# US 2026/0234796 A1 · Method of manufacturing molybdenum film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0234796 A1
- Document ID: US20260234796A1
- Status: Published application
- Kind: A1
- Application number: 19/439,012
- Filed: 2026-01-02
- Published: 2026-08-13
- Earliest claimed: 2025-02-07
- Assignees: Foundation for Research and Business, Seoul National University of Science and Technology
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Jeong Hwan Han; Ji Sang Ahn
- Web page: https://patentgrep.com/patent/US20260234796A1

## CPC

- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/14: Deposition of only one other metal element
- C23C 16/18: from metallo-organic compounds
- C23C 16/32: Carbides
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45531: {specially adapted for making ternary or higher compositions}
- C23C 16/45534: {Use of auxiliary reactants other than used for contributing to the composition of the main film, e.g. catalysts, activators or scavengers}
- C23C 16/56: After-treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided is a method of manufacturing a molybdenum film by repeatedly performing a cycle, wherein the cycle includes preparing a substrate including a first region and a second region and injecting a molybdenum precursor onto the substrate, thereby forming a chemisorption layer of the molybdenum precursor, supplying a first purge gas onto a resulting structure in which the chemisorption layer of the molybdenum precursor has been formed, supplying a reducing agent containing water (H2O) onto the chemisorption layer of the molybdenum precursor, thereby forming a molybdenum thin film, and supplying a second purge gas onto a resulting structure in which the molybdenum thin film has been formed.

## Claims

### Claim 1

A method of manufacturing a molybdenum film by repeatedly performing a cycle, wherein the cycle comprises:
injecting a molybdenum precursor onto a substrate comprising a first region and a second region, thereby forming a chemisorption layer of the molybdenum precursor;
supplying a first purge gas onto a first resulting structure in which the chemisorption layer of the molybdenum precursor has been formed;
supplying a reducing agent containing water (H2O) onto the chemisorption layer of the molybdenum precursor, thereby forming a molybdenum thin film; and
supplying a second purge gas onto a second resulting structure in which the molybdenum thin film has been formed.

### Claim 2 (depends on 1)

The method of claim 1, wherein the molybdenum precursor comprises a bis(ethylbenzene)molybdenum (BEBMo) precursor.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cycle is performed at a temperature in a range of about 150° C. to about 400° C., and
the manufactured molybdenum film has resistivity of about 100 μΩ×cm to about 600 μΩ×cm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cycle is performed 1 time to 60 times at a temperature in a range of about 200° C. to about 350° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first region of the substrate comprises a conductive film, and the second region of the substrate comprises an insulating film, and
wherein the chemisorption layer of the molybdenum precursor is formed on the first region of the substrate.

### Claim 6 (depends on 1)

The method of claim 1, comprising performing, under a hydrogen atmosphere, heat treatment on the molybdenum film formed by repeating the cycle.

### Claim 7 (depends on 6)

The method of claim 6, wherein the hydrogen atmosphere comprises about 5% to 15% of hydrogen (H2) gas and about 85% to about 95% of argon (Ar) gas.

### Claim 8 (depends on 6)

The method of claim 6, wherein the heat treatment is performed at a pressure of about 7 torr to about 9 torr and at a maximum temperature of about 750° C. to about 850° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the molybdenum film formed by repeatedly performing the cycle comprises about 60 at % to about 100 at % of molybdenum and about 20 at % to about 40 at % of carbon.

### Claim 10 (depends on 1)

The method of claim 1, wherein the molybdenum film formed by repeatedly performing the cycle comprises 0 at % to about 20 at % of oxygen.

### Claim 11

A method of manufacturing a molybdenum film by repeatedly performing a cycle, wherein the cycle comprises:
injecting a bis(ethylbenzene)molybdenum (BEBMo) precursor onto a substrate comprising a first region and a second region, thereby forming a chemisorption layer of the BEBMo precursor;
supplying a first purge gas onto a first resulting structure in which the chemisorption layer of the BEBMo precursor has been formed;
supplying a reducing agent onto the chemisorption layer of the BEBMo precursor, thereby forming a molybdenum thin film; and
supplying a second purge gas onto a second resulting structure in which the molybdenum thin film has been formed,
wherein the first region of the substrate comprises a conductive film,
wherein the second region of the substrate comprises an insulating film, and
wherein the chemisorption layer of the BEBMo precursor is formed on the first region of the substrate.

### Claim 12 (depends on 11)

The method of claim 11, wherein the reducing agent comprises water (H2O).

### Claim 13 (depends on 11)

The method of claim 11, wherein the cycle is performed 1 time to 60 times at a temperature in a range of about 200° C. to about 350° C., and
wherein during the cycle, the chemisorption layer of the BEBMo precursor has selectivity for the first region relative to the second region of the substrate.

### Claim 14 (depends on 13)

The method of claim 13, wherein a maximum number of repetitions of the cycle in which the BEBMo precursor has the selectivity for the first region of the substrate is inversely proportional to a process temperature at which the cycle is performed.

### Claim 15 (depends on 11)

The method of claim 11, comprising performing, under a hydrogen atmosphere, heat treatment on the molybdenum film formed by repeating the cycle,
wherein the hydrogen atmosphere comprises about 5% to 15% of hydrogen (H2) gas and about 85% to 95% of argon (Ar) gas.

### Claim 16 (depends on 15)

The method of claim 15, wherein the heat treatment is performed at a pressure of about 7 torr to about 9 torr and at a maximum temperature of 800° C.,
wherein a total time of the heat treatment is in a range of about 170 seconds to about 200 seconds, and
wherein the heat treatment is performed by raising a temperature at a certain rate of degrees Celsius per second (° C./sec) from a first temperature to the maximum temperature.

### Claim 17 (depends on 11)

The method of claim 11, wherein the molybdenum film formed by repeatedly performing the cycle comprises about 60 at % to about 100 at % of molybdenum, about 20 at % to about 40 at % of carbon, and 0 at % to about 20 at % of oxygen.

### Claim 18

A method of manufacturing a molybdenum film by repeatedly performing a cycle, wherein the cycle comprises:
injecting a bis(ethylbenzene)molybdenum (BEBMo) precursor onto a substrate comprising a first region and a second region, thereby forming a chemisorption layer of the BEBMo precursor;
supplying a first purge gas onto a first resulting structure in which the chemisorption layer of the BEBMo precursor has been formed;
supplying a reducing agent containing water (H2O) onto the chemisorption layer of the BEBMo precursor, thereby forming a molybdenum thin film; and
supplying a second purge gas onto a second resulting structure in which the molybdenum thin film has been formed,
wherein the first region of the substrate comprises a conductive film,
wherein the second region of the substrate comprises an insulating film, and
wherein the chemisorption layer of the BEBMo precursor has selectivity for the first region relative to the second region of the substrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein the chemisorption layer of the BEBMo precursor has selectivity for the first region relative to the second region of the substrate in a range of 1 time to 60 times of the cycle at a temperature in a range of about 200° C. to about 350° C., and
wherein a number of times of the cycle in which the BEBMo precursor has the selectivity for the first region of the substrate is inversely proportional to a process temperature at which the cycle is performed.

### Claim 20 (depends on 18)

The method of claim 18, comprising performing, under a hydrogen atmosphere, heat treatment on the molybdenum film formed by repeating the cycle,
wherein the hydrogen atmosphere comprises about 5% to 15% of hydrogen (H2) gas and about 85% to 95% of argon (Ar) gas, and
wherein the heat treatment is performed at a pressure of about 7 torr to about 9 torr and at a maximum temperature of 800° C.