# US 2026/0231712 A1 · Method of cleaning semiconductor wafer, method of producing semiconductor wafer, and semiconductor wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0231712 A1
- Document ID: US20260231712A1
- Status: Published application
- Kind: A1
- Application number: 19/152,207
- Filed: 2023-12-14
- Published: 2026-08-06
- Earliest claimed: 2023-02-22
- Assignees: Sumco Corporation
- Applicants: SUMCO Corporation
- Inventors: Ryoichi YANAI
- Web page: https://patentgrep.com/patent/US20260231712A1

## CPC

- H10P 70/15: {by wet cleaning only (H10P70/52 takes precedence)}
- H10P 70/56: {Cleaning of wafer backside}
- H10P 72/0414: {using mainly spraying means, e.g. nozzles}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method of cleaning a semiconductor wafer that can suppress occurrence of ladle-shaped defects. The method of cleaning a semiconductor wafer includes a spin cleaning process of supplying a cleaning liquid to at least a front surface of the semiconductor wafer while rotating the semiconductor wafer. The spin cleaning process includes one or more sets of combinations of an ozonized water cleaning process in which the cleaning liquid is ozonized water, followed by a hydrofluoric acid cleaning process in which the cleaning liquid is hydrofluoric acid. The method further includes a pretreatment process, prior to the spin cleaning process, of supplying a conductive liquid selected from the group consisting of hydrofluoric acid, carbonated water, and carbonated ozonized water to only a back surface of the semiconductor wafer while rotating the semiconductor wafer.

## Claims

### Claim 1

A method of cleaning a semiconductor wafer, the method comprising:
a spin cleaning process of supplying a cleaning liquid to at least a front surface of the semiconductor wafer while rotating the semiconductor wafer,
the spin cleaning process including one or more sets of combinations of an ozonized water cleaning process in which the cleaning liquid is ozonized water, followed by a hydrofluoric acid cleaning process in which the cleaning liquid is hydrofluoric acid; and
a pretreatment process, prior to the spin cleaning process, of supplying a conductive liquid selected from the group consisting of hydrofluoric acid, carbonated water, and carbonated ozonized water to only a back surface of the semiconductor wafer while rotating the semiconductor wafer.

### Claim 2 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein the conductive liquid is hydrofluoric acid.

### Claim 3 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein the conductive liquid is carbonated water.

### Claim 4 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein the conductive liquid is carbonated ozonized water.

### Claim 5 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein a rotation speed of the semiconductor wafer in the pretreatment process is 10 rpm or more and 100 rpm or less.

### Claim 6 (depends on 5)

The method of cleaning a semiconductor wafer according to claim 5, wherein the spin cleaning process comprises a first period during which the rotation speed of the semiconductor wafer is the same as the rotation speed of the semiconductor wafer in the pretreatment process, followed by a second period during which the rotation speed of the semiconductor wafer is greater than 100 rpm and 1000 rpm or less.

### Claim 7 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein a flow rate of the conductive liquid in the pretreatment process is 0.3 L/min or more and 1.5 L/min or less.

### Claim 8 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein a supply time of the conductive liquid in the pretreatment process is 1.0 s or longer to 5.0 s or shorter.

### Claim 9 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein the conductive liquid is ejected from a nozzle via a piping line and supplied to the back surface of the semiconductor wafer, and the piping line and the nozzle are made of non-metallic material.

### Claim 10 (depends on 1)

The method of cleaning a semiconductor wafer according to claim 1, wherein the semiconductor wafer is a silicon wafer.

### Claim 11 (depends on 1)

A method of producing a semiconductor wafer, the method comprising the method of cleaning a semiconductor wafer according to claim 1.

### Claim 12

A semiconductor wafer before device formation, wherein
a number of defects on a front surface of the semiconductor wafer is zero, when the defects are defined as each having a convex portion that has a height of 5 nm or more and 20 nm or less and a concave portion that has a depth of 5 nm or more and 20 nm or less adjacent to the convex portion.