# US 2026/0237566 A1 · Electrolytic capacitor and method for producing electrolytic capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0237566 A1
- Document ID: US20260237566A1
- Status: Published application
- Kind: A1
- Application number: 19/153,573
- Filed: 2024-02-19
- Published: 2026-08-13
- Earliest claimed: 2023-02-28
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: TAKEHIRO KOBAYASHI; KAZUHIRO TAKATANI
- Web page: https://patentgrep.com/patent/US20260237566A1

## CPC

- H01G 9/02: Diaphragms; Separators
- H01G 9/145: Liquid electrolytic capacitors (H01G11/00 takes precedence)
- H01G 9/00: Electrolytic capacitors, rectifiers, detectors, switching devices, light-sensitive or temperature-sensitive devices; Processes of their manufacture
- H01G 9/0029: {Processes of manufacture}
- H01G 9/0032: {formation of the dielectric layer}
- H01G 9/0036: {Formation of the solid electrolyte layer}
- H01G 9/025: Solid electrolytes (H01G11/54 takes precedence)
- H01G 9/028: Organic semiconducting electrolytes, e.g. TCNQ
- H01G 9/035: Liquid electrolytes, e.g. impregnating materials (H01G11/54 takes precedence)
- H01G 9/055: Etched foil electrodes
- H01G 9/07: Dielectric layers
- H01G 9/15: Solid electrolytic capacitors (H01G11/00 takes precedence)
- H01G 11/48: Conductive polymers
- H01G 11/52: Separators
- H01G 9/151: {with wound foil electrodes}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

An electrolytic capacitor includes a laminate and a liquid component impregnated into the laminate. The laminate includes an anode foil including a dielectric layer disposed on a surface thereof, a cathode foil, a separator, and a conductive polymer layer disposed in the separator. The anode foil and the cathode foil are laminated with the separator interposed therebetween. In the log differential pore volume distribution curve of the separator in which the conductive polymer layer is disposed, a log differential pore volume at the maximum peak in the log differential pore volume distribution curve is in the range from 1.0 cm3/g to 2.3 cm3/g, inclusive.

## Claims

### Claim 1

An electrolytic capacitor, comprising:
a laminate; and
a liquid component impregnated into the laminate, wherein:
the laminate includes:
an anode foil including a dielectric layer disposed on a surface of the anode foil,
a cathode foil,
a separator, and
a conductive polymer layer disposed in the separator,
the anode foil and the cathode foil are laminated with the separator disposed between the anode foil and the cathode foil, and
in a log differential pore volume distribution curve of the separator in which the conductive polymer layer is disposed, a log differential pore volume at a maximum peak in the log differential pore volume distribution curve is in a range from 1.0 cm3/g to 2.3 cm3/g, inclusive.

### Claim 2

A method for producing an electrolytic capacitor comprising a cathode foil and an anode foil including a dielectric layer disposed on a surface of the anode foil, the method comprising, in this order:
a step (i) of forming a conductive polymer layer in a separator using a coating liquid containing a conductive polymer component;
a step (ii) of forming a laminate including the conductive polymer layer by laminating the anode foil, the cathode foil, and the separator to interpose the separator between the anode foil and the cathode foil; and
a step (iii) of impregnating the laminate with a liquid component,
wherein in the step (i), the conductive polymer layer is formed so that a log differential pore volume at a maximum peak in a log differential pore volume distribution curve of the separator in which the conductive polymer layer is formed is in a range from 1.0 cm3/g to 2.3 cm3/g, inclusive.

### Claim 3 (depends on 2)

The method according to claim 2, further comprising:
between the step (ii) and the step (iii),
a step (x) of impregnating the conductive polymer layer with a liquid including water and an organic compound that does not boil at 100° C. at 1 atm; and
a step (y) of removing a part of the liquid with which the conductive polymer layer is impregnated while remaining the organic compound in the conductive polymer layer.