# US 2026/0234039 A1 · Tin oxide doped with bismuth and copper semiconductor material for wastewater treatment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0234039 A1
- Document ID: US20260234039A1
- Status: Published application
- Kind: A1
- Application number: 19/048,614
- Filed: 2025-02-07
- Published: 2026-08-13
- Earliest claimed: 2025-02-07
- Assignees: Imam Abdulrahman Bin Faisal University
- Applicants: Imam Abdulrahman Bin Faisal University
- Inventors: Imen MASSOUDI
- Web page: https://patentgrep.com/patent/US20260234039A1

## CPC

- C02F 1/725: {by catalytic oxidation}
- B01J 23/8437: {Bismuth}
- B01J 35/33: Electric or magnetic properties
- B01J 35/39: Photocatalytic properties
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/45: Nanoparticles
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 35/77: Compounds characterised by their crystallite size
- B01J 37/031: {Precipitation}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C02F 1/32: with ultraviolet light
- C02F 2101/306: {Pesticides}
- C02F 2101/308: {Dyes; Colorants; Fluorescent agents}
- C02F 2209/44: Time
- C02F 2305/10: Photocatalysts
- Y02W 10/37: using solar energy
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A semiconductor material is described. The semiconductor material includes tin oxide, bismuth and copper, where the tin oxide is doped with the bismuth and the copper, and where the bismuth is present in an amount of 1 to 5 weight percent (wt. %) based on a total weight of the semiconductor material. The copper is present in an amount of 1 to 5 wt. % based on the total weight of the semiconductor material, and where the tin oxide is in the form of a tetragonal phase with a crystallite size of 15 to 25 nm.

## Claims

### Claim at position 1

1: A semiconductor material, comprising:
tin oxide;
bismuth; and
copper,
wherein the tin oxide is doped with the bismuth and the copper,
wherein the bismuth is present in an amount of 1 to 5 weight percent (wt. %) based on a total weight of the semiconductor material,
wherein the copper is present in an amount of 1 to 5 wt. % based on the total weight of the semiconductor material, and
wherein the tin oxide is in the form of a tetragonal phase with a crystallite size of 15-25 nm.

### Claim at position 2 (depends on 1)

2: The semiconductor material of claim 1, wherein the bismuth is present in an amount of 2 to 4 wt. % based on a total weight of the semiconductor material.

### Claim at position 3 (depends on 1)

3: The semiconductor material of claim 1, wherein the copper is present in an amount of 2 to 4 wt. % based on a total weight of the semiconductor material.

### Claim at position 4 (depends on 1)

4: The semiconductor material of claim 1, wherein the semiconductor material has a crystallite size of 21 to 25 nm.

### Claim at position 5 (depends on 1)

5: The semiconductor material of claim 1, wherein the semiconductor material has a unit cell volume of 71.95 to 72.05 Å3.

### Claim at position 6 (depends on 1)

6: The semiconductor material of claim 1, wherein the semiconductor material has a band gap of 2.85 to 2.9 eV.

### Claim at position 7 (depends on 1)

7: The semiconductor material of claim 1, wherein the semiconductor material has a dielectric constant of 3000 to 3500 at a frequency of 50 Hz.

### Claim at position 8 (depends on 1)

8: The semiconductor material of claim 1, wherein the semiconductor material is made by a process, comprising:
dissolving a tin salt and a copper salt in a first organic solvent to form a first solution;
dissolving a bismuth salt in a second organic solvent to form a second solution;
mixing the first solution and the second solution and adding a base to form a precipitate;
calcinating the precipitate at a first temperature of 350 to 450° C. for 30 to 90 minutes; and
calcinating the precipitate at a second temperature of 550 to 650° C. for 1 to 3 hours to form the semiconductor material.

### Claim at position 9 (depends on 1)

9: A method of photocatalytic degradation, comprising:
contacting the semiconductor material of claim 1 with a solution comprising one or more pollutants;
irradiating the solution; and
degrading the one or more pollutants in the solution.

### Claim at position 10 (depends on 9)

10: The method of claim 9, wherein the one or more pollutants are selected from a group consisting of Congo red, imidacloprid, and malachite green.

### Claim at position 11 (depends on 9)

11: The method of claim 9, wherein the irradiating occurs for 5 to 70 minutes.

### Claim at position 12 (depends on 9)

12: The method of claim 9, wherein the semiconductor material has a photocatalytic efficiency of 90 to 99% based on an initial concentration of the one or more pollutants.

### Claim at position 13 (depends on 9)

13: The method of claim 9, wherein the semiconductor material has an adsorption activity of 25 to 35% based on an initial concentration of the one or more pollutants.

### Claim at position 14 (depends on 10)

14: The method of claim 10, wherein the one or more pollutants is Congo red and the semiconductor material has a photocatalytic efficiency of 96 to 98% based on an initial concentration of the Congo red.

### Claim at position 15 (depends on 10)

15: The method of claim 10, wherein the one or more pollutants is imidacloprid and the semiconductor material has a photocatalytic efficiency of 92 to 94% based on an initial concentration of the imidacloprid.

### Claim at position 16 (depends on 10)

16: The method of claim 10, wherein the one or more pollutants is malachite green and the semiconductor material has a photocatalytic efficiency of 97 to 99% based on an initial concentration of the malachite green.

### Claim at position 17 (depends on 11)

17: The method of claim 11, wherein the irradiating occurs for 60 minutes and the semiconductor material has a chemical oxygen demand removal of 92 to 96%.

### Claim at position 18 (depends on 11)

18: The method of claim 11, wherein the irradiating occurs for 60 minutes and the semiconductor material has a total organic carbon removal of 94 to 98%.

### Claim at position 19 (depends on 9)

19: The method of claim 9, wherein hydroxyl radicals and superoxide anion radicals are involved in the degradation of the one or more pollutants.

### Claim at position 20 (depends on 9)

20: The method of claim 9, further comprising:
repeating the contacting and the irradiating 2 to 5 times,
wherein the one or more pollutants in the solution are degraded by at least 85% based on an initial concentration of the one or more pollutants.