# US 2026/0242296 A1 · Composition of flexible ceramic nanofibers for thermal insulation applications and method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242296 A1
- Document ID: US20260242296A1
- Status: Published application
- Kind: A1
- Application number: 19/217,403
- Filed: 2025-05-23
- Published: 2026-08-20
- Earliest claimed: 2025-02-19
- Inventors: Jazze Marie Gorman
- Web page: https://patentgrep.com/patent/US20260242296A1

## CPC

- C04B 35/62259: {Fibres based on titanium oxide}
- C04B 35/632: Organic additives
- C04B 35/63488: {Polyethers, e.g. alkylphenol polyglycolether, polyethylene glycol [PEG], polyethylene oxide [PEO]}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 38/04: by dissolving-out added substances
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/441: Alkoxides, e.g. methoxide, tert-butoxide
- C04B 2235/5212: Organic
- C04B 2235/5232: Silica or silicates other than aluminosilicates, e.g. quartz
- C04B 2235/6562: Heating rate
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2235/9607: Thermal properties, e.g. thermal expansion coefficient
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The present disclosure relates to a method (200) for preparing flexible ceramic nanofibers for thermal insulation applications, comprising preparing a titanium precursor solution by dissolving tetra butyl titanate (TBOT) in anhydrous methanol. The method (200) comprising adding glacial acetic acid in a particular ratio to tetra butyl titanate (TBOT) while stirring. The method (200) comprising adding acetylacetone in a particular ratio to tetra butyl titanate (TBOT) and stirring vigorously. The method (200) comprising preparing a silica precursor solution by dissolving tetraethyl orthosilicate (TEOS) in anhydrous methanol in a particular ratio. The method (200) comprising adding polyethylene oxide (PEO) and heating mixture. The method (200) comprising mixing the titanium precursor solution and silica precursor solutions and constantly stirring to form a TiO2/SiO2 electrospinning precursor solution. The method (200) comprising electrospinning the precursor solution to form nanofibrous membranes under the pre-determined conditions. The method (200) comprising sintering the nanofibrous membranes to obtain porous ceramic nanofiber membranes.

## Claims

### Claim 1

A composition of flexible ceramic nanofibers for thermal insulation applications, the composition comprising:
tetraethyl orthosilicate (TEOS) as a silica precursor;
tetra butyl titanate (TBOT) as a titanium precursor;
polyethylene oxide (PEO) as a porogen;
glacial acetic acid as a catalyst for hydrolysis and condensation reactions; and
acetylacetone as a chelating agent for precursor stabilization.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the composition comprising:
a 208.33 Mw of tetraethyl orthosilicate (TEOS);
a 340.32 Mw of tetra butyl titanate (TBOT);
a 1,000,000 Mw of polyethylene oxide (PEO);
a 60 Mw of glacial acetic acid; and
a 100 Mw of acetylacetone.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the composition also comprises anhydrous methanol (CH3OH).

### Claim 4 (depends on 3)

The composition of claim 3, wherein the composition also comprises a 32 Mw of anhydrous methanol (CH3OH).

### Claim 5 (depends on 1)

The composition of claim 1, wherein the composition also comprises deionized water.

### Claim 6 (depends on 5)

The composition of claim 5, wherein the composition also comprises an 18 Mw of deionized water.

### Claim 7

A method for preparation of flexible ceramic nanofibers for thermal insulation applications, the method comprising:
preparing a titanium precursor solution by dissolving tetra butyl titanate (TBOT) in anhydrous methanol;
adding glacial acetic acid in a particular ratio to tetra butyl titanate (TBOT) while stirring;
adding acetylacetone in a particular ratio to tetra butyl titanate (TBOT) and stirring vigorously;
preparing a silica precursor solution by dissolving tetraethyl orthosilicate (TEOS) in anhydrous methanol in a particular ratio;
adding polyethylene oxide (PEO) and heating mixture;
mixing the titanium precursor solution and silica precursor solutions and constantly stirring to form a TiO2/SiO2 electrospinning precursor solution;
electrospinning the precursor solution to form nanofibrous membranes under the pre-determined conditions; and
sintering the nanofibrous membranes to obtain porous ceramic nanofiber membranes.

### Claim 8 (depends on 7)

The method of claim 7, wherein the glacial acetic acid is added in a molar ratio of 3:1 to tetra butyl titanate (TBOT).

### Claim 9 (depends on 7)

The method of claim 7, wherein the acetylacetone is added in a 1:1 molar ratio to tetra butyl titanate (TBOT).

### Claim 10 (depends on 7)

The method of claim 7, wherein the tetraethyl orthosilicate (TEOS) is dissolved in anhydrous methanol in a molar ratio of 0.2 relative to tetra butyl titanate (TBOT).

### Claim 11 (depends on 8)

The method of claim 8, wherein a 3% v/v of glacial acetic acid is added to the tetraethyl orthosilicate (TEOS) dissolved in anhydrous methanol.

### Claim 12 (depends on 7)

The method of claim 7, wherein the polyethylene oxide (PEO) at 1% w/v concentration is added to tetraethyl orthosilicate (TEOS).

### Claim 13 (depends on 7)

The method of claim 7, wherein the TiO2/SiO2 electrospinning precursor solution have viscosity between 500 and 2000 cp.

### Claim 14 (depends on 7)

The method of claim 7, wherein the process of sintering further includes:
heating to 600° C. at a rate of 1° C./min;
maintaining the membranes at 600° C. for 2 hours; and
cooling to room temperature to obtain porous ceramic nanofiber membranes.

### Claim 15 (depends on 7)

The method of claim 7, wherein the electrospinning of the precursor solution is performed at ambient temperature of approximately 25° C.

### Claim 16 (depends on 7)

The method of claim 7, wherein the electrospinning of the precursor solution is performed at relative humidity of 45%-55%.

### Claim 17 (depends on 7)

The method of claim 7, wherein the electrospinning of the precursor solution is performed at spinning voltage of 15 kV.

### Claim 18 (depends on 7)

The method of claim 7, wherein the electrospinning of the precursor solution is performed using needle gauge of 25G and syringe advancement rate of 2 mL/h, with a 20 cm distance between needle and collector.

### Claim 19 (depends on 7)

The method of claim 7, wherein the electro-spined precursor solution is collected by a roller receiver.

### Claim 20 (depends on 7)

The method of claim 7, wherein the method also includes performing calcination to decompose polyethylene oxide (PEO) in the final ceramic structure.