# US 2026/0239638 A1 · Method for manufacturing semiconductor device and mesa diode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0239638 A1
- Document ID: US20260239638A1
- Status: Published application
- Kind: A1
- Application number: 19/135,845
- Filed: 2024-08-05
- Published: 2026-08-13
- Earliest claimed: 2023-12-21
- Assignees: Shindengen Electric Manufacturing Co., Ltd.
- Applicants: Shindengen Electric Manufacturing Co., Ltd.
- Inventors: Atsushi OGASAWARA; Koji ITO; Ryota MURAI
- Web page: https://patentgrep.com/patent/US20260239638A1

## CPC

- H10D 8/422: {PN diodes having the PN junctions in mesas}
- H10P 58/20: {comprising two or more processes, e.g. etching and cutting}
- H10D 8/045: {of PN junction diodes}
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10P 14/6346: {using printing, e.g. ink-jet printing}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/642: {Chemical etching}
- H10P 54/40: by sawing, e.g. using revolving or reciprocating blades
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a semiconductor device using lead-free glass without using a photolithography step and a large amount of chemicals is provided. Insulating films are formed on an upper surface and lower surface of a silicone wafer having a PN junction. A groove is formed in the upper surface having a depth exceeding the PN junction. The inner surface of the groove is wet-etched to reduce a surface roughness and a silicon oxide film is formed on the inner surface of the groove. A lead-free glass layer is formed on the silicon oxide film and the insulating films are removed. Metal films are formed on the upper surface and the lower surface of the silicon wafer. The lead-free glass layer and the silicon wafer are cut along a center of a bottom surface of the groove.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, comprising:
forming insulating films on upper and lower surfaces of a silicon wafer having a PN junction;
cutting the upper surface of the silicon wafer with a dicing blade to form a groove with a depth exceeding the PN junction;
wet-etching an inner surface of the groove to reduce a surface roughness of the inner surface of the groove to 0.1 μm or less;
forming a silicon oxide film on the inner surface of the groove;
forming a lead-free glass layer on the silicon oxide film on the inner surface of the groove;
removing the insulating films;
forming metal films on the upper and lower surfaces of the silicon wafer; and
cutting the lead-free glass layer and the silicon wafer along a center of a bottom surface of the groove.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the formed silicon oxide film is an oxide film having a thickness of 100 nm or less.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein an angle formed between the bottom surface and a side surface of the groove in a cross section of the formed groove is equal to or greater than 60° and equal to or less than 90°.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the wet etching includes a wet etching solution comprising a mixed solution of hydrofluoric acid, nitric acid, sulfuric acid, phosphoric acid, and water.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the formed insulating film comprises a silicon oxide film formed by a thermal oxidation method.

### Claim 6 (depends on 2)

The method for manufacturing a semiconductor device according to claim 2,
wherein the lead-free glass layer is formed on the silicon oxide film on the inner surface of the groove by an electrophoretic deposition method.

### Claim 7 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the lead-free glass layer is formed on the silicon oxide film on the inner surface of the groove by a printing method.

### Claim 8

A mesa diode comprising:
a first-conductivity-type semiconductor layer;
a second-conductivity-type semiconductor layer in contact with the first-conductivity-type semiconductor layer;
a silicon oxide film formed on a side surface of the second-conductivity-type semiconductor layer, an end portion of an interface between the second-conductivity-type semiconductor layer and the first-conductivity-type semiconductor layer, and a portion of a side surface of the first-conductivity-type semiconductor layer; and
a lead-free glass layer disposed on the silicon oxide film,
wherein a surface roughness of each of the side surfaces of the second-conductivity-type semiconductor layer, the end portion of the interface between the second-conductivity-type semiconductor layer and the first-conductivity-type semiconductor layer, and the portion of the side surface of the first-conductivity-type semiconductor layer is equal to or less than 0.1 μm.

### Claim 9

A mesa diode comprising:
a first-conductivity-type semiconductor layer;
a second-conductivity-type semiconductor layer that is in contact with the first-conductivity-type semiconductor layer;
a silicon oxide film formed on a side surface of the first-conductivity-type semiconductor layer, an end portion of an interface between the first-conductivity-type semiconductor layer and the second-conductivity-type semiconductor layer, and a portion of a side surface of the second-conductivity-type semiconductor layer; and
a lead-free glass layer disposed on the silicon oxide film,
wherein a surface roughness of each of the side surfaces of the first-conductivity-type semiconductor layer, the end portion of the interface between the first-conductivity-type semiconductor layer and the second-conductivity-type semiconductor layer, and the portion of the side surface of the second-conductivity-type semiconductor layer is equal to or less than 0.1 μm.

### Claim 10 (depends on 8)

The mesa diode according to claim 8,
wherein a thickness of the silicon oxide film is equal to or less than 100 nm.

### Claim 11 (depends on 9)

The mesa diode according to claim 9,
Wherein a thickness of the silicon oxide film is equal to or less than 100 nm.