# US 2026/0241626 A1 · Method and manufacturing system for producing molded product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0241626 A1
- Document ID: US20260241626A1
- Status: Published application
- Kind: A1
- Application number: 19/539,053
- Filed: 2026-02-13
- Published: 2026-08-20
- Earliest claimed: 2025-02-20
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Yoshiki NAKASHIMA; Hideki TANAKA; Akio FUKASE; Mami HIJIKATA
- Web page: https://patentgrep.com/patent/US20260241626A1

## CPC

- B29C 35/0288: {Controlling heating or curing of polymers during moulding, e.g. by measuring temperatures or properties of the polymer and regulating the process (controlling or regulating chemical, physical or physico- chemical processes in general B01J19/0006)}
- B29C 45/7207: {of the moulded articles}
- B29C 45/0001: {characterised by the choice of material}
- B29C 45/78: of temperature
- B29C 71/02: Thermal after-treatment {(B29C71/0063 and B29C71/0072 take precedence)}
- B29C 2945/76531: Temperature
- B29C 2945/76769: Moulded articles
- B29K 2001/08: {Cellulose derivatives}
- B29K 2001/12: {Cellulose acetate}
- B29K 2001/14: {Cellulose acetate-butyrate}
- B29K 2001/18: {Cellulose nitrate}
- B29K 2003/00: Use of starch or derivatives as moulding material
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for producing a molded product includes: a first step of molding a material containing a cellulose derivative into a molded body, and a second step of performing temperature control in which a molded product is produced by maintaining the molded body produced in the first step within a predetermined temperature range for a predetermined time t, wherein, when the phase transition point of the molded body is A(°C), the temperature range in the second step is A−10°C or more and A+50°C or less.

## Claims

### Claim 1

A method for producing a molded product comprising:
molding a material containing a cellulose derivative into a molded body, and
performing temperature control on the molded body produced by the molding within a predetermined temperature range for a predetermined time t,
wherein, when a phase transition point of the molded body is A (°C), the temperature range is from A−10°C to A+50°C.

### Claim 2 (depends on 1)

The method for producing the molded product according to claim 1, wherein the time t is a duration longer than the time corresponding to an endothermic peak of the molded body.

### Claim 3 (depends on 1)

The method for producing the molded product according to claim 1, wherein the time t is a duration at which a heat absorption amount of the molded body is 0.0001 W/g or less.

### Claim 4 (depends on 1)

The method for producing the molded product according to claim 1, wherein the time t is 150 seconds or more and 3500 seconds or less.

### Claim 5 (depends on 1)

The method for producing the molded product according to claim 1, wherein the temperature control includes controlling a heater that heats the molded body so that the molded body maintains the temperature range.

### Claim 6 (depends on 1)

The method for producing the molded product according to claim 1, comprising initiating cooling of the molded body after the temperature control.

### Claim 7

A manufacturing system comprising:
a molding machine configured to mold a material containing a cellulose derivative into a molded body, and
a heat-retaining chamber configured to perform temperature control on the molded body molded by the molding machine by maintaining the molded body within a predetermined temperature range for a predetermined time t,
wherein, when a phase transition point of the molded body is A (°C), the temperature range is A−10°C or more and A+50°C or less.