# US 2026/0226645 A1 · Electrodeposition of Thin Copper Films on Conductive Substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0226645 A1
- Document ID: US20260226645A1
- Status: Published application
- Kind: A1
- Application number: 19/145,142
- Filed: 2024-01-16
- Published: 2026-08-06
- Earliest claimed: 2023-01-18
- Assignees: MacDermid Enthone Inc.
- Applicants: MacDermid Enthone Inc.
- Inventors: Lian Guo; Jianwen Han; Eric Yakobson; Wenbo Shao; Kyle M. Whitten; Elie H. Najjar
- Web page: https://patentgrep.com/patent/US20260226645A1

## CPC

- C25D 3/38: of copper
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- C25D 5/38: of refractory metals or nickel
- C25D 7/00: Electroplating characterised by the article coated
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A copper electrolyte comprising (a) a water soluble copper salt; (b) a complexant; (c) a leveler; (d) optionally a polar solvent; (e) optionally, a pH adjuster; and (f) balance water. The copper electrolyte has a pH in the range of about 8 to about 11, preferably about 8.2 to about 9.5. The copper electrolyte can be used to deposit an ultrathin copper layer on a conductive substrate that is free of pinholes and other defects and that suppresses metal dissolution.

## Claims

### Claim 1

A copper electrolyte comprising:
a. a water soluble copper salt;
b. a complexant;
c. a leveler;
d. optionally a polar solvent;
e. optionally, a pH adjuster; and
f. balance water,
wherein the copper electrolyte has a pH in the range of about 8 to about 11.

### Claim 2 (depends on 1)

The copper electrolyte according to claim 1, wherein the water soluble copper salt comprises a copper (II) salt.

### Claim 3 (depends on 2)

The copper electrolyte according to claim 2, wherein the copper (II) salt is selected from the group consisting of copper (II) sulfate, copper (II) chloride, and copper (II) acetate.

### Claim 4 (depends on 3)

The copper electrolyte according to claim 3, wherein the copper (II) salt comprises copper (II) sulfate.

### Claim 5 (depends on 1)

The copper electrolyte according to claim 1, wherein the complexant is selected from the group consisting of citric acid, tartaric acid, ethylenediaminetetraacetic acid (EDTA), N-(hydroxyethyl)-ethylenediaminetriacetic acid (HEDTA), ethylenediamine, 1,6 diamino-cyclohexane, diethylene-triamine, triethylene-tetramine, N,N,N,N-tetramethyl-ethylene-diamine, N,N-Bis(2-hydroxyethyl)ethylenediamine, N,N,N,N-tetrakis(2-hydroxyethyl)ethylenediamine, glycine, 2-amino-ethyl-phosphonic acid, salicylic acid, salicylhydroxamic acid, catechol, 1,2-dihydroxybenzene-4-sulfonic acid, acetylacetone, acetylacetonate, dimethylglyoxime and 1,3-diamino-propane.

### Claim 6 (depends on 5)

The copper electrolyte according to claim 5, wherein the complexant comprises diethylenetriamine.

### Claim 7 (depends on 1)

The copper electrolyte according to claim 1, wherein the leveler is selected from the group consisting of polyethylene imine and derivatives thereof, quaternized polyethylene imine, polyglycine, poly(allylamine), polyaniline, polyurea, polyacrylamide, poly(melamine-co-formaldehyde), reaction products of amines with epichlorohydrin, reaction products of an amine, epichlorohydrin, and polyalkylene oxide, reaction products of an amine with a polyepoxide, polyvinylpyridine, and polyvinylimidazole.

### Claim 8 (depends on 1)

The copper electrolyte according to claim 1, wherein the pH adjuster is selected from the group consisting of tetraethylammonium hydroxide and tetrabutylammonium hydroxide.

### Claim 9 (depends on 1)

The copper electrolyte according to claim 1, wherein the polar solvent is present in the electrolyte and is selected from the group consisting of ethylene glycol, propylene glycol, glycerol, ethylene glycol monomethyl either, ethylene glycol monoethyl ether, ethylene glycol monopropyl ether, dipropylene glycol monomethyl ether and combinations of the foregoing.

### Claim 10 (depends on 9)

The copper electrolyte according to claim 9, wherein the polar solvent is glycerol.

### Claim 11 (depends on 1)

The copper electrolyte according to claim 1, comprising:
a. about 40 to about 80 g/L of the water soluble copper salt;
b. about 4 to about 20 g/L of the complexant; and
c. about 15 to about 25 g/L of the leveler.

### Claim 12 (depends on 9)

The copper electrolyte according to claim 9, comprising:
a. about 2 to about 25 g/L of the water soluble copper salt;
b. about 0.1 to about 2.0 g/L of the complexant;
c. about 2 to about 8 g/L of the leveler; and
d. about 150 to 250 g/L of the polar solvent.

### Claim 13

A copper electrolyte consisting essentially of:
a. a water soluble copper salt;
b. a complexant;
c. a leveler;
d. 0 to 300 g/L of a polar solvent;
e. optionally, a pH adjuster; and
f. balance water,
wherein the copper electrolyte has a pH in the range of about 8 to about 11.

### Claim 14

A copper electrolyte consisting of:
a. a water soluble copper salt;
b. a complexant;
c. a leveler;
d. 0 to 300 g/L of a polar solvent;
e. optionally, a pH adjuster; and
f. balance water,
wherein the copper electrolyte has a pH in the range of about 8 to about 11.

### Claim 15

A method of depositing a copper film on a conductive substrate, the method comprising the steps of:
a) optionally, pretreating the conductive substrate, wherein the pretreatment step removes surface oxides; and
b) immersing the conductive substrate into a copper electrolyte, wherein the copper electrolyte comprises:
a. a water soluble copper salt;
b. a complexant;
c. a leveler;
d. optionally a polar solvent;
e. optionally, a pH adjuster; and
f. balance water,
wherein the copper electrolyte has a pH in the range of about 8 to about 11, and
c) electrodepositing the copper film on the conductive substrate using the copper electrolyte described herein, wherein the copper film is an ultrathin copper film having a thickness of less than about 5 nm, wherein the ultrathin copper film is a continuous copper film that is free of any pinholes or other defects.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the pretreatment step comprises contacting the conductive substrate with a pretreatment solution containing a dilute weak acid.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the dilute weak acid comprises a solution of citric acid.

### Claim 18 (depends on 15)

The method according to claim 15, wherein the ultrathin copper film has a thickness of less than 4 nm.

### Claim 19 (depends on 1)

The copper electrolyte according to claim 1, wherein the copper electrolyte has a pH in the range of about 8.2 to about 9.5.