# US 2026/0239898 A1 · Equal matching of oxidation rate between sige and si through clustered pre-clean and pre-surface nitridation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0239898 A1
- Document ID: US20260239898A1
- Status: Published application
- Kind: A1
- Application number: 19/309,135
- Filed: 2025-08-25
- Published: 2026-08-13
- Earliest claimed: 2025-02-07
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Edy CARDONA; Christopher Sean OLSEN
- Web page: https://patentgrep.com/patent/US20260239898A1

## CPC

- H10P 14/6308: {of Group IV semiconductors}
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/34: more than one element being applied in more than one step
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6319: {Formation by plasma treatments, e.g. plasma oxidation of the substrate}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 14/6504: {In-situ cleaning}
- H10P 14/6512: {by exposure to a gas or vapour}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6526: {introduced into an oxide material, e.g. changing SiO to SiON}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments disclosed herein generally relate to methods and systems that facilitate the formation of silicon dioxide (SiO2) layers in complementary metal-oxide semiconductor (CMOS) film stack structures. In some embodiments, a method of forming a metal phosphide hardmask includes providing the substrate to a processing chamber, the substrate comprising a silicon (Si) layer and a silicon germanium (SiGe) layer, removing native oxides from the Si layer and the SiGe layer, performing thermal nitridation on the Si layer and the SiGe layer, and oxidizing the Si layer and the SiGe layer with atomic oxygen or hydroxyl (OH) radicals.

## Claims

### Claim 1

A method of processing a substrate, comprising:
providing the substrate to a processing chamber, the substrate comprising a silicon (Si) layer and a silicon germanium (SiGe) layer;
removing native oxides from the Si layer and the SiGe layer;
performing thermal nitridation on the Si layer and the SiGe layer; and
oxidizing the Si layer and the SiGe layer with atomic oxygen or hydroxyl (OH) radicals.

### Claim 2 (depends on 1)

The method of claim 1, wherein a process temperature during the thermal nitridation ranges from 500 degrees Celsius (° C.) to 900 °C.

### Claim 3 (depends on 1)

The method of claim 1, wherein a chamber pressure during the thermal nitridation ranges from 1 Torr to 750 Torr.

### Claim 4 (depends on 1)

The method of claim 1, wherein a flow of ammonia (NH3) during the thermal nitridation ranges from 0.5 standard liter per minute (SLM) to 10 SLM.

### Claim 5 (depends on 1)

The method of claim 1, wherein a process temperature during the oxidizing ranges from 600° C. to 1000° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein a chamber pressure during the oxidizing ranges from 0.3 Torr to 3 Torr.

### Claim 7 (depends on 1)

The method of claim 1, wherein a flow of the atomic oxygen or OH radicals during the oxidizing ranges from 0.5 SLM to 12 SLM.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
forming silicon dioxide (SiO2) layers on the Si layer and the SiGe layer, wherein the SiO2 layers have a substantially equal thickness.

### Claim 9

A method of processing a substrate, comprising:
providing the substrate to a processing chamber, the substrate comprising a silicon (Si) layer and a silicon germanium (SiGe) layer;
performing thermal nitridation on the Si layer and the SiGe layer; and
oxidizing the Si layer and the SiGe layer with atomic oxygen or hydroxyl (OH) radicals.

### Claim 10 (depends on 9)

The method of claim 9, wherein a process temperature during the thermal nitridation ranges from 500 degrees Celsius (° C.) to 900° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein a chamber pressure during the thermal nitridation ranges from 1 Torr to 750 Torr.

### Claim 12 (depends on 9)

The method of claim 9, wherein a flow of ammonia (NH3) during the thermal nitridation ranges from 0.5 standard liter per minute (SLM) to 10 SLM.

### Claim 13 (depends on 9)

The method of claim 9, wherein a process temperature during the oxidizing ranges from 600° C. to 1000° C.

### Claim 14 (depends on 9)

The method of claim 9, wherein a chamber pressure during the oxidizing ranges from 0.3 Torr to 3 Torr.

### Claim 15 (depends on 9)

The method of claim 9, wherein a flow of the atomic oxygen or OH radicals during the oxidizing ranges from 0.5 SLM to 12 SLM.

### Claim 16 (depends on 9)

The method of claim 9, further comprising:
forming silicon dioxide (SiO2) layers on the Si layer and the SiGe layer, wherein the SiO2 layers have a substantially equal thickness.

### Claim 17

A system for processing a substrate, comprising:
a first chamber configured to expose a silicon (Si) layer and a silicon germanium (SiGe) layer of the substrate to dielectric processing;
a second chamber configured to remove native oxides from the Si layer and the SiGe layer;
a third chamber configured to perform thermal nitridation on the Si layer and the SiGe layer; and
a fourth chamber configured to oxidize the Si layer and the SiGe layer with atomic oxygen or hydroxyl (OH) radicals.

### Claim 18 (depends on 17)

The system of claim 17, wherein to perform the thermal nitridation, the third chamber operates with:
a process temperature ranging from 500 degrees Celsius (° C.) to 900° C.;
a chamber pressure ranging from 1 Torr to 750 Torr; and
a flow of ammonia (NH3) ranging from 0.5 standard liter per minute (SLM) to 10 SLM.

### Claim 19 (depends on 17)

The system of claim 17, wherein to oxidize the Si layer and the SiGe layer, the fourth chamber operates with:
a process temperature ranging from 600° C. to 1000° C.;
a chamber pressure ranging from 0.3 Torr to 3 Torr; and
a flow of the atomic oxygen or OH radicals ranging from 0.5 SLM to 12 SLM.

### Claim 20 (depends on 17)

The system of claim 17, wherein the first chamber, the second chamber, the third chamber, and the fourth chamber are coupled to a main frame.