# US 2026/0241480 A1 · Projection welded joint and method for manufacturing projection welded joint

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0241480 A1
- Document ID: US20260241480A1
- Status: Published application
- Kind: A1
- Application number: 18/870,319
- Filed: 2023-06-01
- Published: 2026-08-20
- Earliest claimed: 2022-06-01
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Tohru OKADA; Hiroki FUJIMOTO; Seiji FURUSAKO
- Web page: https://patentgrep.com/patent/US20260241480A1

## CPC

- B23K 11/14: Projection welding
- B23K 11/00: Resistance welding; Severing by resistance heating
- B23K 11/0053: {Stud welding, i.e. resistive}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- B23K 2101/006: {Vehicles}
- B23K 2101/18: Sheet panels
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A projection welded joint according to one aspect of the present disclosure includes a steel sheet, a steel member, and a projection weld joining the steel sheet and the steel member, the projection weld includes a melted and solidified portion and a corona bond area around the melted and solidified portion, the steel sheet has a carbon content at a thickness center of 0.25 mass % or more, and the corona bond area includes an outer end portion having a hardness lower than that at a position of ¼ of a sheet thickness of the steel sheet outside the corona bond area. The steel sheet preferably includes a softened layer, in a range from the surface on the side to which the steel member is joined to a depth of 20 μm, having a hardness of 95% or less of that at the position of ¼ of the steel sheet thickness.

## Claims

### Claim 1

A projection welded joint comprising:
a steel sheet;
a steel member; and
a projection weld joining the steel sheet and the steel member, wherein
the projection weld includes a melted and solidified portion and a corona bond area around the melted and solidified portion,
the steel sheet has a carbon content at a thickness center of 0.25 mass % or more, and
the corona bond area includes an outer end portion having a hardness lower than a hardness at a position of ¼ of a sheet thickness of the steel sheet outside the corona bond area.

### Claim 2 (depends on 1)

The projection welded joint according to claim 1, wherein
the steel sheet includes a softened layer in a range from a surface to a depth of 20 μm, the surface on a side to which the steel member is joined, and
the softened layer has a hardness of 95% or less of the hardness at the position of ¼ of the sheet thickness of the steel sheet.

### Claim 3 (depends on 2)

The projection welded joint according to claim 2, wherein
the steel sheet includes a portion in a range from the surface on the side to which the steel member is joined to a depth of 20 μm to 200 μm, the portion having a hardness of 95% of the hardness at the position of ¼ of the sheet thickness of the steel sheet.

### Claim 4 (depends on 1)

The projection welded joint according to claim 1, wherein
the outer end portion of the corona bond area has a Vickers hardness of 700 Hv or less.

### Claim 5 (depends on 1)

The projection welded joint according to claim 1, wherein
the projection welded joint includes a plurality of the melted and solidified portions, and
a cross-sectional area of a first melted and solidified portion in a cross section along a sheet thickness direction of the steel sheet is 1.5 times or more a cross-sectional area of a second melted and solidified portion in a cross section along the sheet thickness direction of the steel sheet.

### Claim 6 (depends on 1)

A method for manufacturing the projection welded joint according to claim 1, the method comprising:
pressing a projection portion of a steel member against a steel sheet; and
energizing the projection portion to perform projection welding, wherein
the steel sheet has a carbon content at a thickness center of 0.25 mass % or more, the steel sheet includes a softened layer in a range from a surface to a depth of 20 μm, the surface on a side against which the projection portion is pressed, and
the softened layer has a hardness of 95% or less of a hardness at a position of ¼ of a sheet thickness of the steel sheet.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the steel sheet includes a portion in a range from the surface on the side against which the projection portion is pressed to a depth of 20 μm to 200 μm, the portion having a hardness of 95% of the hardness at the position of ¼ of the sheet thickness of the steel sheet.