# US 2026/0242973 A1 · Laminated structure and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242973 A1
- Document ID: US20260242973A1
- Status: Published application
- Kind: A1
- Application number: 19/642,847
- Filed: 2026-04-09
- Published: 2026-08-20
- Earliest claimed: 2023-11-06
- Assignees: Murata Manufacturing Co., Ltd.
- Applicants: Murata Manufacturing Co., Ltd.
- Inventors: Ryotaro NAMBA; Yusuke Arakawa
- Web page: https://patentgrep.com/patent/US20260242973A1

## CPC

- C23C 18/2086: {with use of organic or inorganic compounds other than metals, first}
- C25D 5/56: of plastics
- B32B 3/30: characterised by a layer formed with recesses or projections, e.g. {hollows, grooves, protuberances, ribs (apertured layer B32B3/266; layer with cavities or internal voids B32B3/26)}
- B32B 15/08: of synthetic resin
- C23C 18/1653: {Two or more layers with at least one layer obtained by electroless plating and one layer obtained by electroplating}
- C23C 18/1689: {After-treatment}
- C23C 18/20: of organic surfaces, e.g. resins
- C23C 18/2006: {by other methods than those of C23C18/22 - C23C18/30}
- C23C 18/204: {Radiation, e.g. UV, laser}
- C23C 18/22: Roughening, e.g. by etching
- C23C 18/24: using acid aqueous solutions
- C23C 18/285: {Sensitising or activating with tin based compound or composition}
- C23C 18/30: Activating {or accelerating or sensitising with palladium or other noble metal}
- C23C 18/32: Coating with nickel, cobalt or mixtures thereof with phosphorus or boron (C23C18/50 takes precedence)
- C23C 18/38: Coating with copper
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23F 17/00: Multi-step processes for surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by subclass C21D or C22F or class C25 (coating for obtaining at least two superposed coatings either by methods not provided for in a single one of main groups C23C2/00 - C23C26/00, or by combinations of methods providedfor in subclasses C23C and C25D, C23C28/00)
- C25D 3/38: of copper
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 5/617: {Crystalline layers}
- C25D 7/00: Electroplating characterised by the article coated
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A laminated structure is provided that can be manufactured without using any chemical liquid with a strong oxidizing power and that has high adhesion between a resin substrate and a metal layer. The laminated structure includes a resin substrate including a substrate body and a modified layer that covers a surface of the substrate body; and a metal layer that covers a surface of the modified layer. A surface of the modified layer has an oxygen element concentration of 17 atom % or more and 30 atom % or less. In a sectional view, the modified layer has a needle-like structure on the surface.

## Claims

### Claim 1

A laminated structure comprising:
a resin substrate including a substrate body and a modified layer that covers a surface of the substrate body; and
a metal layer that covers a surface of the modified layer,
wherein the surface of the modified layer has an oxygen element concentration of 17 atom % or more and 30 atom % or less,
wherein, in a sectional view, the modified layer has a needle-like structure.

### Claim 2 (depends on 1)

The laminated structure according to claim 1, wherein the oxygen element concentration at the surface of the modified layer is higher than an oxygen element concentration of the substrate body.

### Claim 3 (depends on 1)

The laminated structure according to claim 1, wherein the modified layer has a thickness in the sectional view that is 10 nm or more and 5000 nm or less.

### Claim 4 (depends on 1)

The laminated structure according to claim 1, wherein the resin substrate contains one or more selected from the group consisting of an acrylonitrile-butadiene-styrene (ABS), a polycarbonate/acrylonitrile-butadiene-styrene (PC/ABS), an acrylonitrile-styrene-acrylate (ASA), a silicon-based composite rubber-acrylonitrile-styrene (SAS), a noryl, a polypropylene, a polycarbonate (PC), a polycarbonate-based alloy, an acrylonitrile-styrene, a polyacetate, a polylactic acid, a polystyrene, a polyamide, an aromatic polyamide, a polyethylene, a polyether ketone, a polyethylene terephthalate, a polybutylene terephthalate, a polysulfone, a polyether ether sulfone, a polyether imide, a modified polyphenylene ether, a polyphenylene sulfide, a polyphenylene oxide, a polyamide, a polyimide, a modified polyimide, an epoxy resin, a cycloolefin polymer, a polynorbornene, a perfluoroalkoxy fluorine polymer, a polytetrafluoroethylene, and a vinylidene fluoride, a vinyl resin, a phenol resin, a polyacetal, a nylon, a liquid crystal polymer, and copolymers of the polymers.

### Claim 5 (depends on 1)

The laminated structure according to claim 1, wherein the needle-like structure comprises a plurality of protrusions that each have an elongated shape.

### Claim 6 (depends on 5)

The laminated structure according to claim 5, wherein the elongated shape of the plurality of protrusions is in a longitudinal direction that is substantially perpendicular to the surface of the modified layer.

### Claim 7 (depends on 1)

The laminated structure according to claim 1, wherein the needle-like structure has an aspect ratio of a length to a width of 2 or more, and a length of at least 30 nanometers (nm).

### Claim 8 (depends on 1)

The laminated structure according to claim 1, wherein the metal layer contains one or more selected from the group consisting of Fe, V, Ni, Ti, Ca, Ag, Zn, Al, Mg, Rh, Pt, Au, Pd, Co, Mn, and Cu.

### Claim 9 (depends on 1)

The laminated structure according to claim 1, wherein the modified layer has a higher oxygen element concentration throughout than the substrate body.

### Claim 10 (depends on 1)

The laminated structure according to claim 1, wherein the surface of the substrate body is entirely covered with the modified layer.

### Claim 11 (depends on 1)

The laminated structure according to claim 1, wherein the metal layer comprises:
an electroless plating layer, and
an electrolytic plating layer that covers the electroless plating layer.

### Claim 12 (depends on 1)

The laminated structure according to claim 1, wherein the oxygen element concentration is an element concentration of oxygen defined by a total element concentration of oxygen, carbon, nitrogen, and copper at the surface of the modified layer as 100 atom %.

### Claim 13

A method for manufacturing a laminated structure, the method comprising:
treating a surface of a resin substrate to form a surface-treated resin substrate that includes a substrate body and a softened layer that covers the substrate body;
heat-treating the surface-treated resin substrate to cure the softened layer and form a modified layer;
dissolving a part of a surface of the modified layer to form a needle-like structure; and
forming a metal layer on a surface of the modified layer including the needle-like structure,
wherein the modified layer has an oxygen element concentration of 17 atom % or more and 30 atom % or less.

### Claim 14 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the treating of the surface of the resin substrate includes subjecting the surface of the resin substrate to one or more treatments selected from the group consisting of UV irradiation, plasma treatment, corona treatment, and electron beam irradiation.

### Claim 15 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the treating of the surface of the resin substrate includes ultraviolet irradiation having an irradiation time of 10 seconds to 30 minutes and an irradiation intensity of 5 to 250 mW/cm2.

### Claim 16 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the heat-treating of the surface-treated resin substrate is performed at a temperature of 60° C. to 300° C.

### Claim 17 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the heat-treating of the surface-treated resin substrate is performed for a heating time of 1 minute to 120 minutes.

### Claim 18 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the forming of the metal layer comprises electroless plating and forming an electrolytic plating layer on the metal layer.

### Claim 19 (depends on 13)

The method for manufacturing the laminated structure according to claim 13, wherein the treating of the surface of the resin substrate further comprises introducing an oxygen-based functional group into a site where a chemical bond of a polymer chain in the resin substrate is broken to increase the oxygen element concentration of the modified layer.

### Claim 20 (depends on 13)

The method for manufacturing a laminated structure according to claim 13, wherein forming the metal layer comprises partially dissolving by immersion the surface of the modified layer in a plating bath for electroless plating to form the needle-like structure.