# US 2026/0243025 A1 · Method and plant for making a cellulose-based web

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0243025 A1
- Document ID: US20260243025A1
- Status: Published application
- Kind: A1
- Application number: 19/471,147
- Filed: 2024-03-25
- Published: 2026-08-20
- Earliest claimed: 2023-03-31
- Assignees: Comas - Costruzioni Macchine Speciali - S.P.A.
- Applicants: Comas - Costruzioni Macchine Speciali - S.P.A.
- Inventors: Alessandro GRANZOTTO
- Web page: https://patentgrep.com/patent/US20260243025A1

## CPC

- D21H 19/52: Cellulose; Derivatives thereof
- D21H 27/00: Special paper not otherwise provided for, e.g. made by multi-step processes
- B27N 1/00: Pretreatment of moulding material
- B27N 3/02: from particles
- B27N 3/04: from fibres
- B27N 3/18: Auxiliary operations, e.g. preheating, humidifying, cutting-off
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)

## Abstract

A method for making a continuous web from cellulose-based material, includes a step of feeding a first quantity of at least one liquid and a second quantity of dry product in fibre, ground and/or powdered form into a mixing space of a kneader, where the dry product comprises cellulose. The method includes a step of mixing the second quantity of dry product with the first quantity of liquid in the kneader to obtain a mixture, followed by a step of forming a continuous web from the mixture. In particular, the step of forming a continuous web is accomplished by performing a first step of laminating the mixture via a first pair of rollers to obtain a laminated semi-finished product, and a second step of laminating the laminated semi-finished product via a second pair of rollers to obtain a continuous web.

## Claims

### Claim 1

A method for making a continuous web from cellulose-based material, comprising the following steps:
a step of feeding a first quantity of at least one liquid into a mixing space of a kneader;
a step of feeding a second quantity of at least one dry product into the mixing space of the kneader; the at least one dry product comprising cellulose in fibre and/or ground or powdered form;
a step of mixing the second quantity of dry product with the first quantity of liquid in the kneader to obtain a mixture, where said mixture has a moisture content of between 10% and 65%, preferably between 15% and 35%, more preferably between 20% and 30% and still more preferably, approximately 25%, and a cellulose content of between 40% and 80%, preferably between 40% and 65%, more preferably between 50% and 60% and still more preferably, approximately 55%;
a subsequent step of forming a continuous web from said mixture,
wherein said step of forming a continuous web comprises the following sub-steps:
performing a first step of laminating the mixture via a first pair of rollers to obtain a laminated semi-finished product;
performing a second step of laminating the laminated semi-finished product via a second pair of rollers to obtain a continuous web.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first and/or the second step of laminating is a step of vertical laminating.

### Claim 3 (depends on 1)

The method according to claim 1, comprising, between the steps of laminating, a step of scraping the semi-finished product off the first pair of rollers and, once it has been scraped off, feeding the semi-finished product, in particular by gravity, to the second pair of rollers

### Claim 4 (depends on 1)

The method according to claim 1, wherein the semi-finished product leaving the first pair of rollers, in particular, scraped off the first pair of rollers, has a flaky structure.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the mixture produced by the step of mixing has a sandy and/or grainy texture, with a particle size of between 1 and 6 mm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the mixture produced by the step of mixing is sent directly to the first pair of rollers, preferably by gravity feed or by a conveyor, where the first step of laminating can be carried out.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the mixture has a density of between 250 kg/m3 and 500 kg/m3, preferably between 300 kg/m3 and 500 kg/m3.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first quantity of at least one liquid comprises water and, preferably, at least one additional component preferably pre-mixed with the water, the additional liquid comprising one or more between glycerine, nicotine, lactic acid, propylene glycol, colourants and at least one binding agent.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the steps of feeding a second quantity of at least one dry product and of mixing the second quantity of dry product with the first quantity of liquid are carried out by feeding the dry product in two separate sub-steps, and mixing them between one sub-step and the other; preferably, the percentage of the dry product fed during the first sub-step being between 20% and 40%, more preferably approximately 30%, and the rest of the dry product being fed during the second sub-step.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising, after the second step of laminating, a step of multi-stage laminating, preferably horizontal, to reduce the thickness of the continuous web in controlled manner until reaching a calibrated thickness value.

### Claim 11 (depends on 1)

The method according to claim 1. further comprising a step of drying to obtain a dry continuous web.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the dry web has a density of between 0.60 g/cm3 and 1.1 g/cm3 , preferably between 0.75 g/cm3 and 0.90 g/cm3 .