# US 2026/0242937 A1 · Method of forming thin film, and semiconductor substrate and semiconductor device fabricated using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242937 A1
- Document ID: US20260242937A1
- Status: Published application
- Kind: A1
- Application number: 19/159,341
- Filed: 2024-02-22
- Published: 2026-08-20
- Earliest claimed: 2023-02-23
- Applicants: Soulbrain Co., Ltd.
- Inventors: Jae Sun JUNG; Chang Bong YEON; Ji Hyun NAM; Deok-Hyun CHO
- Web page: https://patentgrep.com/patent/US20260242937A1

## CPC

- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C07F 11/00: Compounds containing elements of Groups 6 or 16 of the Periodic Table
- C23C 16/08: from metal halides
- C23C 16/14: Deposition of only one other metal element
- C23C 16/18: from metallo-organic compounds
- C23C 16/303: {Nitrides}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/44: characterised by the method of coating (C23C16/04 takes precedence)
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- C23C 16/455: characterised by the method used for introducing gases into reaction chamber or for modifying gas flows in reaction chamber
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45534: {Use of auxiliary reactants other than used for contributing to the composition of the main film, e.g. catalysts, activators or scavengers}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/56: After-treatment
- H10P 14/42: using a gas or vapour
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a method of forming a thin film, and a semiconductor substrate and semiconductor device fabricated using the same. According to the method of the present invention, by applying a predetermined reducing agent, even in the case of forming a thin film on a substrate having a highly integrated or complex structure, the thickness uniformity of a thin film may be greatly improved, impurities may be reduced, and the density and resistivity of the thin film may be improved, thereby effectively improving film quality.

## Claims

### Claim 1 (depends on 1)

A method of forming a thin film, comprising:
injecting a precursor compound into a chamber to adsorb the precursor compound onto a surface of a substrate; and injecting a reducing agent into the chamber to form a deposition film,
wherein the reducing agent comprises one or more selected from hydrogen iodide, hydrogen iodide water, hydrogen bromide, and hydrogen bromide water.
The method according to claim 1, wherein the reducing agent is 3 N to 15 N hydrogen iodide, a gas mixture containing 1 to 99% by weight of 3 N to 15 N hydrogen iodide and a residual amount (amount that makes a total amount 100% by weight) of an inert gas, or an aqueous solution mixture containing 0.5 to 70% by weight of 3 N to 15 N hydrogen iodide and a residual amount (amount that makes a total amount 100% by weight) of water,
wherein the inert gas is nitrogen, helium, or argon having a purity of 4 N to 9 N.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the thin film is a laminated film containing one or more selected from the group consisting of Al, Cu, Au, Mo, Ag, W, Pt, Ta, Co, Ru, and Ti.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the thin film is a nitride film, a metal film, or a selective thin film thereof formed on an entire substrate or a part of the substrate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the precursor compound is a molecule composed of one or more selected from the group consisting of Al, Cu, Au, Mo, Ag, W, Pt, Ta, Co, Ru, and Ti, and is a compound having a vapor pressure of more than 0.01 mTorr and 100 Torr or less at 25° C.

### Claim 6 (depends on 1)

The method according to claim 1, comprising injecting a precursor compound into a chamber to adsorb the precursor compound onto a surface of a substrate; performing first purging of the inside of the chamber with a purge gas; injecting the reducing agent into the chamber to reduce the adsorbed precursor compound; and performing second purging of the inside of the chamber with a purge gas.

### Claim 7 (depends on 1, 6)

The method according to claim 1 or 6, further comprising injecting a nitriding agent or an additional reaction gas into the chamber to form a nitride film.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the chamber is an ALD chamber, a CVD chamber, a PEALD chamber, or a PECVD chamber.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the substrate loaded into the chamber is heated to 100 to 800° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the thin film is an aluminum metal film, a copper metal film, a gold metal film, a molybdenum metal film, a silver metal film, a tungsten metal film, a platinum metal film, a tantalum metal film, a cobalt metal film, a ruthenium metal film, a titanium metal film, an aluminum nitride film, a copper nitride film, a gold nitride film, a molybdenum nitride film, a silver nitride film, a tungsten nitride film, a platinum nitride film, a tantalum nitride film, a cobalt nitride film, a ruthenium nitride film, or a titanium nitride film.

### Claim 11 (depends on 1)

A semiconductor substrate fabricated using the method according to claim 1.

### Claim 12 (depends on 11)

The semiconductor substrate according to claim 11, wherein the thin film has a multilayer structure of 2 or 3 layers.

### Claim 13 (depends on 11)

A semiconductor device comprising the semiconductor substrate according to claim 11.