# US 2026/0236060 A1 · Foldable display screen and method for manufacturing glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0236060 A1
- Document ID: US20260236060A1
- Status: Published application
- Kind: A1
- Application number: 18/707,176
- Filed: 2023-08-01
- Published: 2026-08-13
- Earliest claimed: 2022-08-31
- Assignees: Chengdu Boe Optoelectronics Technology Co., Ltd.; Boe Technology Group Co., Ltd.
- Applicants: Chengdu BOE Optoelectronics Technology Co., Ltd.; BOE Technology Group Co., Ltd.
- Inventors: Shiyou WANG; Tiejun BI; Yongxiao GAO; Qiang TANG; Zhihui WANG
- Web page: https://patentgrep.com/patent/US20260236060A1

## CPC

- G06F 1/1616: {with folding flat displays, e.g. laptop computers or notebooks having a clamshell configuration, with body parts pivoting to an open position around an axis parallel to the plane they define in closed position}
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 17/322: {Polyurethanes or polyisocyanates}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- G06F 1/1656: {Details related to functional adaptations of the enclosure, e.g. to provide protection against EMI, shock, water, or to host detachable peripherals like a mouse or removable expansions units like PCMCIA cards, or to provide access to internal components for maintenance or to removable storage supports like CDs or DVDs, or to mechanically mount accessories (mounting of accessories to a computer display G06F1/1607; display hoods G06F1/1603; cooling arrangements for portable computers G06F1/203)}
- G06F 1/20: Cooling means
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a foldable display screen, including: glass, wherein the glass includes a recess formed in a first plane of the glass; wherein the recess is disposed in a bendable region of the foldable display screen, the recess extends in a lengthwise direction of the bendable region and runs through the first plane, and a distance between two side surfaces of the recess gradually increases along a direction close to the first plane; wherein each of the side surfaces of the recess includes a first arcuate surface and a second arcuate surface, wherein the first arcuate surface is connected to the first plane and curved towards a bottom surface of the recess, the second arcuate surface is connected to the bottom surface of the recess and curved towards the first plane, and the first arcuate surface is connected to the second arcuate surface.

## Claims

### Claim 1

A foldable display screen, comprising: glass, wherein the glass comprises a recess formed in a first plane of the glass; wherein
the recess is disposed in a bendable region of the foldable display screen, the recess extends in a lengthwise direction of the bendable region and runs through the first plane, and a distance between two side surfaces of the recess gradually increases along a direction close to the first plane;
wherein each of the side surfaces of the recess comprises a first arcuate surface and a second arcuate surface, wherein the first arcuate surface is connected to the first plane and curved towards a bottom surface of the recess, the second arcuate surface is connected to the bottom surface of the recess and curved towards the first plane, and the first arcuate surface is connected to the second arcuate surface.

### Claim 2 (depends on 1)

The foldable display screen according to claim 1, wherein the bottom surface of the recess is parallel to the first plane, and a distance between the bottom surface of the recess and a second plane, away from the first plane, of the glass is greater than or equal to 30 μm and less than or equal to 50 μm.

### Claim 3 (depends on 1)

The foldable display screen according to claim 1, wherein a distance between a side edge, close to the bottom surface of the recess, of an orthographic projection of the side surface of the recess on the first plane and a side edge, away from the bottom surface of the recess, of the orthographic projection of the side surface of the recess on the first plane is greater than or equal to 5 mm and less than or equal to 10 mm.

### Claim 4 (depends on 1)

The foldable display screen according to claim 1, wherein the first arcuate surface and the second arcuate surface are both circular arcuate surfaces, and curvature radii of cross-sections of the two arcuate surfaces are both greater than or equal to 10 mm.

### Claim 5 (depends on 1)

The foldable display screen according to claim 1, further comprising: a transparent filling layer configured to fill the recess, wherein a refractive index of the transparent filling layer is greater than or equal to 1.41 and less than or equal to 1.61.

### Claim 6 (depends on 5)

The foldable display screen according to claim 5, further comprising: a display panel, a cover layer, and a heat dissipation support layer, wherein the cover layer is configured to cover and protect the display panel, and the glass is disposed in the cover layer.

### Claim 7 (depends on 5)

The foldable display screen according to claim 5, wherein a surface of the glass is coated with potassium ions and/or sodium ions.

### Claim 8 (depends on 1)

A method for manufacturing glass, applicable to manufacturing the glass in the foldable display screen as defined in claim 1, the method comprising:
forming a recess having a predetermined depth by thinning a selected region in a first plane of a glass substrate, wherein the selected region corresponds to a bendable region of the foldable display screen, and a non-selected region in the first plane corresponds to a non-bendable region of the foldable display screen;
forming the glass by cutting the thinned glass substrate; and
strengthening an impact strength of the glass.

### Claim 9 (depends on 8)

The method according to claim 8, wherein strengthening the impact strength of the glass comprises:
comparing the predetermined depth of the recess with a depth threshold; and
in a case where the predetermined depth is less than or equal to the depth threshold, performing a single chemical strengthening treatment on the non-bendable region and the bendable region of the glass; or
in a case where the predetermined depth is greater than the depth threshold, performing n chemical strengthening treatments on the glass, wherein n is a positive integer greater than or equal to 2.

### Claim 10 (depends on 9)

The method according to claim 9, wherein
a chemical strengthening treatments in the n chemical strengthening treatments are performed on both the non-bendable region and the bendable region of the glass, wherein a is a positive integer greater than or equal to 1 and less than or equal to n−1; and
n−a chemical strengthening treatments in the n chemical strengthening treatments are performed only on the non-bendable region in the first plane, such that a thickness of a strengthening layer in the non-bendable region is greater than a thickness of a strengthening layer in the bendable region.

### Claim 11 (depends on 10)

The method according to claim 10, wherein performing n chemical strengthening treatments on the glass comprises:
shielding the bendable region of the glass by providing a strengthening shielding layer;
performing a first chemical strengthening treatment on the non-bendable region of the glass for a first duration by immersing the glass into a molten first strengthening material at a first predetermined temperature;
removing the strengthening shielding layer and the first strengthening material remaining on a surface of the glass;
performing a second chemical strengthening treatment on the bendable region and the non-bendable region of the glass for a second duration by immersing the glass into a molten second strengthening material at a second predetermined temperature; and
removing the second strengthening material remaining on the surface of the glass.

### Claim 12 (depends on 10)

The method according to claim 10, wherein performing n chemical strengthening treatments on the glass comprises:
performing a first chemical strengthening treatment on the bendable region and the non-bendable region of the glass for a first duration by immersing the glass into a molten first strengthening material at a first predetermined temperature;
removing the first strengthening material remaining on a surface of the glass;
providing a strengthening shielding layer that shields the bendable region of the glass, such that the bendable region is prevented from being chemically strengthened;
performing a second chemical strengthening treatment on the non-bendable region of the glass for a second duration by immersing the glass into a molten second strengthening material at a second predetermined temperature;
removing the strengthening shielding layer and the second strengthening material remaining on the surface of the glass;
performing a third chemical strengthening treatment on the bendable region and the non-bendable region of the glass for a third duration by immersing the glass into a molten third strengthening material at a third predetermined temperature; and
removing the third strengthening material remaining on the surface of the glass;
wherein the first duration is less than the second duration, and the third duration is less than the first duration.

### Claim 13 (depends on 8)

The method according to claim 8, wherein forming the recess having the predetermined depth by thinning the selected region in the first plane of the glass substrate comprises:
providing a thinning shielding layer configured to shield the non-selected region of the glass substrate, such that the non-selected region is prevented from being etched;
etching the selected region such that the glass substrate is thinned at the selected region by the predetermined depth and the recess is formed; and
removing the thinning shielding layer.

### Claim 14 (depends on 13)

The method according to claim 13, wherein etching the selected region such that the glass substrate is thinned at the selected region by the predetermined depth and the recess is formed comprises:
etching an etching region within the selected region to a specified depth;
increasing a width of the etching region by a predetermined value, determining the increased etching region as a new etching region, and etching the new etching region to the specified depth; an
repeating the step of increasing the width of the etching region by the predetermined value until an etching depth is equal to the predetermined depth of the recess.

### Claim 15 (depends on 8)

The method according to claim 8, wherein the bottom surface of the recess is parallel to the first plane, and a distance between the bottom surface of the recess and a second plane, away from the first plane, of the glass is greater than or equal to 30 μm and less than or equal to 50 μm.

### Claim 16 (depends on 8)

The method according to claim 8, wherein a distance between a side edge, close to the bottom surface of the recess, of an orthographic projection of the side surface of the recess on the first plane and a side edge, away from the bottom surface of the recess, of the orthographic projection of the side surface of the recess on the first plane is greater than or equal to 5 mm and less than or equal to 10 mm.

### Claim 17 (depends on 8)

The method according to claim 8, wherein the first arcuate surface and the second arcuate surface are both circular arcuate surfaces, and curvature radii of cross-sections of the two arcuate surfaces are both greater than or equal to 10 mm.

### Claim 18 (depends on 8)

The method according to claim 8, wherein the foldable display screen further comprises a transparent filling layer configured to fill the recess, wherein a refractive index of the transparent filling layer is greater than or equal to 1.41 and less than or equal to 1.61.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the foldable display screen further comprises a display panel, a cover layer, and a heat dissipation support layer, wherein the cover layer is configured to cover and protect the display panel, and the glass is disposed in the cover layer.

### Claim 20 (depends on 18)

The method according to claim 18, wherein a surface of the glass is coated with potassium ions and/or sodium ions.