# US 2026/0241644 A1 · Method for producing composite fiber materials with a particularly low degree of fiber warpage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0241644 A1
- Document ID: US20260241644A1
- Status: Published application
- Kind: A1
- Application number: 18/870,260
- Filed: 2022-11-25
- Published: 2026-08-20
- Earliest claimed: 2022-05-30
- Assignees: Bond-Laminates GmbH
- Applicants: Bond-Laminates GmbH
- Inventors: Stefan SEIDEL
- Web page: https://patentgrep.com/patent/US20260241644A1

## CPC

- B29C 70/22: oriented in at least two directions forming a two-dimensional [2D] structure
- C08J 5/08: glass fibres
- B29C 70/003: {characterised by the matrix material, e.g. material composition or physical properties}
- B29C 70/504: {using rollers or pressure bands (for corrugating B29C53/22)}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2105/0845: {Woven fabrics}
- B29K 2309/08: Glass
- C08J 2323/12: Polypropene
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The invention relates to a method for producing fiber composite materials comprising a thermoplastic molding composition A and at least one layer of reinforcing fibers B. The thermoplastic molding composition A is embedded into the at least one layer of reinforcing fibers B as a matrix, wherein the embedding is realized by moving the molding composition relative to the reinforcing fibers B within a consolidating step, in which the reinforcing fibers B remain immobile except for a one-dimensional production advancing movement, the thermoplastic molding composition A has at least one chemically reactive functionality, and the surface of the reinforcing fibers B is treated with a sizing, and the concentration of functional groups for the chemically reactive functionalities of the molding composition A is at least 0.3 mol %.

## Claims

### Claim 1

A process for producing a fiber composite material comprising a thermoplastic molding composition A as polymer matrix M, reinforcing fibers B, comprising the steps of
i) providing at least one fabric F in the form of a weave composed of reinforcing fibers B treated with a silane size,
ii) providing a thermoplastic molding composition A that serves as matrix M, having at least 0.3 mol %, based on component A, of a chemically reactive functionality in the form of functional monomers,
iii) optionally incorporating at least one additive C into the thermoplastic molding composition A,
iv) introducing the thermoplastic molding composition A that serves as matrix M into the at least one fabric F by embedding the thermoplastic molding composition A into the reinforcing fibers B by means of a relative movement in which the reinforcing fibers B remain immobile apart from a continuous or discontinuous one-dimensional production feed, and consolidating this composite composed of at least one fabric F and the matrix M,
v) reacting the chemically reactive functionalities of the thermoplastic molding composition A with the polar groups at the surface of the reinforcing fibers B that have been treated with the silane size,
vi) cooling the fiber composite material, and optionally further process steps,
wherein the chemically reactive functionality of the thermoplastic molding composition A is based on components selected from the group of maleic anhydride, N-phenylmaleimide, and glycidyl (meth)acrylate, and steps iv) to vi) are conducted at a temperature of at least 150° C., and steps v) to vi) by pressing under elevated pressure.

### Claim 2 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the thermoplastic molding composition A is based on amorphous or semicrystalline plastic.

### Claim 3 (depends on 2)

The process for producing a thermoplastic fiber composite material as claimed in claim 2, characterized in that the thermoplastic molding composition A is based on at least one polymer from the group of polyolefins, polyamides, thermoplastic elastomers, polycarbonates, polybutadiene terephthalates, polylactides, polyphenylene sulfides and styrene copolymers.

### Claim 4 (depends on 3)

The process for producing a thermoplastic fiber composite material as claimed in claim 3, characterized in that the polyolefin used is polypropylene.

### Claim 5 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that reinforcing fibers B treated with a silane size are used.

### Claim 6 (depends on 5)

The process for producing a thermoplastic fiber composite material as claimed in claim 5, characterized in that reinforcing fibers B used are glass fibers.

### Claim 7 (depends on 6)

The process for producing a thermoplastic fiber composite material as claimed in claim 6, characterized in that the glass fibers used as reinforcing fibers B have silanol groups on the surface as a chemically reactive functionality.

### Claim 8 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the process, especially process steps iv) and v) or optionally also process step vi), is conducted on a double belt press, interval heating press or on a static press.

### Claim 9 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the temperature in the production of the fiber composite material is at least 150° C., preferably at least 200° C. and more preferably at least 250° C.

### Claim 10 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the dwell time in the production of the fiber composite material at temperatures of at least 200° C. is not more than 10 minutes, preferably not more than 5 minutes, more preferably not more than 2 minutes and in particular not more than 1 minute.

### Claim 11 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the relative movement of the thermoplastic molding composition A in relation to the reinforcing fibers B is achieved by the fixing of the reinforcing fibers B in the direction of relative movement.

### Claim 12 (depends on 11)

The process for producing a thermoplastic fiber composite material as claimed in claim 11, characterized in that the fixing of the reinforcing fibers B upstream and downstream of the region in which the movement of the thermoplastic molding composition A is created by a surface pressure >10 bar at a temperature of at least 10° C. above the crystallite melting temperature or glass transition temperature in the case of amorphous thermoplastics is effected by means of mechanical clamping, winding or with the aid of securing elements, and this hold is maintained by application of opposing force under constant strain.

### Claim 13 (depends on 11)

The process for producing a thermoplastic fiber composite material as claimed in claim 11, characterized in that the reinforcing fibers B are fixed in position such that the strain in longitudinal direction prevents movement in any spatial direction.

### Claim 14 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the reinforcing fibers B in the form of weaves are fixed and kept under tension by an automatic draw system in roll form on retarded unwinding drums upstream of the region of application of temperature and pressure, and as a consolidated stack downstream of the region of application of temperature and pressure.

### Claim 15 (depends on 1)

The process for producing a thermoplastic fiber composite material as claimed in claim 1, characterized in that the chemically reactive functionality of the thermoplastic molding composition A is based on maleic anhydride, and steps iv) to vi) are conducted at a temperature of at least 150° C., and steps v) to vi) are conducted by pressing under elevated pressure, and the thermoplastic molding composition contains 90% to 99.7% by weight of polypropylene and 0.1% to 10% by weight of maleic anhydride, and also 0% to 40% by weight, preferably 0.1% to 25% by weight, of at least one additive C.