# US 2026/0242936 A1 · Method for manufacturing transition metal dichalcogenide thin film having highly uniform three-dimensional hierarchical structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242936 A1
- Document ID: US20260242936A1
- Status: Published application
- Kind: A1
- Application number: 19/121,561
- Filed: 2023-07-04
- Published: 2026-08-20
- Earliest claimed: 2022-07-13
- Assignees: Korea Research Institute of Standards and Science
- Applicants: Korea Research Institute of Standards and Science
- Inventors: Sang Woo KANG; Ji Hun MUN; Jeong In SONG
- Web page: https://patentgrep.com/patent/US20260242936A1

## CPC

- C23C 16/02: Pretreatment of the material to be coated (C23C16/04 takes precedence)
- C23C 16/305: {Sulfides, selenides, or tellurides}
- C23C 16/01: on temporary substrates, e.g. substrates subsequently removed by etching
- C23C 16/0227: {by cleaning or etching}
- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/40: Oxides
- C23C 16/44: characterised by the method of coating (C23C16/04 takes precedence)
- C23C 16/448: characterised by the method used for generating reactive gas streams, e.g. by evaporation or sublimation of precursor materials
- C23C 16/4481: {by evaporation using carrier gas in contact with the source material (C23C16/4486 takes precedence)}
- C23C 16/455: characterised by the method used for introducing gases into reaction chamber or for modifying gas flows in reaction chamber
- C23C 16/56: After-treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present invention relates to a method for manufacturing a highly uniform three-dimensional transition metal dichalcogenide thin film, and more specifically, to a method for manufacturing a transition dichalcogenide thin film having a highly uniform three-dimensional hierarchical structure in which impurities contained in a transition metal-containing precursor act as seeds.

## Claims

### Claim 1

A method for manufacturing a three-dimensional transition metal dichalcogenide thin film, comprising supplying a chalcogen-containing precursor and an impurity-containing transition metal-containing precursor in a deposition chamber to deposit a two-dimensional transition metal dichalcogenide planar layer and a three-dimensional hierarchical structure on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising a step of reducing the surface energy of a substrate by treating the surface of the substrate prior to the deposition step.

### Claim 3 (depends on 1)

The method of claim 1, wherein the impurities include elements selected from a group consisting of carbon, oxygen, chlorine, copper, lead, zinc, cadmium, iron and combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the impurities act as seed elements for the formation of a three-dimensional structure.

### Claim 5 (depends on 1)

The method of claim 1, wherein the chalcogen-containing precursor is an S-containing organic compound or an S-containing inorganic compound.

### Claim 6 (depends on 1)

The method of claim 1, wherein the transition metal-containing precursor comprises a transition metal selected from a group consisting of Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Nb, Ta, Mo, W, Tc, Re, Ru, Os, Rh, Ir, Pt, Ag, Au, Cd, In, Tl, Sn, Pb, Sb, Bi, Zr, Te, Pd, Hf and combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate is selected from a group consisting of SiO2, Al2O3, HfO2, LiAlO3, MgO, Si, Ge, GaN, AlN, GaP, InP, GaAs, SiC, glass, quartz, sapphire, graphite, graphene, plastic, polymer, boron nitride (h-BN), and combinations thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the ratio between the transition metal-containing precursor and the chalcogen-containing precursor is 1:1 to 20.

### Claim 9 (depends on 1)

The method of claim 1, wherein the deposition is performed for 30 minutes to 10 hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein the deposition step includes steps of:
forming a two-dimensional planar transition metal dichalcogenide planar layer on the substrate;
growing a thin film in a vertical direction at a location of the two-dimensional planar transition metal dichalcogenide planar layer containing impurities at a faster decomposition rate of the transition metal-containing precursor and the chalcogen-containing precursor; and
forming a three-dimensional hierarchical structure of a thin film by accelerating the decomposition speed of a transition metal-containing precursor and a chalcogen-containing precursor by impurities contained thin film grown in the vertical direction.

### Claim 11 (depends on 2)

The method of claim 2, wherein surface treatment of the substrate is performed by a wet treatment method selected from a group consisting of a piranha solution treatment, a sulfuric acid (H2SO4) solution treatment, a hydrochloric acid (HCL) solution treatment, and an alkali metal hydroxide solution treatment; or a dry treatment method selected from a group consisting of an O2 plasma treatment and a heat treatment using water vapor.

### Claim 12 (depends on 1)

The method of claim 1, wherein the deposition step is performed at a temperature of 500° C. or lower.

### Claim 13 (depends on 1)

The method of claim 1, wherein the deposition step is performed using the chemical vapour deposition (CVD) method.

### Claim 14

A method for manufacturing a three-dimensional transition metal dichalcogenide thin film, comprising generating a two-dimensional transition metal dichalcogenide planar layer and a three-dimensionally hierarchical structure of a transition metal dichalcogenide thin film on the substrate for 30 minutes to 10 hours by supplying a chalcogen-containing precursor and a impurity-containing transition metal-containing precursor within a deposition chamber under a temperature of 500° C. or less and a pressure of 0.001 Torr to 760 Torr.

### Claim 15 (depends on 14)

The method of claim 14, wherein the ratio between the transition metal-containing precursor partial pressure and the chalcogen-containing precursor partial pressure is 1:1 to 20.