# US 2026/0237610 A1 · Fluoride coating to improve chamber performance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0237610 A1
- Document ID: US20260237610A1
- Status: Published application
- Kind: A1
- Application number: 19/561,847
- Filed: 2026-03-10
- Published: 2026-08-13
- Earliest claimed: 2020-08-03
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Jennifer Y. Sun; Ren-Guan Duan; Gayatri Natu; Tae Won Kim; Jiyong Huang; Nitin Deepak; Paul Brillhart; Lin Zhang; Yikai Chen; Sanni Sinikka Seppälä; Ganesh Balasubramanian; JuanCarlos Rocha; Shankar Venkataraman; Katherine Elizabeth Woo
- Web page: https://patentgrep.com/patent/US20260237610A1

## CPC

- H01J 37/32495: {Means for protecting the vessel against plasma}
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45529: {specially adapted for making a layer stack of alternating different compositions or gradient compositions}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Embodiments of the disclosure relate to articles, coated chamber components and methods of coating chamber components with a protective coating that includes at least one metal fluoride having a formula selected from the group consisting of M1xFw, M1xM2yFw and M1xM2yM3zFw, where at least one of M1, M2, or M3 is magnesium or lanthanum. The protective coating can be deposited by atomic layer deposition, chemical vapor deposition, electron beam ion assisted deposition, or physical vapor deposition.

## Claims

### Claim 1

A method comprising:
depositing, by atomic layer deposition (ALD), chemical vapor deposition (CVD), electron beam ion assisted deposition (EB-IAD) or physical vapor deposition (PVD), a protective coating on an un-roughened surface of a substrate,
wherein the protective coating comprises at least one metal fluoride having a formula selected from a group consisting of M1xFw, M1xM2yFw, and M1xM2yM3zFw,
wherein:
a) when the metal fluoride has the formula of M1xFw, x is 1, and w ranges from 1 to 3,
b) when the metal fluoride has the formula of M1xM2yFw, x ranges from 0.1 to 1, y ranges from 0.1 to 1, and w ranges from 1 to 3, and
c) when the metal fluoride has the formula of M1xM2yM3zFw, x ranges from 0.1 to 1, y ranges from 0.1 to 1, z ranges from 0.1 to 1, and w ranges from 1 to 3;
wherein at least one of M1, M2, or M3 comprises magnesium or lanthanum.

### Claim 2 (depends on 1)

The method of claim 1, wherein the protective coating comprises at least one of MgxFw, LaxFw, YxMgyFw, YxLayFw, LaxMgyFw, or YxMgyLazFw.

### Claim 3 (depends on 1)

The method of claim 1, further comprising depositing an adhesion and fluorine diffusion barrier layer between the surface of the substrate and the protective coating.

### Claim 4 (depends on 1)

The method of claim 1, comprising depositing continuously, by ALD, the protective coating to attain a target thickness.

### Claim 5 (depends on 1)

The method of claim 1, wherein the protective coating is crystalline, and wherein depositing tunes the roughness of a top surface of the protective coating to range from about 0.1 microinches to about 200 microinches.

### Claim 6 (depends on 1)

The method of claim 1, comprising depositing, by ALD, alternating amorphous and crystalline layers to attain a multi-layer lamellar structure, wherein each layer is uniform and conformal.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate comprises aluminum alloy, AlN, Al2O3, Ni, stainless steel, or nickel-chromium alloy.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate is a heater, electrostatic chuck, faceplate, showerhead, liner, blocker plate, gas box, edge ring, or bellow.

### Claim 9 (depends on 1)

The method of claim 1, wherein the protective coating comprises a stack of a plurality of alternating compositionally different first metal fluoride layers and second metal fluoride layers, the first metal fluoride layers and second metal fluoride layers having a thickness ratio between about 10:1 and about 3:1.

### Claim 10 (depends on 9)

The method of claim 9, wherein the protective coating comprises above 2 atom % up to about 25 atom % oxygen, the compositionally different first metal fluoride layers and second metal fluoride layers comprising at least one metal fluoride having a formula selected from the group consisting of M1xFw, M1xM2yFw and M1xM2yM3zFw.

### Claim 11

A method for coating a surface of a substrate using atomic layer deposition (ALD) with a protective coating, comprising:
depositing an adsorption layer on the surface of the substrate by pulsing one or more metal precursors of M1, M2, M3, or a combination thereof into an ALD processing chamber,
introducing a fluorine component into the ALD processing chamber to form the protective coating, the protective coating comprising at least one metal fluoride having a formula selected from a group consisting of M1xFw, M1xM2yFw, and M1xM2yM3zFw, wherein:
a) when the metal fluoride has the formula of M1xFw, x is 1, and w ranges from 1 to 3,
b) when the metal fluoride has the formula of M1xM2yFw, x ranges from 0.1 to 1, y ranges from 0.1 to 1, and w ranges from 1 to 3, and
c) when the metal fluoride has the formula of M1xM2yM3zFw, x ranges from 0.1 to 1, y ranges from 0.1 to 1, z ranges from 0.1 to 1, and w ranges from 1 to 3;
wherein at least one of M1, M2, or M3 comprises magnesium or lanthanum.

### Claim 12 (depends on 11)

The method of claim 11, wherein introducing comprises directly fluorinating the adsorption layer by pulsing a fluorine containing reactant into the ALD processing chamber.

### Claim 13 (depends on 11)

The method of claim 11, wherein introducing comprises pulsing an oxygen containing reactant into the ALD processing chamber to react with the adsorption layer followed by exposing the oxygen reacted adsorption layer to a fluorine containing species to fluorinate and convert the oxygen reacted adsorption layer to at least one metal fluoride having a formula of M1xM2yM3zFw.

### Claim 14 (depends on 11)

The method of claim 11, wherein the protective coating comprises at least one of MgxFw LaxFw, YxMgyFw, YxLayFw, LaxMgyFw, or YxMgyLazFw.

### Claim 15 (depends on 11)

The method of claim 11, wherein the protective coating is crystalline.

### Claim 16 (depends on 11)

The method of claim 11, wherein depositing tunes a roughness of a top surface of the protective coating to range from about 0.1 microinches to about 200 microinches.

### Claim 17 (depends on 11)

The method of claim 11, wherein the substrate comprises aluminum alloy, AlN, Al2O3, Ni, stainless steel, or nickel-chromium alloy.

### Claim 18 (depends on 11)

The method of claim 11, wherein the substrate is a heater, electrostatic chuck, faceplate, showerhead, liner, blocker plate, gas box, edge ring, or bellow.

### Claim 19 (depends on 11)

The method of claim 11, wherein the protective coating comprises a stack of a plurality of alternating compositionally different first metal fluoride layers and second metal fluoride layers, the first metal fluoride layers and second metal fluoride layers having a thickness ratio between about 10:1 and about 3:1.

### Claim 20 (depends on 19)

The method of claim 19, wherein the protective coating comprises above 2 atom % up to about 25 atom % oxygen, the compositionally different first metal fluoride layers and second metal fluoride layers comprising at least one metal fluoride having a formula selected from the group consisting of M1xFw, M1xM2yFw and M1xM2yM3zFw.