# US 2026/0241668 A1 · Aluminum-plated stainless steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0241668 A1
- Document ID: US20260241668A1
- Status: Published application
- Kind: A1
- Application number: 19/152,776
- Filed: 2024-01-19
- Published: 2026-08-20
- Earliest claimed: 2023-01-31
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Satoshi SAMPEI; Shinichi TERAOKA; Chikara ITO; Akinori KAWANO; Tooru MATSUHASHI; Manabu OKU
- Web page: https://patentgrep.com/patent/US20260241668A1

## CPC

- B32B 15/012: {one layer being formed of an iron alloy or steel, another layer being formed of aluminium or an aluminium alloy}
- C22C 21/00: Alloys based on aluminium
- C22C 21/02: with silicon as the next major constituent
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/30: with cobalt
- C22C 38/32: with boron
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/50: with titanium or zirconium
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 9/46: for sheet metals
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

An aluminum-plated stainless steel sheet: includes a stainless steel sheet, an aluminum-plating layer, and an alloy phase between the stainless steel sheet and the aluminum-plating layer; and contains predetermined components. The aluminum-plating layer contains 1 to 10% of Fe, 3 to 18% of Si, 0.1 to 1% of Cr, and a balance of Al, and contains a eutectic Si and an intermetallic compound phase consisting of Al—Si—Fe. An area ratio of the eutectic Si is 30% or less in a cross section of the aluminum-plating layer in a sheet thickness direction excluding a 1-μm-topmost layer, an area ratio of the intermetallic compound phase consisting of Al—Si—Fe is 5% or less in a cross section of the aluminum-plating layer, a thickness of the alloy phase is 15 μm or less, and a non-plated area ratio is 1.0% or less.

## Claims

### Claim 1

An aluminum-plated stainless steel sheet, comprising:
a stainless steel sheet;
an aluminum-plating layer on a surface of the stainless steel sheet; and
an alloy phase between the stainless steel sheet and the aluminum-plating layer, wherein
the stainless steel sheet contains, by mass %, 0.02% or less of C, 0.02 to 0.50% of Si, 0.02 to 1.00% of Mn, 0.040% or less of P, 0.0002 to 0.0100% of S, 0.004 to 0.100% of Al, 10.0 to 25.0% of Cr, 0.02 to 0.40% of Ti, 0.05% or less of N, and a balance of Fe and an impurity element,
the aluminum-plating layer contains, by mass %, 1 to 10% of Fe, 3 to 18% of Si, 0.01 to 0.05% of Cr, and a balance of Al,
the aluminum-plating layer contains a eutectic Si and an intermetallic compound phase consisting of Al—Si—Fe,
an area ratio of the eutectic Si is 30% or less in a cross section in a rolling direction and in a sheet thickness direction excluding a 1-μm-topmost layer of the aluminum-plating layer,
an area ratio of the intermetallic compound phase consisting of Al—Si—Fe is 5% or less in a cross section in the rolling direction and in the sheet thickness direction of the aluminum-plating layer,
a thickness of the alloy phase is 15 m or less, and
a non-plated area ratio is 1.0% or less.

### Claim 2 (depends on 1)

The aluminum-plated stainless steel sheet according to claim 1, wherein in place of a part of the Fe, the stainless steel sheet further contains, by mass %, one or more of 0.02 to 0.40% of Ni, 0.02 to 1.40% of Mo, and 0.02 to 1.40% of Cu.

### Claim 3 (depends on 1)

The aluminum-plated stainless steel sheet according to claim 1, wherein in place of a part of the Fe, the stainless steel sheet further contains, by mass %, one or more of 0.0001 to 0.0020% of B, 1.00% or less of V, 0.005 to 0.50% of Zr, 0.030% or less of Ga, 0.001 to 0.10% of REM, 0.10% or less of Ta, 0.005 to 0.50% of Sn, 1.00% or less of W, 1.00% or less of Co, and 0.005 to 0.50% of Sb.

### Claim 4 (depends on 2)

The aluminum-plated stainless steel sheet according to claim 2, wherein in place of a part of the Fe, the stainless steel sheet further contains, by mass %, one or more of 0.0001 to 0.0020% of B, 1.00% or less of V, 0.005 to 0.50% of Zr, 0.030% or less of Ga, 0.001 to 0.10% of REM, 0.10% or less of Ta, 0.005 to 0.50% of Sn, 1.00% or less of W, 1.00% or less of Co, and 0.005 to 0.50% of Sb.