# US 2026/0231780 A1 · Manufacturing method of electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0231780 A1
- Document ID: US20260231780A1
- Status: Published application
- Kind: A1
- Application number: 19/426,091
- Filed: 2025-12-19
- Published: 2026-08-06
- Earliest claimed: 2025-02-05
- Assignees: Innolux Corporation
- Applicants: InnoLux Corporation
- Inventors: Kuang-Ming FAN
- Web page: https://patentgrep.com/patent/US20260231780A1

## CPC

- H10W 70/095: {of vias therein}
- G01L 1/241: {by photoelastic stress analysis}
- G01N 21/41: Refractivity; Phase-affecting properties, e.g. optical path length (G01N21/21 takes precedence)
- H05K 3/0029: {of inorganic insulating material}
- H05K 2203/163: Monitoring a manufacturing process
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- G01L: MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE (weighing G01G)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A manufacturing method of an electronic device includes: providing a substrate; performing a laser modification step on the substrate to form modified regions; performing a first inspection step on the substrate by a first equipment, the first inspection step including providing a first light to pass through the substrate, so as to obtain a first phase difference and calculate a first stress value; performing a perforation step on the substrate to form through holes in the modified regions; and performing a second inspection step on the substrate by the first equipment, the second inspection step including providing a second light to pass through the substrate, so as to obtain a second phase difference and calculate a second stress value. The substrate has a first temperature during the first inspection step, and the substrate has a second temperature different from the first temperature during the second inspection step.

## Claims

### Claim 1

A manufacturing method of an electronic device, comprising:
providing a substrate;
performing a laser modification step on the substrate to form a plurality of modified regions;
performing a first inspection step on the substrate by a first equipment after the laser modification step, wherein the first inspection step comprises providing a first light to pass through the substrate, so as to obtain a first phase difference and calculate a first stress value;
performing a perforation step on the substrate to form a plurality of through holes in the plurality of modified regions; and
performing a second inspection step on the substrate by the first equipment after the perforation step, wherein the second inspection step comprises providing a second light to pass through the substrate, so as to obtain a second phase difference and calculate a second stress value,
wherein the substrate has a first temperature during the first inspection step, the substrate has a second temperature during the second inspection step, and the second temperature is different from the first temperature.

### Claim 2 (depends on 1)

The manufacturing method of the electronic device according to claim 1, wherein the first inspection step further comprises placing the substrate on a platform of the first equipment and heating the substrate to the first temperature before providing the first light.

### Claim 3 (depends on 2)

The manufacturing method of the electronic device according to claim 2, wherein the second inspection step further comprises placing the substrate on the platform of the first equipment and heating the substrate to the second temperature before providing the second light.

### Claim 4 (depends on 2)

The manufacturing method of the electronic device according to claim 2, wherein the first inspection step further comprises: monitoring whether a temperature of the substrate reaches the first temperature by the first equipment, and providing the first light to pass through the substrate when the temperature of the substrate reaches the first temperature.

### Claim 5 (depends on 2)

The manufacturing method of the electronic device according to claim 2, wherein the platform is movable along a first direction, and the first direction is perpendicular to a normal direction of the substrate.

### Claim 6 (depends on 1)

The manufacturing method of the electronic device according to claim 1, wherein the first light and the second light are individually selected from visible light having a wavelength of 360 nm to 830 nm, near-infrared light having a wavelength of 700 nm to 1400 nm, short-wave infrared light having a wavelength of 1400 nm to 3000 nm, mid-wave infrared light having a wavelength of 3000 nm to 5000 nm, or long-wave infrared light having a wavelength of 8 μm to 12 μm.

### Claim 7 (depends on 1)

The manufacturing method of the electronic device according to claim 1, wherein the first inspection step comprises:
enabling the first light to pass through a first polarizer and then through the substrate to form a first inspection light; and
enabling the first inspection light to pass through a second polarizer to obtain the first phase difference.

### Claim 8 (depends on 7)

The manufacturing method of the electronic device according to claim 7, wherein the second inspection step comprises:
enabling the second light to pass through the first polarizer and then through the substrate to form a second inspection light; and
enabling the second inspection light to pass through the second polarizer to obtain the second phase difference.

### Claim 9 (depends on 1)

The manufacturing method of the electronic device according to claim 1, further comprising:
forming a conductive layer in the plurality of through holes; and
performing a third inspection step on the substrate by the first equipment after forming the conductive layer, wherein the third inspection step comprises providing a third light to pass through the substrate, so as to obtain a third phase difference and calculate a third stress value,
wherein the substrate has a third temperature during the third inspection step, and the third temperature is different from the first temperature and the second temperature.

### Claim 10 (depends on 1)

The manufacturing method of the electronic device according to claim 1, wherein the first equipment comprises a heating chamber, a light-emitting module and a camera module, and the light-emitting module and the camera module are disposed on two opposite sides of the heating chamber, wherein the first inspection step comprises:
placing the substrate in the heating chamber and heating the substrate to the first temperature;
enabling the light-emitting module to provide the first light such that the first light passes through the substrate to form a first inspection light; and
receiving the first inspection light by the camera module to obtain the first phase difference.

### Claim 11 (depends on 10)

The manufacturing method of the electronic device according to claim 10, wherein the second inspection step comprises:
placing the substrate in the heating chamber and heating the substrate to the second temperature;
enabling the light-emitting module to provide the second light such that the second light passes through the substrate to form a second inspection light; and
receiving the second inspection light by the camera module to obtain the second phase difference.

### Claim 12 (depends on 10)

The manufacturing method of the electronic device according to claim 10, wherein a refractive index of the heating chamber is greater than or equal to 1.4 and less than or equal to 1.6.

### Claim 13 (depends on 12)

The manufacturing method of the electronic device according to claim 12, wherein the refractive index of the heating chamber is equal to a refractive index of the substrate.

### Claim 14 (depends on 10)

The manufacturing method of the electronic device according to claim 10, wherein the light-emitting module comprises a first polarizer, and the camera module comprises a second polarizer.

### Claim 15 (depends on 10)

The manufacturing method of the electronic device according to claim 10, wherein the first equipment further comprises an oxygen detector connected to the heating chamber, and the manufacturing method of the electronic device further comprises detecting an oxygen concentration inside the heating chamber by the oxygen detector before heating the substrate.

### Claim 16 (depends on 15)

The manufacturing method of the electronic device according to claim 15, wherein the substrate is heated when the oxygen concentration is less than 20 parts per million.

### Claim 17 (depends on 10)

The manufacturing method of the electronic device according to claim 10, further comprising introducing nitrogen gas into the heating chamber before heating the substrate.

### Claim 18 (depends on 10)

The manufacturing method of the electronic device according to claim 10, wherein the heating chamber and the light-emitting module are movable along a first direction, and the first direction is perpendicular to a normal direction of the substrate.

### Claim 19 (depends on 18)

The manufacturing method of the electronic device according to claim 18, wherein the camera module is movable along a second direction, and the second direction is perpendicular to both the first direction and the normal direction of the substrate.

### Claim 20 (depends on 18)

The manufacturing method of the electronic device according to claim 18, wherein the first equipment further comprises another camera module, and an included angle between a light-receiving direction of the another camera module and the normal direction of the substrate is different from an included angle between a light-receiving direction of the camera module and the normal direction of the substrate.