# US 2026/0226601 A1 · Zinc-aluminum-magnesium-plated steel plate and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0226601 A1
- Document ID: US20260226601A1
- Status: Published application
- Kind: A1
- Application number: 19/146,200
- Filed: 2024-01-09
- Published: 2026-08-06
- Earliest claimed: 2023-01-10
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Kai Wang; Xinyan Jin; Yuling Ren; Chuanhua Lin; Shaoming Qiang; Liangquan Shi
- Web page: https://patentgrep.com/patent/US20260226601A1

## CPC

- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- B05D 3/0263: {with IR heaters}
- C22C 18/04: with aluminium as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/12: Aluminium or alloys based thereon
- C23C 2/26: After-treatment (C23C2/14 takes precedence)
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- B05D 5/00: Processes for applying liquids or other fluent materials to surfaces to obtain special surface effects, finishes or structures
- B05D 2202/10: based on Fe
- B05D 2350/65: metal layer
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A zinc-aluminum-magnesium-plated steel plate and manufacturing method therefor. The steel plate comprises a steel substrate and a plating layer provided on the steel substrate, and the surface of the plating layer is coated with a fingerprint-resistant film; the plating layer comprises the following components in mass percentage: Al: 45%-65%, Mg: 0.2%-5.0%, Si: 0.1%-3.0%, Zr: 0.001%-0.15%, Ca: 0.001%-0.15%, and the balance being Zn and inevitable impurities.

## Claims

### Claim 1

A zinc-aluminum-magnesium-plated steel plate, comprising a steel substrate and a plating layer provided on the steel substrate, wherein the surface of the plating layer is coated with a fingerprint-resistant film; the plating layer comprises the following components in mass percentage: Al: 45%-65%, Mg: 0.2%-5.0%, Si: 0.1%-3.0%, Zr: 0.001%-0.15%, Ca: 0.001%-0.15%, and the balance being Zn and inevitable impurities.

### Claim 2 (depends on 1)

The zinc-aluminum-magnesium-plated steel plate according to claim 1, wherein the mass percentage contents of each component in the plating layer satisfy at least one of the following:
Al
:
50
⁢
%
-
60
⁢
%
,
Mg
:
1.
%
-
3.
%
,
Si
:
1.
%
-
2.
%
,
Zr
:
0.01
%
-
0.1
%
,
Ca
:
0.01
%
-
0.1
%
.

### Claim 3 (depends on 1)

The zinc-aluminum-magnesium-plated steel plate according to claim 1, wherein the plating layer has a thickness of 8-38 km.

### Claim 4 (depends on 1)

The zinc-aluminum-magnesium-plated steel plate according to claim 1, wherein the fingerprint-resistant film has a thickness of 0.5-2.5 km.

### Claim 5 (depends on 4)

The zinc-aluminum-magnesium-plated steel plate according to claim 4, wherein the fingerprint-resistant film has a thickness of 1.0-2.0 km.

### Claim 6 (depends on 1)

The zinc-aluminum-magnesium-plated steel plate according to claim 1, wherein a surface color difference ΔE of the zinc-aluminum-magnesium-plated steel plate before and after treatment for 24 hours under laminated humid-heat conditions is <3, where ΔE is the difference between the surface lightness value before laminated humid-heat treatment and the surface lightness value after 24 hours of humid-heat treatment.

### Claim 7 (depends on 1)

A method for manufacturing the zinc-aluminum-magnesium-plated steel plate according to claim 1, wherein the method comprises the following steps carried out in sequence:
(1) performing a pretreatment for a steel substrate;
(2) feeding the pretreated steel substrate into a plating bath to perform hot-dip galvanizing in the plating bath, obtaining a plated steel plate;
(3) after the plated steel plate leaves the plating bath, performing staged cooling as follows: a first stage is air cooling, the steel plate is cooled to 300° C. or less, a cooling rate of the first stage is 10-60° C./s; a second step is roll cooling or roll cooling+air cooling, in which a cooling rate of roll cooling is 60-100° C./s; a third step is water-cooling in a quenching water tank, and a plate temperature is lower than 100° C. when the plated steel plate enters the quenching water tank;
(4) coating a fingerprint-resistant film on the surface of the plated steel plate and heating and baking at 100-160° C. to cure the film;
(5) cooling the plated steel plate to room temperature;
(6) coiling the plated steel plate into a finished product coil.

### Claim 8 (depends on 7)

The method according to claim 7, wherein in step (2), a temperature of the plating bath is 570-610° C.; and/or in step (3), the second stage is roll cooling+air cooling, in which a cooling rate of roll cooling is 60-100° C./s, and a cooling rate of air cooling is 20-30° C./s.

### Claim 9 (depends on 7)

The method according to claim 7, wherein in step (4), the heating and baking is performed at 110-140° C.

### Claim 10 (depends on 7)

The method according to in claim 7, wherein, in step (4), the heating and baking is performed by electromagnetic induction heating.

### Claim 11 (depends on 7)

The method according to claim 7, wherein, in step (5), the cooling is performed by air cooling, and a cooling rate of the plated steel plate is 5-20° C./s.

### Claim 12 (depends on 2)

The zinc-aluminum-magnesium-plated steel plate according to claim 2, wherein a surface color difference ΔE of the zinc-aluminum-magnesium-plated steel plate before and after treatment for 24 hours under laminated humid-heat conditions is <3, where ΔE is the difference between the surface lightness value before laminated humid-heat treatment and the surface lightness value after 24 hours of humid-heat treatment.

### Claim 13 (depends on 3)

The zinc-aluminum-magnesium-plated steel plate according to claim 3, wherein a surface color difference ΔE of the zinc-aluminum-magnesium-plated steel plate before and after treatment for 24 hours under laminated humid-heat conditions is <3, where ΔE is the difference between the surface lightness value before laminated humid-heat treatment and the surface lightness value after 24 hours of humid-heat treatment.

### Claim 14 (depends on 4)

The zinc-aluminum-magnesium-plated steel plate according to claim 4, wherein a surface color difference ΔE of the zinc-aluminum-magnesium-plated steel plate before and after treatment for 24 hours under laminated humid-heat conditions is <3, where ΔE is the difference between the surface lightness value before laminated humid-heat treatment and the surface lightness value after 24 hours of humid-heat treatment.

### Claim 15 (depends on 5)

The zinc-aluminum-magnesium-plated steel plate according to claim 5, wherein a surface color difference ΔE of the zinc-aluminum-magnesium-plated steel plate before and after treatment for 24 hours under laminated humid-heat conditions is <3, where ΔE is the difference between the surface lightness value before laminated humid-heat treatment and the surface lightness value after 24 hours of humid-heat treatment.