wherein, in the providing of the metal-bonded ceramic substrate, the dummy pattern is disposed to cross a central portion of the dummy area.

### Claim 5 (depends on 1)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 1, wherein, in the providing of the metal-bonded ceramic substrate, the dummy pattern is formed in a bar shape.

### Claim 6 (depends on 1)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 1, wherein, in the providing of the metal-bonded ceramic substrate, the dummy pattern has a length of 100 mm or more and a width of 2 mm or more.

### Claim 7 (depends on 3)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 3, wherein, in the providing of the metal-bonded ceramic substrate, a first cutting line is formed between the circuit patterns, and between the circuit pattern and the dummy area.

### Claim 8 (depends on 3)

The method for measuring peel strength of a metal-bonded ceramic substrate of claim 3, wherein, in the providing of the metal-bonded ceramic substrate, a second cutting line is formed on both sides of the dummy area, and is a portion corresponding to an extension line of a boundary between the circuit pattern and the dummy area.

### Claim 9

A method for manufacturing a metal-bonded ceramic substrate, comprising:
providing a ceramic material; and
forming a plurality of circuit patterns in rows and columns on at least one surface of the ceramic material and forming a dummy pattern in at least one of a plurality of dummy areas encompassing an area where the circuit patterns are formed,
wherein in the forming of the dummy pattern, when the circuit pattern is formed in the area where the circuit patterns are formed, the dummy pattern for measuring peel strength is formed together in at least one of the plurality of dummy areas.

### Claim 10 (depends on 9)

The method for manufacturing a metal-bonded ceramic substrate of claim 9, wherein, in the forming of the dummy pattern, the dummy pattern is disposed to cross a central portion of the dummy area.

### Claim 11 (depends on 9)

The method for manufacturing a metal-bonded ceramic substrate of claim 9, wherein, in the forming of the dummy pattern, the dummy pattern is formed in a bar shape.

### Claim 12 (depends on 9)

The method for manufacturing a metal-bonded ceramic substrate of claim 9, wherein, in the forming of the dummy pattern, the dummy pattern has a length of 100 mm or more and a width of 2 mm or more.

### Claim 13 (depends on 9)

The method for manufacturing a metal-bonded ceramic substrate of claim 9, wherein the forming of the dummy pattern comprises:
bonding a metal layer to at least one surface of the ceramic material; and
forming the circuit patterns and the dummy pattern by etching the metal layer.

### Claim 14 (depends on 13)

The method for manufacturing a metal-bonded ceramic substrate of claim 13, wherein the forming of the circuit patterns and the dummy pattern comprises:
forming a photoresist pattern on an upper surface of the metal layer; and
etching the metal layer by using the photoresist pattern as an etching mask.

### Claim 15

A metal-bonded ceramic substrate including metal layers bonded to a surface of the metal-bonded ceramic substrate to form a plurality of circuit patterns disposed in rows and columns, wherein, when the circuit patterns are formed, a dummy pattern for measuring peel strength is formed together in at least one of a plurality of dummy areas encompassing an area where the circuit patterns are formed.

### Claim 16 (depends on 15)

The metal-bonded ceramic substrate of claim 15, wherein the dummy pattern is disposed to cross a central portion of the dummy area.

### Claim 17 (depends on 15)

The metal-bonded ceramic substrate of claim 15, wherein the dummy pattern is formed in a bar shape.

### Claim 18 (depends on 15)

The metal-bonded ceramic substrate of claim 15, wherein the dummy pattern has a length of 100 mm or more and a width of 2 mm or more.

### Claim 19 (depends on 15)

The metal-bonded ceramic substrate of claim 15, wherein a first cutting line is formed between the circuit patterns, and between the circuit pattern and the dummy area.

### Claim 20 (depends on 15)

The metal-bonded ceramic substrate of claim 15, wherein a second cutting line is formed on both sides of the dummy area, and is a portion corresponding to an extension line of a boundary between the circuit pattern and the dummy area.