- Inventors: Zheng JU; Jiajie CEN; Ruinan ZHOU; Zhiyuan WU; Kevin KASHEFI
- Web page: https://patentgrep.com/patent/US20260234810A1

## CPC

- C23C 16/0227: {by cleaning or etching}
- C23C 30/005: {on hard metal substrates}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/06: characterised by the deposition of metallic material
- G01N 33/553: Metal or metal coated
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/432: {using selective deposition}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/034: {bottomless barrier, adhesion or liner layers}
- H10W 20/035: {combinations of barrier, adhesion or liner layers, e.g. multi-layered barrier layers}
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- H10W 20/047: {by introducing additional elements therein}
- H10W 20/052: {by treatments not introducing additional elements therein}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/054: {by selectively removing parts thereof (H10W20/034 takes precedence)}
- H10W 20/055: {by formation methods other than physical vapour deposition [PVD], chemical vapour deposition [CVD] or liquid deposition}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/076: {in via holes or trenches}
- H10W 20/0765: {the thin functional dielectric layers being temporary, e.g. sacrificial layers}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/084: {for dual-damascene structures}
- H10W 20/096: {by contacting with gases, liquids or plasmas}
- H10W 20/425: {Barrier, adhesion or liner layers}
- C23C 28/30: {Coatings combining at least one metallic layer and at least one inorganic non-metallic layer}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a microelectronic device includes pre-treating a metal surface formed on a substrate, depositing a self-assembled monolayer (SAM) selectively on the metal surface against a dielectric surface formed on the substrate, depositing a barrier layer selectively on the dielectric surface against the SAM, and removing the SAM.

## Claims

### Claim 1

A method of forming a microelectronic device, the method comprising:
pre-treating a metal surface formed on a substrate;
depositing a self-assembled monolayer (SAM) selectively on the metal surface against a dielectric surface formed on the substrate;
depositing a barrier layer selectively on the dielectric surface against the SAM; and
removing the SAM.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal surface comprises copper (Cu), cobalt (Co), tungsten (W), molybdenum (Mo), ruthenium (Ru), titanium nitride (TiN), or any combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein pre-treating the metal surface comprises soaking the substrate in nitrogen containing molecules or gas.

### Claim 4 (depends on 1)

The method of claim 1, wherein depositing the SAM comprises soaking the substrate in blocking molecules.

### Claim 5 (depends on 4)

The method of claim 4, wherein the blocking molecules comprise alkyne molecules.

### Claim 6 (depends on 1)

The method of claim 1, wherein the barrier layer comprises one or more of tantalum nitride (TaN), titanium nitride (TiN), silicon nitride (Si3N4), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), or silicon oxynitride (SiON).

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
selectively depositing a metal liner on the barrier layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the metal liner comprises ruthenium (Ru), cobalt (Co), molybdenum (Mo), tantalum (Ta), or any combination thereof.

### Claim 9

A method of forming a microelectronic device, the method comprising:
pre-cleaning and pre-treating a top surface of a first metal layer exposed within a feature opening extending through a dielectric layer that is formed on the first metal layer;
depositing a blocking layer selectively on the top surface of the first metal layer exposed within the feature opening against sidewalls of the feature opening;
depositing a barrier layer selectively on the sidewalls of the feature opening against the blocking layer;
removing the blocking layer; and
filling the feature opening with a second metal layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first metal layer comprises copper (Cu), cobalt (Co), tungsten (W), molybdenum (Mo), ruthenium (Ru), titanium nitride (TiN), or any combination thereof.

### Claim 11 (depends on 9)

The method of claim 9, wherein pre-treating the top surface of the first metal layer comprises soaking the top surface of the first metal layer in nitrogen containing molecules or gas.

### Claim 12 (depends on 9)

The method of claim 9, wherein depositing the blocking layer comprises soaking the top surface of the first metal layer in blocking molecules.

### Claim 13 (depends on 12)

The method of claim 12, wherein the blocking molecules comprise alkyne molecules.

### Claim 14 (depends on 9)

The method of claim 9, wherein the barrier layer comprises one or more of tantalum nitride (TaN), titanium nitride (TiN), silicon nitride (Si3N4), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), or silicon oxynitride (SiON).

### Claim 15 (depends on 9)

The method of claim 9, further comprising:
prior to filling the feature opening, selectively depositing a metal liner on the barrier layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the metal liner comprises ruthenium (Ru), cobalt (Co), molybdenum (Mo), tantalum (Ta), or any combination thereof.

### Claim 17 (depends on 9)

The method of claim 9, wherein the second metal layer comprises copper (Cu) or cobalt (Co).

### Claim 18

A method of removal of self-assembled monolayer (SAM) from a metal surface, the method comprising:
soaking the metal surface in ammonia (NH3) gas supplied at a flow rate of between 500 sccm and 3000 sccm, for a time duration of between 10 seconds and 60 seconds;
subsequent to soaking the metal surface, depositing a self-assembled monolayer (SAM) on the metal surface; and
removing the SAM from the metal surface, wherein carbon (C) residue on the metal surface after the removing the SAM is reduced as compared to a SAM removal without the soaking the metal surface.

### Claim 19 (depends on 18)

The method of claim 18, wherein the metal surface comprises copper (Cu), cobalt (Co), tungsten (W), molybdenum (Mo), ruthenium (Ru), titanium nitride (TiN), or any combination thereof.

### Claim 20 (depends on 18)

The method of claim 18, wherein depositing the SAM comprises soaking the metal surface in blocking molecules comprising alkyne molecules.