# US 2026/0234302 A1 · Polyvinyl alcohol resin, water-soluble film, extrusion-molded article, filament, nonwoven fabric, container, method for producing water-soluble film, and aqueous solution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0234302 A1
- Document ID: US20260234302A1
- Status: Published application
- Kind: A1
- Application number: 19/152,762
- Filed: 2024-01-30
- Published: 2026-08-13
- Earliest claimed: 2023-01-31
- Assignees: Kuraray Co., Ltd.
- Applicants: Kuraray Co., Ltd.
- Inventors: Yoshiaki ASANUMA; Yosuke KUMAKI
- Web page: https://patentgrep.com/patent/US20260234302A1

## CPC

- C08F 116/06: Polyvinyl alcohol {; Vinyl alcohol}
- C08L 101/16: the macromolecular compounds being biodegradable
- B29C 48/05: Filamentary, e.g. strands
- B29C 48/08: flexible, e.g. films
- B65D 65/466: {Bio- or photodegradable packaging materials}
- C08F 8/14: Esterification
- D01F 6/14: from polymers of unsaturated alcohols, e.g. polyvinyl alcohol, or of their acetals or ketals
- D04H 3/007: Addition polymers
- B29K 2029/04: {PVOH, i.e. polyvinyl alcohol (B29K2031/04 takes precedence)}
- B29K 2995/006: Bio-degradable, e.g. bioabsorbable, bioresorbable or bioerodible
- B29K 2995/0062: water-soluble
- D10B 2321/06: polymers of unsaturated alcohols, e.g. polyvinyl alcohol, or of their acetals or ketals
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

To provide: a polyvinyl alcohol resin which enables obtaining a water-soluble film having favorable cold-water solubility and mechanical strength, has favorable biodegradability, and is superior in filterability in a state of an aqueous solution; a water-soluble film, an extruded product, a filament, a non-woven fabric, and a container each containing such a polyvinyl alcohol resin; a method for producing a water-soluble film; and an aqueous solution. The polyvinyl alcohol resin contains, as a principal component, a modified polyvinyl alcohol containing a unit represented by the following formula (1), wherein a ratio (N1/N2) of the number (N1) of 1-μm-size particles to the number (N2) of 2-μm-size particles contained in 1 mL of a 2% by mass aqueous solution of the polyvinyl alcohol resin is 0.1 or more and 50 or less. In the formula (1), R represents a single bond or a divalent organic group, and M represents a hydrogen atom, a metal atom, or an ammonium group.

## Claims

### Claim 1

A polyvinyl alcohol resin comprising, as a principal component, a modified polyvinyl alcohol comprising a unit represented by formula (1),
wherein a ratio (N1/N2) of the number (N1) of 1-μm-size particles to the number (N2) of 2-μm-size particles comprised in 1 mL of a 2% by mass aqueous solution of the polyvinyl alcohol resin is 0.1 or more and 50 or less,
wherein in the formula (1), R represents a single bond or a divalent organic group, and M represents a hydrogen atom, a metal atom, or an ammonium group.

### Claim 2 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein the modified polyvinyl alcohol has a content of the unit represented by the formula (1) of 0.5 mol % or more and 20 mol % or less, a degree of saponification of 68 mol % or more and 99.9 mol % or less, and an average degree of polymerization of 200 or more and 4,500 or less.

### Claim 3 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein a total volume of the 1-μm-size particles and the 2-μm-size particles comprised in 1 mL of the 2% by mass aqueous solution of the polyvinyl alcohol resin is 1 μm3 or more and 10,000 μm3 or less.

### Claim 4 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein in the formula (1), R represents a divalent aliphatic organic group.

### Claim 5 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein in the formula (1), R represents a divalent saturated aliphatic organic group.

### Claim 6 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein in the formula (1), R represents a divalent saturated aliphatic hydrocarbon group having 1 or more and 3 or less carbon atoms.

### Claim 7 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein in the unit represented by the formula (1), 5% or more and 100% or less of M is a metal atom or an ammonium group.

### Claim 8 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein in the unit represented by the formula (1), 5% or more and 100% or less of M is a sodium atom.

### Claim 9 (depends on 1)

The polyvinyl alcohol resin according to claim 1, having a biodegradation rate of 60% or more.

### Claim 10 (depends on 1)

The polyvinyl alcohol resin according to claim 1, wherein when a cast film obtained from the polyvinyl alcohol resin and having an average thickness of 50 μm is subjected to moisture conditioning at 20° C. and 65% RH for 1 week and then to an aqueous dissolution test at 5° C., a period of time of the dissolution is 5 sec or more and 3,000 sec or less.

### Claim 11 (depends on 1)

A water-soluble film comprising the polyvinyl alcohol resin according to claim 1.

### Claim 12 (depends on 11)

The water-soluble film according to claim 11, formed from the polyvinyl alcohol resin in accordance with at least one process selected from the group consisting of a solvent casting process, a calender process, a blow molding process, an extrusion process, and a blow extrusion process.

### Claim 13 (depends on 1)

An extruded product obtained by extruding the polyvinyl alcohol resin according to claim 1, the extruded product having a film shape or a filament shape.

### Claim 14 (depends on 1)

A filament comprising the polyvinyl alcohol resin according to claim 1.

### Claim 15 (depends on 14)

A non-woven fabric comprising the filament according to claim 14.

### Claim 16 (depends on 11)

A container comprising the water-soluble film according to claim 11 as a packaging material.

### Claim 17 (depends on 16)

The container according to claim 16, configured to be charged with at least one selected from the group consisting of an agrochemical, an oxidant, and a detergent.

### Claim 18 (depends on 1)

A method for producing a water-soluble film, the method comprising:
preparing an aqueous solution comprising the polyvinyl alcohol resin according to claim 1; and
forming a film by using the aqueous solution.

### Claim 19 (depends on 18)

The method for producing a water-soluble film according to claim 18, the method further comprising:
before the forming,
filtering the aqueous solution with a filter.

### Claim 20 (depends on 1)

An aqueous solution comprising the polyvinyl alcohol resin according to claim 1,
wherein a content of the polyvinyl alcohol resin is 0.1 ppm or more and 50 ppm or less.

### Claim 21 (depends on 20)

The aqueous solution according to claim 20, having a temperature of 20° C. or more and 25° C. or less.

### Claim 22 (depends on 20)

The aqueous solution according to claim 20, further comprising at least one of a magnesium ion or a calcium ion,
wherein a total content of the magnesium ion and the calcium ion is 10 ppm or more and 400 ppm or less.

### Claim 23 (depends on 1)

An aqueous solution comprising the polyvinyl alcohol resin according to claim 1,
wherein a content of the polyvinyl alcohol resin is 3% by mass or more and 12% by mass or less.