# US 2026/0241441 A1 · Steel strip for battery case and method for producing steel strip

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0241441 A1
- Document ID: US20260241441A1
- Status: Published application
- Kind: A1
- Application number: 19/164,736
- Filed: 2023-09-18
- Published: 2026-08-20
- Earliest claimed: 2023-05-22
- Assignees: Institute of Research of Iron and Steel, Jiangsu Province/Sha-Steel, Co., Ltd.; Jiangsu Shagang Group Co., Ltd.; Zhangjiagang Yangtze River Cold Rolled Plate Co. Ltd
- Applicants: Institute of Research of Iron and Steel, Jiangsu Province/Sha-Steel, Co. Ltd; Jiangsu Shagang Group Co., Ltd.; Zhangjiagang Yangtze River Cold Rolled Plate Co. Ltd
- Inventors: Yanzhao ZHOU; Jianchao MA; Jiaqi ZHAO; Ning LI
- Web page: https://patentgrep.com/patent/US20260241441A1

## CPC

- B22D 11/117: by treating with gases (B22D11/118, B22D11/119 take precedence)
- C21C 7/0075: {Treating in a ladle furnace, e.g. up-/reheating of molten steel within the ladle}
- B22D 11/001: {of specific alloys}
- C21C 7/06: Deoxidising, e.g. killing
- C21C 7/076: Use of slags or fluxes as treating agents (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C21C 7/10: Handling in a vacuum
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/14: containing titanium or zirconium
- H01M 50/119: Metals
- Y02E 60/10: Energy storage using batteries
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing a steel strip for a battery case is provided. The steel strip for a battery case includes the following chemical composition in percentage by mass: carbon: 0.003-0.006%, silicon: ≤0.03%, manganese: 0.35-0.45%, titanium: 0.040-0.050%, aluminum: 0.040-0.060%, phosphorus: ≤0.020%, sulfur: ≤0.012%, nitrogen: ≤0.0040%, and the balance of iron and other inevitable impurities, wherein 7>Ti/(C+N)>5. The process flow of the production is as follows: hot metal pretreatment→converter smelting→LF refining→RH treatment→continuous pouring→hot rolling→acid pickling→cold rolling→continuous annealing→finishing. By means of designing the chemical composition, the Δr value of strip steel is reduced, and the isotropy and processability of the strip steel are improved; and by means of the process, precise control over steel composition and effective control over the amount and size of inclusions in the steel are achieved, the amount of inclusions in a shallow surface layer of a slab is reduced, the peeling depth is reduced or peeling is avoided, and the yield is increased.

## Claims

### Claim 1

A method for producing a steel strip for a battery case, comprising steps of hot metal pretreatment, converter smelting, LF (ladle furnace) refining, RH treatment, and continuous casting, wherein
LF refining is as follows: a ladle, after being placed, is moved to a power-on heating position, and power-on heating is started; a bottom blowing flow rate of the ladle is controlled at 300-500 NL/min during heating process; when a molten steel temperature reaches a target temperature of 1618-1635° C., a temperature and an oxygen content are measured, wherein a free oxygen content in molten steel is 0.06-0.07%; and the bottom blowing flow rate of the ladle is adjusted to 100-200 NL/min, and a slag modifier and lime are added according to the free oxygen content in the molten steel;
RH treatment is as follows: an RH arrival temperature is 1610-1630° C., an arrival free oxygen content is 0.06-0.07%, an arrival carbon content is 0.025-0.035%, and a T·Fe content in a RH ladle slag composition upon arrival is 5-8%; after carrying out RH decarburization for 15-18 min, the free oxygen content in the molten steel is 0.025-0.030%, and aluminum particles, carbon-containing ferromanganese, metallic manganese and a titanium-containing alloy are added in turn according to composition requirements, wherein an addition amount of the carbon-containing ferromanganese is 2.3-2.7 kg/t steel, an addition amount of the metallic manganese is 1.1-1.3 kg/t steel, and after the Al particles and manganese-containing alloy are added, the titanium-containing alloy is added after circulating; time between RH vacuum breaking and cast start in continuous casting ranges from 10-15 min; and a carbon content in the carbon-containing ferromanganese is 0.8-1.2%, and a titanium content in the titanium-containing alloy is more than or equal to 99.6%;
continuous casting is as follows: tundish superheat is 25-35° C., an immersion depth of a submerged nozzle is 160-220 mm, an opening angle is 20°, and an argon flow rate of a stopper for continuous casting is 8-12 L/min;
the steel strip for a battery case comprises the following chemical composition in percentage by mass: 0.003-0.006% of carbon, less than or equal to 0.03% of silicon, 0.35-0.45% of manganese, 0.040-0.050% of titanium, 0.040-0.060% of aluminum, less than or equal to 0.020% of phosphorus, less than or equal to 0.012% of sulfur, less than or equal to 0.0040% of nitrogen, and a balance of iron and other inevitable impurities, wherein Ti/(C+N) is more than 5 and less than 7.

### Claim 2 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein the hot metal pretreatment comprises: stirring the hot metal for desulfurization, wherein a sulfur content in the hot metal after desulfurization is less than or equal to 0.0050%.

### Claim 3 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein converter smelting is as follows: at least two bottom blowing holes are clearly visible, an argon gas is blown at the bottom in the whole blowing process, wherein an argon gas flow rate is more than or equal to 300 Nm3/h, an endpoint temperature of converter blowing is 1640-1660° C., an endpoint carbon content of a converter is 0.03-0.04%, an endpoint free oxygen content of the converter is 0.06-0.08%, a T·Fe content in a converter final slag is 15-18%, and a slag amount during converter tapping is 2-4 kg/t.

### Claim 4 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein after continuous casting, the method further comprises hot rolling, acid pickling, cold rolling, continuous annealing, and finishing.

### Claim 5 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein during LF refining, 400-500 kg of slag modifier and 400-500 kg of lime are added.

### Claim 6 (depends on 5)

The method for producing the steel strip for a battery case according to claim 5, wherein the slag modifier has composition as follows: 45-50% of Al, 20-25% of CaO, 10-15% of Al2O3, 10-15% of CaCO3, and other inevitable impurities.

### Claim 7 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein during RH refining, the T·Fe content in the ladle slag composition during RH vacuum breaking is less than or equal to 5%.

### Claim 8 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein during RH treatment, after Al particles and manganese-containing alloy are added, a circulation is carried out for 3 min before the titanium-containing alloy is added.

### Claim 9 (depends on 1)

The method for producing the steel strip for a battery case according to claim 1, wherein during continuous casting, a final product has inclusions less than or equal to 15 μm in size, and has a total oxygen content of less than or equal to 15 ppm.