# US 2026/0233280 A1 · Steel sheet and member, and methods of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0233280 A1
- Document ID: US20260233280A1
- Status: Published application
- Kind: A1
- Application number: 19/154,362
- Filed: 2023-11-21
- Published: 2026-08-13
- Earliest claimed: 2023-03-23
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Junya TOBATA; Hideyuki KIMURA
- Web page: https://patentgrep.com/patent/US20260233280A1

## CPC

- B21D 5/14: by passing between rollers (B21D5/06 takes precedence)
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/19: by interrupted quenching
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/007: {containing Co}
- C21D 6/008: {containing Si}
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C25D 3/22: of zinc
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Provided is a steel sheet that has a TS of 1320 MPa or more, as well as excellent stretch flangeability, and excellent toughness and crash properties after paint baking. The steel sheet has a defined chemical composition and a microstructure where an area fraction of tempered martensite is 95% or more, an area fraction of retained austenite is less than 3%, a total area fraction of bainitic ferrite and ferrite is less than 5%, and a 20° or greater grain boundary density in tempered martensite is 1.0 μm/μm2 or more, satisfying the following Expression ⁢ ( 1 )  KAM ⁡ ( S ) / KAM ⁡ ( C ) > 1. ( l )

## Claims

### Claim 1

A steel sheet comprising: a chemical composition containing, in mass %,
C: 0.030% or more and 0.500% or less,
Si: 0.010% or more and 2.500% or less,
Mn: 0.10% or more and 5.00% or less,
P: 0.100% or less,
S: 0.0200% or less,
N: 0.0100% or less,
O: 0.0100% or less, and
Al: 1.000% or less,
with the balance being Fe and inevitable impurity; and a steel microstructure wherein
area fraction of tempered martensite is 95% or more,
area fraction of retained austenite is less than 3%,
total area fraction of ferrite and bainitic ferrite is less than 5%,
20° or greater grain boundary density in the tempered martensite is 1.0 μm/μm2 or more, and
the following Expression (1) is satisfied,
KAM
⁡
(
S
)
/
KAM
⁡
(
C
)
>
1.
(
l
)
where,
KAM(S) is an average KAM value at a depth of 100 μm from a surface of the steel sheet, and
KAM(C) is an average KAM value at a mid-thickness position of the steel sheet.

### Claim 2 (depends on 1)

The steel sheet according to claim 1, wherein the chemical composition further contains, in mass %, at least one selected from the group consisting of
Ti: 0.200% or less,
Nb: 0.200% or less,
V: 0.200% or less,
Ta: 0.10% or less,
W: 0.10% or less,
B: 0.0100% or less,
Cr: 1.00% or less,
Mo: 1.00% or less,
Ni: 1.00% or less,
Co: 0.010% or less,
Cu: 1.00% or less,
Sn: 0.200% or less,
Sb: 0.200% or less,
Ca: 0.0100% or less,
Mg: 0.0100% or less,
REM: 0.0100% or less,
Zr: 0.100% or less,
Te: 0.100% or less,
Hf: 0.10% or less, and
Bi: 0.200% or less.

### Claim 3 (depends on 1)

The steel sheet according to claim 1, further comprising a coated or plated layer on a surface.

### Claim 4 (depends on 2)

The steel sheet according to claim 2, further comprising a coated or plated layer on a surface.

### Claim 5 (depends on 1)

A member made using the steel sheet according to claim 1.

### Claim 6 (depends on 1)

A method of producing the steel sheet according to claim 1, the method comprising:
a preparation process of preparing a blank sheet having the chemical composition according to claim 1;
a heating process of heating the blank sheet under a set of conditions including
an average heating rate in a temperature range from 700° C. to 750° C. of 5.0° C./s or less, and
heating to an annealing temperature T1;
an annealing process of annealing the blank sheet under a set of conditions including the annealing temperature T1 being 800° C. or more, and
an annealing time t1 of 10 s or longer;
a bending process of applying bending once or more to the blank sheet using a roller that has a radius of 800 mm or less in a temperature range from the annealing temperature T1 to 700° C.;
a first cooling process of cooling the blank sheet under a set of conditions including an average cooling rate in a temperature range from 700° C. to 550° C. of 10° C./s or more,
to a first cooling end temperature;
a second cooling process of cooling the blank sheet under a set of conditions including an average cooling rate in a temperature range from 300° C. to 100° C. of 300° C./s or more, and
applying tension to the blank sheet in the temperature range from 300° C. to 100° C. of 5 MPa or more,
to a second cooling end temperature;
a tempering process of tempering the blank sheet under a set of conditions including a tempering temperature T2 of 100° C. or more and 400° C. or less, and
a tempering time t2 of 10 s or longer and 10,000 s or shorter; and
a straightening process of applying straightening to the blank sheet by leveling under a set of conditions including a straightening start temperature of 100° C. or less,
an entry side intermesh pressing amount of 4.0 mm or more and 10.0 mm or less,
a delivery intermesh pressing amount of 1.0 mm or more and 10.0 mm or less,
an entry side tension of 20 MPa or more and 500 MPa or less, and
a delivery tension of 25 MPa or more and 550 MPa or less.

### Claim 7 (depends on 6)

The method of producing a steel sheet according to claim 6, further comprising a coating or plating process of applying a coating or plating treatment to the blank sheet between the first cooling process and the second cooling process, or between the tempering process and the straightening process.

### Claim 8 (depends on 1)

A method of producing a member, wherein the steel sheet according to claim 1 is subjected to at least one of a forming process or a joining process to produce the member.

### Claim 9 (depends on 2)

A member made using the steel sheet according to claim 2.

### Claim 10 (depends on 3)

A member made using the steel sheet according to claim 3.

### Claim 11 (depends on 4)

A member made using the steel sheet according to claim 4.

### Claim 12 (depends on 2)

A method of producing the steel sheet according to claim 2, the method comprising:
a preparation process of preparing a blank sheet having the chemical composition according to claim 2;
a heating process of heating the blank sheet under a set of conditions including
an average heating rate in a temperature range from 700° C. to 750° C. of 5.0° C./s or less, and
heating to an annealing temperature T1;
an annealing process of annealing the blank sheet under a set of conditions including the annealing temperature T1 being 800° C. or more, and
an annealing time t1 of 10 s or longer;
a bending process of applying bending once or more to the blank sheet using a roller that has a radius of 800 mm or less in a temperature range from the annealing temperature T1 to 700° C.;
a first cooling process of cooling the blank sheet under a set of conditions including an average cooling rate in a temperature range from 700° C. to 550° C. of 10° C./s or more,
to a first cooling end temperature;
a second cooling process of cooling the blank sheet under a set of conditions including an average cooling rate in a temperature range from 300° C. to 100° C. of 300° C./s or more, and
applying tension to the blank sheet in the temperature range from 300° C. to 100° C. of 5 MPa or more,
to a second cooling end temperature;
a tempering process of tempering the blank sheet under a set of conditions including a tempering temperature T2 of 100° C. or more and 400° C. or less, and
a tempering time t2 of 10 s or longer and 10,000 s or shorter; and
a straightening process of applying straightening to the blank sheet by leveling under a set of conditions including a straightening start temperature of 100° C. or less,
an entry side intermesh pressing amount of 4.0 mm or more and 10.0 mm or less,
a delivery intermesh pressing amount of 1.0 mm or more and 10.0 mm or less,
an entry side tension of 20 MPa or more and 500 MPa or less, and
a delivery tension of 25 MPa or more and 550 MPa or less.

### Claim 13 (depends on 12)

The method of producing a steel sheet according to claim 12, further comprising a coating or plating process of applying a coating or plating treatment to the blank sheet between the first cooling process and the second cooling process, or between the tempering process and the straightening process.

### Claim 14 (depends on 2)

A method of producing a member, wherein the steel sheet according to claim 2 is subjected to at least one of a forming process or a joining process to produce the member.

### Claim 15 (depends on 3)

A method of producing a member, wherein the steel sheet according to claim 3 is subjected to at least one of a forming process or a joining process to produce the member.

### Claim 16 (depends on 4)

A method of producing a member, wherein the steel sheet according to claim 4 is subjected to at least one of a forming process or a joining process to produce the member.