# US 2026/0234434 A1 · Two-component acid-curing coating composition and coated article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0234434 A1
- Document ID: US20260234434A1
- Status: Published application
- Kind: A1
- Application number: 19/149,573
- Filed: 2023-02-09
- Published: 2026-08-13
- Earliest claimed: 2023-02-09
- Assignees: Sherwin-Williams (Guangdong) New Material Co., Ltd.
- Applicants: Sherwin-Williams (Guangdong) New Material Co., Ltd.
- Inventors: Wei YANG; Mijin ADIKKALATHIL
- Web page: https://patentgrep.com/patent/US20260234434A1

## CPC

- C09D 167/06: Unsaturated polyesters having carbon-to-carbon unsaturation
- C09D 167/08: Polyesters modified with higher fatty oils or their acids, or with natural resins or resin acids
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The present application relates to a two-component acid-curing coating composition and coated article. In particular, the two-component acid-curing coating composition comprises a) a film-forming resin composition, said film-forming resin composition comprising at least one alkyd resin, at least one second resin, and at least one amino resin, and b) at least one acid catalyst, wherein the at least one second resin is incompatible with the at least one amino resin; and wherein the at least one alkyd resin is present in an amount of at least 20 wt. % relative to the total weight of the film-forming resin composition. In some embodiments of the present application, at least one second resin differs from at least one amino resin in density by at least 8%. In some embodiments of the present application, at least one second resin differs from at least one amino resin in solubility parameter by at least 20%. In some embodiments of the present application, a mixture of at least one second resin with at least one amino resin in a weight ratio of 1:1 has a transparency of no greater than 70%.

## Claims

### Claim 1

A two-component acid-curing coating composition comprising:
a) a film-forming resin composition comprising at least one alkyd resin, at least one second resin, and at least one amino resin; and
b) at least one acidic catalyst,
wherein at least one second resin is incompatible with at least one amino resin; and
wherein the at least one alkyd resin is present in an amount of at least 20 wt. % relative to the total weight of the film-forming resin composition.

### Claim 2 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein at least one second resin differs from at least one amino resin in density by at least 8%, preferably at least one second resin differs from at least one amino resin in density by at least 10%, more preferably at least one second resin differs from at least one amino resin in density by at least 12% and no greater than 20%.

### Claim 3 (depends on 2)

The two-component acid-curing coating composition according to claim 2, wherein at least one second resin has a density lower than at least one amino resin by at least 8%, preferably by at least 10%, more preferably by at least 12% and no greater than 20%.

### Claim 4 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein at least one second resin differs from at least one amino resin in solubility parameter by at least 20%, preferably at least one second resin differs from at least one amino resin in solubility parameter by at least 25%, more preferably at least one second resin differs from at least one amino resin in solubility parameter by at least 30% and no greater than 60%.

### Claim 5 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein a mixture of at least one second resin and at least one amino resin at a weight ratio of 1:1 has a transparency of not more than 70%.

### Claim 6 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one alkyd resin comprises at least one saturated fatty acid-based alkyd resin with low oil content, at least one saturated fatty acid-based alkyd resin with medium oil content, at least one saturated fatty acid-based alkyd resin with high oil content, at least one saturated fatty acid-based alkyd resin with extreme high oil content, or combinations thereof, preferably comprising at least one saturated fatty acid-based alkyd resin with low oil content.

### Claim 7 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one alkyd resin has a hydroxyl value in the range of 140 to 240 mg KOH/g resin, preferably in the range of 140-200 mg KOH/g resin, more preferably in the range of 140-180 mg KOH/g resin, and still more preferably in the range of 145-170 mg KOH/g resin, as determined according to DIN EN ISO 4629-2:2016.

### Claim 8 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one alkyd resin has a density in the range of 1.09 to 1.10 g/cm3.

### Claim 9 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one second resin comprises a hydroxyl-functional polyester, preferably linear.

### Claim 10 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one second resin has a hydroxyl value in the range of 260 to 400 mg KOH/g resin,
preferably in the range of 290 to 380 mg KOH/g resin, more preferably in the range of 300 to 350 mg KOH/g resin, still more preferably in the range of 315 to 330 mg KOH/g resin;
alternatively, preferably in the range of 140-240 mg KOH/g resin, more preferably 140-200 mg KOH/g resin, even more preferably 140-180 mg KOH/g resin;
alternatively, preferably in the range of 260-400 mg KOH/g resin, preferably 290-380 mg KOH/g resin, and more preferably 300-350 mg KOH/g resin, as determined according to DIN EN ISO 4629-2:2016.

### Claim 11 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one second resin has a density in the range of 0.97 to 0.99 g/cm3.

### Claim 12 (depends on 1)

The two-component acid-curing coating composition according to claim 1,
wherein the at least one amino resin is a reaction product of at least one aldehyde with at least one amino compound; and
wherein the at least one amino compound comprises melamine, urea, phenyl-substituted melamine, methyl-substituted melamine, or combinations thereof.

### Claim 13 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one amino resin is etherified, preferably with n-butanol, isobutanol, methanol, or combinations thereof.

### Claim 14 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one amino resin has a density in the range of 1.09 to 1.10 g/cm3.

### Claim 15 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the film-forming resin composition further comprises at least one fluorocarbon resin-modified acrylics polymer.

### Claim 16 (depends on 15)

The two-component acid-curing coating composition according to claim 15, wherein the at least one fluorocarbon resin-modified acrylics polymer has a density less than three of the at least one alkyd resin, the at least one amino resin and the at least one second resin.

### Claim 17 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the film-forming resin composition comprises, relative to the total weight of the film-forming resin composition
20-35 wt. % of the at least one alkyd resin
1-30 wt. %, preferably 1-20 wt. % of the at least one second resin
20-30 wt. % of the at least one amino resin,
0-2 wt. % of the at least one fluorocarbon resin-modified acrylics polymer
2-40 wt. % of at least one solvent; and
0-5 wt. % of the at least one additional additive, wherein the at least one additional additive comprises: at least one pigment, at least one filler, at least one anti-settling agent, at least one thickener, at least one dispersant, at least one wetting agent, at least one film forming aid, at least one coupling agent, at least one fungicide, at least one anti-mold agent, or combinations thereof.

### Claim 18 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein the at least one acidic catalyst is selected from the group comprising p-toluenesulfonic acid, benzenesulfonic acid, methanesulfonic acid, dinonylnaphthalenesulfonic acid, dinonylnaphthalenedisulfonic acid, dodecylbenzenesulfonic acid, oxalic acid, maleic acid, phthalic acid, acrylic acid, mono(di)alkyl phosphate, phosphoric acid, mono(di)alkyl pyrophosphate, or combinations thereof.

### Claim 19 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein when the two-component acid-curing coating composition is applied and cured at room temperature for 7 days or more, the resulting coating has an interlayer adhesion of at least 5 kg, as determined using a BYK-Balanced Beam Scrape Adhesion Tester according to ASTM D2197.

### Claim 20 (depends on 1)

The two-component acid-curing coating composition according to claim 1, wherein when the two-component acid-curing coating composition is applied and cured at room temperature for 7 days or more, the resulting coating has a surface scratch resistance of at least 150 grams, as determined using a BYK-Hoffman scratch hardness tester according to E50TF61-S1.

### Claim 21 (depends on 1)

An article comprising
a substrate having at least one major surface; and
a coating at least partially applied directly or indirectly on the at least one major surface of the substrate,
wherein the coating is formed by the two-component acid-curing coating composition according to claim 1.

### Claim 22 (depends on 21)

The article of claim 21, wherein the substrate is selected from wood, wood composite, paper, metal, plastic, fabric, ceramic, cementious material, or combinations thereof.