# US 2026/0229555 A1 · Bonding layer for an electrode in solid oxide fuel cells and method of manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0229555 A1
- Document ID: US20260229555A1
- Status: Published application
- Kind: A1
- Application number: 19/468,709
- Filed: 2026-02-03
- Published: 2026-08-06
- Earliest claimed: 2025-02-03
- Applicants: University of Connecticut
- Inventors: Xiao-Dong Zhou; Yudong Wang; Nengneng Xu; Zizhou He; Christabel Adjah-Tetteh
- Web page: https://patentgrep.com/patent/US20260229555A1

## CPC

- H01M 8/0236: Glass; Ceramics; Cermets
- H01M 8/12: operating at high temperature, e.g. with stabilised ZrO2 electrolyte
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A bonding layer disposed on a substrate is disclosed. The bonding layer includes a single-phase spinel-type metal oxide having a nominal composition MnxCo3-xO4, where x ranges from 0 to 3, excluding x=2. The bonding layer is formed by sintering a reduced calcined intermediate, during which the reduced calcined intermediate is reoxidized to form the single-phase spinel-type metal oxide. The reduced calcined intermediate is derived from a calcined intermediate produced by calcining an oxide intermediate precursor formed via a combustion reaction between an organic fuel and a precursor comprising one or more metal nitrates. The metal nitrates include manganese nitrate, cobalt nitrate, iron nitrate, copper nitrate, nickel nitrate, zinc nitrate, or combinations thereof. Also disclosed herein is a method of forming the bonding layer.

## Claims

### Claim 1

A bonding layer disposed on a substrate, the bonding layer comprising:
a single-phase spinel-type metal oxide having a nominal composition of MnxCo3-xO4, where x ranges from 0 to 3, excluding x=2,
wherein the bonding layer is formed by sintering a reduced calcined intermediate such that the reduced calcined intermediate is reoxidized during the sintering to form the single-phase spinel-type metal oxide, and
wherein the reduced calcined intermediate is from a calcined intermediate produced by calcining an oxide intermediate precursor formed by a combustion reaction between an organic fuel and a precursor comprising one or more metal nitrates that comprise manganese nitrate, cobalt nitrate, iron nitrate, copper nitrate, nickel nitrate, zinc nitrate, and a combination thereof.

### Claim 2 (depends on 1)

The bonding layer of claim 1, wherein the one or more metal nitrates comprise manganese nitrate Mn(NO3)2·xH2O and cobalt nitrate Co(NO3)2·xH2O, where x is greater than zero.

### Claim 3 (depends on 1)

The bonding layer of claim 1, wherein the single-phase spinel-type metal oxide has a cubic, a distorted cubic, or a tetragonal crystal structure.

### Claim 4 (depends on 1)

The bonding layer of claim 1, wherein the single-phase spinel-type metal oxide is substantially free of secondary oxide phases comprising CoO and Mn2O3, as determined by X-ray diffraction.

### Claim 5 (depends on 1)

The bonding layer of claim 1, wherein x is about 0.5 to about 2.5.

### Claim 6 (depends on 1)

The bonding layer of claim 1, wherein the bonding layer has a thickness of about 5 micrometers to about 100 micrometers.

### Claim 7 (depends on 1)

The bonding layer of claim 1, wherein the bonding layer provides mechanical bonding and electrical contact between the substrate and an adjacent component, wherein the substrate and the adjacent component comprise an anode, a cathode, or an interconnect of a solid oxide fuel cell.

### Claim 8 (depends on 1)

The bonding layer of claim 1, wherein the bonding layer exhibits an area-specific resistance of less than 0.1 Ω·cm2 at an operating temperature of a solid oxide fuel cell.

### Claim 9

A method of forming a bonding layer on a substrate, the method comprising forming a first mixture comprising a precursor, an organic fuel, and a first solvent, wherein the precursor comprises one or more metal nitrates comprising manganese nitrate, cobalt nitrate, iron nitrate, copper nitrate, nickel nitrate, zinc nitrate, and a combination thereof;
stirring the first mixture to form a homogeneous first mixture;
heating the homogeneous first mixture at a first temperature to evaporate the first solvent and form a gel-like first mixture;
heating the gel-like first mixture at a second temperature to initiate a combustion reaction between the organic fuel and the one or more metal nitrates and thereby form an oxide intermediate precursor;
calcining the oxide intermediate precursor at a third temperature in an oxidizing atmosphere to form a calcined intermediate comprising a manganese-cobalt spinel oxide having a nominal composition of MnxCo3-xO4, where x ranges from 0 to 3, excluding x=2;
exposing the calcined intermediate to a reducing gas mixture at a fourth temperature to at least partially reduce the calcined intermediate and form a reduced calcined intermediate;
forming a contact paste comprising the reduced calcined intermediate and an organic constituent and
applying the contact paste to a surface of the substrate and sintering the contact paste at a fifth temperature to remove the organic constituent and form the bonding layer on the substrate, wherein the bonding layer comprises a single-phase spinel-type metal oxide formed by reoxidation of the reduced calcined intermediate during the sintering.

### Claim 10 (depends on 9)

The method of claim 9, wherein forming the contact paste comprises grinding and sieving the reduced calcined intermediate to form a powder having a maximum particle size of 5 micrometers, wherein the grinding comprises ball milling, attrition milling, bead milling, planetary milling, vibratory milling, rod milling, jet milling, a combination thereof.

### Claim 11 (depends on 9)

The method of claim 9, wherein the one or more metal nitrates comprise manganese nitrate Mn(NO3)2·xH2O and cobalt nitrate Co(NO3)2·xH2O, where x is greater than zero.

### Claim 12 (depends on 9)

The method of claim 9, wherein the first temperature is about 130° C. to about 180° C., the second temperature is about 300° C. to about 400° C., the third temperature is about 400° C. to about 600° C., the fourth temperature is about 700° C. to about 800° C., and the fifth temperature is less than 900° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein the fifth temperature is between 75° and 850° C.

### Claim 14 (depends on 9)

The method of claim 9, wherein the organic fuel comprises glycine and wherein the first solvent comprises distilled water, deionized water, or purified water.

### Claim 15 (depends on 9)

The method of claim 9, wherein the organic constituent comprise a binder and a second solvent, wherein the binder comprises ethyl cellulose, polyvinyl butyral, acrylic binders, or a combination thereof, and the second solvent comprises terpineol, alcohols, glycols, or a combination thereof.

### Claim 16 (depends on 9)

The method of claim 9, wherein a molar ratio of the organic fuel to nitrate ions of the one or more metal nitrates is about 1:1.

### Claim 17 (depends on 9)

The method of claim 9, wherein the reducing gas mixture comprises hydrogen and an inert gas, wherein the inert gas comprises argon or nitrogen.

### Claim 18 (depends on 9)

The method of claim 9, wherein the precursor has a maximum particle size of 20 micrometers (μm), and wherein the precursor has an average particle diameter of about 0.1 μm to about 20 μm.

### Claim 19

A solid oxide fuel cell, comprising:
an anode, a cathode, an electrolyte disposed between the anode and the cathode, and an interconnect electrically coupled to at least one of the anode or the cathode; and
a bonding layer disposed on at least one of the anode, the cathode, or the interconnect, wherein the bonding layer comprises a single-phase spinel-type metal oxide having a nominal composition MnxCo3-xO4, where x ranges from 0 to 3, excluding x=2,
wherein the bonding layer is formed by sintering a reduced calcined intermediate such that the reduced calcined intermediate is reoxidized during the sintering to form the single-phase spinel-type metal oxide, and
wherein the reduced calcined intermediate is derived from a calcined intermediate produced by calcining an oxide intermediate precursor formed by a combustion reaction between an organic fuel and a precursor comprising one or more metal nitrates comprising manganese nitrate, cobalt nitrate, iron nitrate, copper nitrate, nickel nitrate, zinc nitrate, or a combination thereof.