# US 2026/0242243 A1 · Precursor, and method for producing positive electrode active material for lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0242243 A1
- Document ID: US20260242243A1
- Status: Published application
- Kind: A1
- Application number: 18/993,960
- Filed: 2023-07-14
- Published: 2026-08-20
- Earliest claimed: 2022-07-15
- Assignees: Tanaka Chemical Corporation
- Applicants: Tanaka Chemical Corporation
- Inventors: Kenji TAKAMORI; Tomoya KURODA
- Web page: https://patentgrep.com/patent/US20260242243A1

## CPC

- C01G 53/84: Hydroxides
- C01G 53/00: Compounds of nickel
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/44: containing manganese
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/502: containing lithium and cobalt
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/54: one element only
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/21: Attrition-index or crushing strength of granulates
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a precursor of a positive electrode active material for a lithium secondary battery, the precursor including a metal composite compound containing at least one metal element selected from the group consisting of Ni, Co, and Mn, and satisfying all of the following requirements (1) to (3): (1) An average particle strength is 10 MPa or more and less than 45 MPa; (2) An average particle diameter D50 is more than 4 μm and equal to or less than 20 μm; (3) Both a moisture content and a sulfate radical content are 1% by mass or less with respect to the total mass of the precursor.

## Claims

### Claim 1

A precursor of a positive electrode active material for a lithium secondary battery, said precursor comprising a metal composite compound containing at least one metal element selected from the group consisting of Ni, Co, and Mn, and satisfying all of the following requirements (1) to (3):
(1) An average particle strength is 10 MPa or more and less than 45 MPa;
(2) An average particle diameter D50 is more than 4 μm and equal to or less than 20 μm;
(3) Both a moisture content and a sulfate radical content are 1% by mass or less with respect to the total mass of said precursor.

### Claim 2 (depends on 1)

The precursor according to claim 1, wherein said metal composite compound is represented by the following composition formula (I):
(said composition formula (I) satisfies 0≤x≤0.5, 0≤y≤0.5, 0≤w≤0.5, 0≤x+y+w<1.0≤z≤3, −0.5≤α≤2, and α−z<2, and M is one or more elements selected from the group consisting of Fe, Cu, Ti, Mg, Al, Zn, Sn, Zr, Nb, Ga, W, Mo, B, and Si.)

### Claim 3 (depends on 1)

The precursor according to claim 1, which has a standard deviation of particle strength of 1 MPa or more and 9 MPa or less.

### Claim 4 (depends on 1)

The precursor according to claim 1, which has a BET specific surface area of 2 m2/g or more and 50 m2/g or less.

### Claim 5 (depends on 1)

The precursor according to claim 1, which has a tap density of 1.0 g/cm3 or more and 3.5 g/cm3 or less.

### Claim 6 (depends on 1)

A method for producing a positive electrode active material for a lithium secondary battery,
the method comprising
a mixing step for mixing the precursor of claim 1 with a lithium compound, and
a calcination step for calcining the obtained mixture at a temperature of 500° C. or more and 1,000° C. or less in an oxygen-containing atmosphere.