# US 2026/0226606 A1 · MAX-Ag ELECTRICALLY CONDUCTIVE COMPOSITE COATING AND PREPARATION METHOD THEREOF

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0226606 A1
- Document ID: US20260226606A1
- Status: Published application
- Kind: A1
- Application number: 19/150,748
- Filed: 2024-04-16
- Published: 2026-08-06
- Earliest claimed: 2023-07-18
- Assignees: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences
- Applicants: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences
- Inventors: Aiying WANG; Zhenyu WANG; Guanshui MA; Li WANG
- Web page: https://patentgrep.com/patent/US20260226606A1

## CPC

- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/0021: {Reactive sputtering or evaporation}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/021: {Cleaning or etching treatments}
- C23C 14/022: {by means of bombardment with energetic particles or radiation}
- C23C 14/028: {Physical treatment to alter the texture of the substrate surface, e.g. grinding, polishing}
- C23C 14/0635: {Carbides}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/165: {by cathodic sputtering}
- C23C 14/325: {Electric arc evaporation}
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C23C 14/345: {using substrate bias}
- C23C 14/3485: {using pulsed power to the target}
- C23C 14/352: {using more than one target (C23C14/56 takes precedence)}
- C23C 14/5806: {Thermal treatment}
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- Y02E 60/10: Energy storage using batteries
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed a MAX-Ag electrically conductive composite coating and a preparation method thereof. The electrically conductive composite coating comprises a MAX phase and an Ag phase. The chemical formula of the MAX phase is Mn+1AXn, where M is a transition metal element, A is an Al element, X is a C or N element, and n is an integer of 1 to 3. The MAX phase is in a lath-like structure, the Ag phase is in a nano-twinned structure, and the Ag phase is aggregated at a grain boundary of the MAX phase. The electrically conductive composite coating as a whole is in an Ag-wrapped MAX phase structure. In the present disclosure, a grain shape heterogeneous design is performed on the MAX phase coating by Ag element doping. The Ag doping affects the growth of the MAX phase grain, so that the MAX phase grain is in a lath-like structure.

## Claims

### Claim 1

A MAX-Ag electrically conductive composite coating, wherein the electrically conductive composite coating comprises a MAX phase and an Ag phase, the chemical formula of the MAX phase is Mn+1AXn, in the formula, M is selected from one of Cr, Ti, and Zr, A is an Al element, X is a C or N element, and n is an integer of 1 to 3, the MAX phase is in a lath-like structure, the Ag phase is in a nano-twinned structure, the Ag phase is aggregated at a grain boundary of the MAX phase, the electrically conductive composite coating as a whole is in an Ag-wrapped MAX phase structure, the Ag content in the electrically conductive composite coating is 1 at. % to 10 at. %, and the preparation method of the MAX-Ag electrically conductive composite coating comprises the following steps:
S1. providing a substrate, and sequentially performing mechanical polishing, ultrasonic cleaning and glow cleaning on the substrate;
S2. placing the substrate in a vacuum chamber, using a simple substance target of M element as an arc target, introducing a reaction gas for providing X element and an inert gas, and depositing an M-X layer by an arc ion plating technology;
S3. using the composite target of A element and Ag as a DC pulsed magnetron sputtering target, and depositing an A—Ag—X layer by the magnetron sputtering technology;
S4. repeating the steps S2 and S3 for 2 to 20 times to form an M-X/A—Ag—X alternately laminated coating;
S5. performing vacuum heat treatment on the alternately laminated coating obtained in the step S4 to obtain a MAX-Ag electrically conductive composite coating.

### Claim 2 (depends on 1)

The MAX-Ag electrically conductive composite coating according to claim 1, wherein the MAX phase has a grain width of 10-90 nm and a grain length of 25-300 nm.

### Claim 3 (depends on 2)

The MAX-Ag electrically conductive composite coating according to claim 2, wherein the MAX phase has a grain aspect ratio of between 2 and 7.

### Claim 4 (depends on 1)

The MAX-Ag electrically conductive composite coating according to claim 1, wherein the Ag phase aggregated at the grain boundary of the MAX phase has a thickness of 1-20 nm.

### Claim 5 (depends on 1)

The MAX-Ag electrically conductive composite coating according to claim 1, wherein the MAX phase is selected from one of Cr2AlC, Cr2AlN, Ti2AlC, Ti2AlN and Zr2AlC.

### Claim 6 (depends on 1)

A preparation method of the MAX-Ag electrically conductive composite coating according to claim 1, wherein the method comprises the following steps:
S1. providing a substrate, and sequentially performing mechanical polishing, ultrasonic cleaning and glow cleaning on the substrate;
S2. placing the substrate in a vacuum chamber, using a simple substance target of M element as an arc target, introducing a reaction gas for providing X element and an inert gas, and depositing an M-X layer by an arc ion plating technology;
S3. using the composite target of A element and Ag as a DC pulsed magnetron sputtering target, and depositing an A—Ag—X layer by the magnetron sputtering technology;
S4. repeating the steps S2 and S3 for 2 to 20 times to form an M-X/A—Ag—X alternately laminated coating;
S5. performing vacuum heat treatment on the alternately laminated coating obtained in the step S4 to obtain a MAX-Ag electrically conductive composite coating.

### Claim 7 (depends on 6)

The preparation method of the MAX-Ag electrically conductive composite coating according to claim 6, wherein in the step S2, the substrate has a bias voltage of (−50)-(−200) V, the target-to-substrate distance between the substrate and the cathode arc target is 15-20 cm, the cathode arc target has a power of 1-3 kW and a current of 30-70 A, the reaction gas is introduced at a flow rate of 15-30 sccm, the inert gas is introduced at a flow rate of 150-200 sccm, and the deposition time is 5-30 min.

### Claim 8 (depends on 6)

The preparation method of the MAX-Ag electrically conductive composite coating according to claim 6, wherein in the step S3, the substrate has a bias voltage of (−50)-(−200) V, the target-to-substrate distance between the substrate and the DC pulsed magnetron sputtering target is 10-15 cm, the DC pulsed magnetron sputtering target has a power of 2-3.5 kW, the reaction gas is introduced at a flow rate of 15-30 sccm, the inert gas is introduced at a flow rate of 150-200 sccm, and the deposition time is 5-30 min.

### Claim 9 (depends on 6)