# US 2026/0242307 A1 · S-type glass fibers in gas generant compositions for improved combustion in pyrotechnic inflators

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242307 A1
- Document ID: US20260242307A1
- Status: Published application
- Kind: A1
- Application number: 19/054,437
- Filed: 2025-02-14
- Published: 2026-08-20
- Earliest claimed: 2025-02-14
- Assignees: Autoliv ASP, Inc.
- Applicants: Autoliv ASP, Inc.
- Inventors: Zayn RHODES; Ivan V. Mendenhall; Francois Peremarty; Steven Butler
- Web page: https://patentgrep.com/patent/US20260242307A1

## CPC

- C06B 23/001: {Fillers, gelling and thickening agents (e.g. fibres) , absorbents for nitroglycerine (binders, plasticisers for propellants C06B45/10; crosslinking or curing agents C06B45/10)}
- C06D 5/06: by reaction of two or more solids
- C06B 23/007: {Ballistic modifiers, burning rate catalysts, burning rate depressing agents, e.g. for gas generating}
- C06B 41/00: Compositions containing a nitrated metallo-organic compound
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})
- C06D: MEANS FOR GENERATING SMOKE OR MIST; GAS-ATTACK COMPOSITIONS; GENERATION OF GAS FOR BLASTING OR PROPULSION (CHEMICAL PART) (fuels C10)

## Abstract

Methods for improving combustion stability in a gas generant for an inflatable restraint system are provided. S-type glass fibers are introduced into a mixture comprising at least one fuel and at least one oxidizer to form the gas generant. Each S-type glass fiber comprises silicon dioxide at ≥about 60% by mass, aluminum oxide at ≥about 20% by mass, and magnesium oxide at ≥about 9% by mass, and has a thermal softening point temperature (Td) of greater than or equal to about 1,000° C. When the S-type glass fibers are absent, wherein the mixture exhibits flame extinguishment and/or reignition during combustion. However, combusting the gas generant comprising plurality of the S-type glass fibers is substantially free of flame extinguishment and/or reignition behavior and any associated pressure excursions. Gas generant compositions including the S-type glass fibers are also provided.

## Claims

### Claim 1

A method for improving combustion stability in a gas generant for an inflatable restraint system, the method comprising:
introducing a plurality of S-type glass fibers into a mixture comprising at least one fuel and at least one oxidizer to form the gas generant, wherein each S-type glass fiber comprises silicon dioxide at greater than or equal to about 60% by mass, aluminum oxide at greater than or equal to about 20% by mass, and magnesium oxide at greater than or equal to about 9% by mass, and has a thermal softening point temperature (Td) of greater than or equal to about 1,000° C., wherein the mixture exhibits flame extinguishment and/or reignition during combustion when the plurality of S-type glass fibers is absent, and the gas generant comprising the plurality of the S-type glass fibers is substantially free of flame extinguishment and/or reignition behavior and any associated pressure excursions during combustion.

### Claim 2 (depends on 1)

The method of claim 1, wherein an amount of S-type glass fibers in the gas generant after the introducing is less than or equal to about 10% by weight of the gas generant.

### Claim 3 (depends on 1)

The method of claim 1, wherein the amount of S-type glass fibers is greater than or equal to about 1% by weight to less than or equal to about 5% by weight of the gas generant.

### Claim 4 (depends on 2)

The method of claim 2, wherein the thermal softening point temperature (Td) of the plurality of S-type glass fibers is greater than or equal to about 1,300° C.

### Claim 5 (depends on 1)

The method of claim 1, further comprising combusting the gas generant, where the combusting is substantially completed in less than or equal to about 50 milliseconds.

### Claim 6 (depends on 5)

The method of claim 5, wherein the combusting of the gas generant occurs at a temperature of −40° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the at least one fuel comprises a primary fuel and a secondary fuel comprising melamine nitrate at greater than or equal to about 1% by weight to less than or equal to about 20% by weight of the gas generant and the at least one oxidizer comprises a primary oxidizer and at least one secondary oxidizer comprising potassium perchlorate at greater than or equal to about 5% by weight to less than or equal to about 20% by weight of the gas generant, wherein during the combusting, the gas generant exhibits (i) a linear burn rate of greater than or equal to about 20 mm/second at 20 MPa, (ii) a burn rate slope is less than or equal to about 0.45, (iii) a maximum flame temperature at combustion (Tc) is less than or equal to about 2100K.

### Claim 8 (depends on 7)

The method of claim 7, wherein the primary fuel comprises guanidine nitrate at greater than or equal to about 20% by weight to less than or equal to about 60% by weight of the gas generant and the primary oxidizer comprises basic copper nitrate at greater than or equal to about 20% by weight to less than or equal to about 60% by weight of the gas generant.

### Claim 9 (depends on 1)

The method of claim 1, wherein the plurality of S-type glass fibers are milled and each S-type glass fiber of the plurality of S-type glass fibers has an average aspect ratio (AR) ranging from about 10:1 to about 20:1 and has a length of greater than or equal to about 60 micrometers to less than or equal to about 260 micrometers.

### Claim 10 (depends on 1)

The method of claim 1, wherein each S-type glass fiber of the plurality of S-type glass fibers has silicon dioxide at greater than or equal to about 61% by mass, aluminum oxide at greater than or equal to about 23% by mass, magnesium oxide at greater than or equal to about 9% by mass, boron oxide at greater than or equal to about 4% by mass, calcium oxide at about 0.05% by mass, cumulative other oxides at about 0.06% by mass, and a balance impurities, which has a modulus of elasticity of greater than or equal to about 85 MPa, a tensile strength of greater than or equal to about 4,500 MPa, a percent elongation of greater than or equal to about 5%, and a density of greater than or equal to about 2,400 kg/m3.

### Claim 11

A gas generant composition comprising:
a primary fuel;
melamine nitrate at greater than or equal to about 1% by weight to less than or equal to about 20% by weight of the gas generant composition;
a primary oxidizer;
potassium perchlorate at greater than or equal to about 5% by weight to less than or equal to about 20% by weight of the gas generant composition; and
a plurality of S-type glass fibers, each S-type glass fiber comprising silicon dioxide at greater than or equal to about 60% by mass, aluminum oxide at greater than or equal to about 20% by mass, and magnesium oxide at greater than or equal to about 9% by mass and having a thermal softening point temperature (Td) of greater than or equal to about 1,000° C., wherein during combustion of the gas generant composition: (i) a linear burn rate is greater than or equal to about 20 mm/second at 20 MPa, (ii) a burn rate slope is less than or equal to about 0.45, and (iii) combustion is substantially free of extinguishment or reignition behavior and any associated pressure excursions.

### Claim 12 (depends on 11)

The gas generant composition of claim 11, wherein the plurality of S-type glass fibers is present at greater than or equal to about 1% and less than about 10% by weight of the gas generant composition.

### Claim 13 (depends on 11)

The gas generant composition of claim 11, wherein the primary fuel comprises guanidine nitrate and is present at greater than or equal to about 20 to less than or equal to about 60 weight % of the total gas generant composition, and the primary oxidizer comprises basic copper nitrate that is present at greater than or equal to about 20 to less than or equal to about 60 weight % of the total gas generant composition.

### Claim 14 (depends on 11)

The gas generant composition of claim 11, wherein the amount of S-type glass fibers is greater than or equal to about 1% by weight to less than or equal to about 5% by weight of the gas generant.

### Claim 15 (depends on 11)

The gas generant composition of claim 11, wherein the thermal softening point temperature (Td) of the plurality of S-type glass fibers is greater than or equal to about 1,300° C.

### Claim 16 (depends on 11)

The gas generant composition of claim 11, wherein (ii) the burn rate slope is less than or equal to about 0.42 and during combustion of the gas generant composition: (iv) a maximum flame temperature at combustion (Tc) is less than or equal to about 2100K.

### Claim 17 (depends on 11)

The gas generant composition of claim 11, wherein the plurality of S-type glass fibers are milled and each S-type glass fiber of the plurality of S-type glass fibers has an average aspect ratio (AR) ranging from about 10:1 to about 20:1 and has a length of greater than or equal to about 6 micrometers to less than or equal to about 260 micrometers.

### Claim 18 (depends on 11)

The gas generant composition of claim 11, wherein each S-type glass fiber of the plurality of S-type glass fibers has silicon dioxide at greater than or equal to about 61% by mass, aluminum oxide at greater than or equal to about 23% by mass, magnesium oxide at greater than or equal to about 9% by mass, boron oxide at greater than or equal to about 4% by mass, calcium oxide at about 0.05% by mass, cumulative other oxides at about 0.06% by mass, and a balance impurities, which has a modulus of elasticity of greater than or equal to about 85 MPa, a tensile strength of greater than or equal to about 4,500 MPa, a percent elongation of greater than or equal to about 5%, and a density of greater than or equal to about 2,400 kg/m3.

### Claim 19 (depends on 11)

The gas generant composition of claim 11, wherein the burn rate slope is less than or equal to about 0.42.

### Claim 20

A gas generant composition comprising:
a primary fuel comprising guanidine nitrate at greater than or equal to about 20 to less than or equal to about 60 weight % of the total gas generant composition;
melamine nitrate at greater than or equal to about 1% by weight to less than or equal to about 20% by weight of the gas generant composition;
a primary oxidizer comprising basic copper nitrate at greater than or equal to about 20 to less than or equal to about 60 weight % of the total gas generant composition;
potassium perchlorate at greater than or equal to about 5% by weight to less than or equal to about 20% by weight of the gas generant composition; and
a plurality of S-type glass fibers at greater than 0 to less than or equal to about 10 weight % of the total gas generant composition, each S-type glass fiber comprising silicon dioxide at greater than or equal to about 60% by mass, aluminum oxide at greater than or equal to about 20% by mass, and magnesium oxide at greater than or equal to about 9% by mass and having a thermal softening point temperature (Td) of greater than or equal to about 1,000° C., and
one or more additives cumulatively present at greater than or equal to 0% to less than or equal to about 10% by weight of the gas generant composition, wherein during combustion of the gas generant composition: (i) a linear burn rate is greater than or equal to about 20 mm/second at 20 MPa, (ii) a burn rate slope is less than or equal to about 0.45, (iii) a maximum flame temperature at combustion (Tc) of less than or equal to about 2100K, and (iv) combustion is substantially free of extinguishment or reignition behavior and any associated pressure excursions.