# US 2026/0234051 A1 · Multilayer structure for low-emissivity glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0234051 A1
- Document ID: US20260234051A1
- Status: Published application
- Kind: A1
- Application number: 19/152,004
- Filed: 2024-01-09
- Published: 2026-08-13
- Earliest claimed: 2023-02-06
- Assignees: KCC Glass Corporation
- Applicants: KCC GLASS Corporation
- Inventors: Bo-Na YU; Chong-Cheol KIM; Seok KIM
- Web page: https://patentgrep.com/patent/US20260234051A1

## CPC

- C03C 17/366: {Low-emissivity or solar control coatings}
- C03C 17/3613: {Coatings of type glass/inorganic compound/metal/inorganic compound/metal/other}
- C03C 17/3626: {one layer at least containing a nitride, oxynitride, boronitride or carbonitride}
- C03C 17/3634: {one layer at least containing carbon, a carbide or oxycarbide}
- C03C 17/3639: {Multilayers containing at least two functional metal layers}
- C03C 17/3642: {the multilayer coating containing a metal layer}
- C03C 17/3644: {the metal being silver}
- C03C 17/3681: {the multilayer coating being used in glazing, e.g. windows or windscreens}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present disclosure relates to a multilayer structure for low-emissivity glass, which includes a first dielectric layer, a first metal protecting layer, a first infrared ray reflecting layer, a second metal protecting layer, a second dielectric layer, a dielectric protecting layer, and an overcoat layer, sequentially, in which the overcoat layer includes a carbon layer.

## Claims

### Claim 1

A multilayer structure for low-emissivity glass, comprising:
a first dielectric layer, a first metal protecting layer, a first infrared ray reflecting layer, a second metal protecting layer, a second dielectric layer, a dielectric protecting layer, and an overcoat layer, sequentially,
wherein the overcoat layer includes a carbon layer.

### Claim 2 (depends on 1)

The multilayer structure of claim 1, wherein each of the first dielectric layer and the second dielectric layer independently includes at least one type selected from a metal nitride, a metal oxide or a metal oxynitride, and
wherein each of the first metal protecting layer and the second metal protecting layer independently includes at least one selected from nickel (Ni), chromium (Cr) or a nickel-chromium (Ni—Cr).

### Claim 3 (depends on 1)

The multilayer structure of claim 1, wherein the dielectric protecting layer includes a metal oxide, a nitride, or an oxynitride of at least one type metal selected from the group consisting of silicon (Si), niobium (Nb), titanium (Ti), zirconium (Zr), and tantalum (Ta).

### Claim 4 (depends on 1)

The multilayer structure of claim 1, wherein the overcoat layer has an average thickness ranging from 1 to 10 nm,
wherein the dielectric protecting layer has an average thickness ranging from 0.5 to 5 nm,
wherein each of the first dielectric layer and the second dielectric layer independently has an average thickness ranging from 10 to 100 nm,
wherein each of the first metal protecting layer and the second metal protecting layer independently has an average thickness ranging from 1 to 7 nm, and
wherein the first infrared ray reflecting layer has an average thickness ranging from 10 to 30 nm.

### Claim 5 (depends on 1)

The multilayer structure of claim 1, further including:
a third metal protecting layer, a second infrared ray reflecting layer, a fourth metal protecting layer, and a third dielectric layer, sequentially, between the second dielectric layer and the dielectric protecting layer.

### Claim 6 (depends on 1)

The multilayer structure of claim 1, wherein emissivity of at most 0.2 is measured in compliance with KS L 2525, a visible light transmittance of at least 50% is measured with respect to a wavelength ranging from 380 to 780 nm in compliance with KS L 2514, and a color difference (ΔE) of less than 4.5 is measured in compliance with ASTM C 1376.