# US 2026/0226238 A1 · Polymer Networks and Composites of Tunable Structures and Methods of Their Production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0226238 A1
- Document ID: US20260226238A1
- Status: Published application
- Kind: A1
- Application number: 19/150,501
- Filed: 2024-01-25
- Published: 2026-08-06
- Earliest claimed: 2023-01-27
- Assignees: The Regents of the University of California
- Applicants: The Regents of the University of California
- Inventors: Ximin He; Yousif Alsaid; Yichen Yan
- Web page: https://patentgrep.com/patent/US20260226238A1

## CPC

- C08J 3/075: Macromolecular gels
- C08K 3/30: Sulfur-, selenium- or tellurium-containing compounds
- H01M 4/38: of elements or alloys
- H01M 4/606: {containing aromatic main chain polymers}
- H01M 10/38: Construction or manufacture
- C08J 2329/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C08J 2333/26: Homopolymers or copolymers of acrylamide or methacrylamide
- C08K 2003/3045: {Sulfates}
- H01M 2300/0005: Acid electrolytes
- H01M 2300/0085: Immobilising or gelification of electrolyte
- Y02E 60/10: Energy storage using batteries
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Systems and methods for producing structured hydrogel electrolytes with interconnected pores are described. The methods implement the cononsolvency effect and the salting, out effect. The hydrogel electrolytes have enhanced mass transport and mechanical properties, and anti-freezing properties, suitable for applications in harsh conditions.

## Claims

### Claim 1

A method of fabricating a hydrogel comprising:
mixing a solute, a solvent, and a cosolvent to form a hydrogel via a cononsolvency effect, wherein the solute dissolves in the solvent and the cosolvent, wherein the solvent and the cosolvent are miscible and have different polarity; and
solidifying the hydrogel in a salt solution, wherein the salt solution induces a formation of a plurality of hydrogen bonds in the hydrogel such that the hydrogel toughens.

### Claim 2 (depends on 1)

The method of claim 1, wherein the cosolvent has a stronger interaction with the solute than the solvent.

### Claim 3 (depends on 1)

The method of claim 1, further comprising heating and stirring the mixed solute, solvent, and cosolvent to form a homogeneous solution before forming a hydrogel.

### Claim 4 (depends on 1)

The method of claim 1, further comprising forming the hydrogel in a mold to achieve a desired shape.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hydrogel is formed in a freezer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solute is a polymer selected from the group consisting of poly(n-isopropyl acrylamide) (PNIPAM), poly(vinyl alcohol) (PVA), polyacrylamide (PAM), and poly(N-tert-butyl acrylamide)-co-polyacrylamide (PNTBAM-co-PAM).

### Claim 7 (depends on 1)

The method of claim 1, wherein the solute is PVA, the solvent is dimethyl sulfoxide (DMSO), the cosolvent is water, and the salt solution comprises zinc sulfate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the toughened hydrogel has a tensile strength of at least 1.5 MPa, a toughness of at least 4.5 MJ/m3, and an ionic conductivity of at least 4.7 mS/cm at −20° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein the toughened hydrogel is anti-freezing at a temperature lower than or equal to −20° C. and is configured to be a portion of a zinc ion battery.

### Claim 10 (depends on 9)

The method of claim 9, wherein the zinc ion battery is a zinc polyaniline battery, and the battery is dendrite-free after at least 3000 cycles from 25° C. to −20° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the solute is selected from the group consisting of PNIPAM, PVA and PNTBAM-co-PAM, the solvent is DMSO, the cosolvent is water, and the salt solution comprises potassium acetate and zinc acetate.

### Claim 12 (depends on 11)

The method of claim 11, wherein the toughened hydrogel has a tensile strength of at least 15 MPa, a toughness of at least 84 MJ/m3, a Young's modulus of at least 8 MPa, and an ionic conductivity of at least 50 mS/cm at 20° C.

### Claim 13 (depends on 11)

The method of claim 11, wherein the toughened hydrogel is anti-freezing at a temperature lower than or equal to −80° C. and is configured to be a portion of a zinc ion battery.

### Claim 14 (depends on 13)

The method of claim 13, wherein the zinc ion battery is a zinc polyaniline battery, the battery is dendrite-free after at least 30,000 cycles from 25° C. to −20° C., and the battery has a reversible capacity of 50 mA h g−1 after 1,000 cycles at 25° C., and a reversible capacity of 57 mA h g−1 after 30,000 cycles at −20° C.

### Claim 15

A method of fabricating a zinc ion battery comprising:
forming a cathode and an anode for a zinc ion battery, and
forming a hydrogel electrolyte positioned in between the cathode and the anode, wherein the hydrogel electrolyte is formed via a process comprising:
mixing a solute, a solvent, and a cosolvent to form a hydrogel via a cononsolvency effect, wherein the solute dissolves in the solvent and the cosolvent, wherein the solvent and the cosolvent are miscible and have different polarity; and
solidifying the hydrogel in a salt solution, wherein the salt solution induces a formation of a plurality of hydrogen bonds in the hydrogel such that the hydrogel toughens.

### Claim 16 (depends on 15)

The method of claim 15, wherein the cosolvent has a stronger interaction with the solute than the solvent.

### Claim 17 (depends on 15)

The method of claim 15, further comprising heating and stirring the mixed solute, solvent, and cosolvent to form a homogeneous solution before forming a hydrogel.

### Claim 18 (depends on 15)

The method of claim 15, further comprising forming the hydrogel in a mold to achieve a desired shape.

### Claim 19 (depends on 15)

The method of claim 15, wherein the hydrogel is formed in a freezer.

### Claim 20 (depends on 15)

The method of claim 15, wherein the solute is a polymer selected from the group consisting of poly(n-isopropyl acrylamide) (PNIPAM), poly(vinyl alcohol) (PVA), polyacrylamide (PAM), and poly(N-tert-butyl acrylamide)-co-polyacrylamide (PNTBAM-co-PAM).

### Claim 21 (depends on 15)

The method of claim 15, wherein the solute is PVA, the solvent is dimethyl sulfoxide (DMSO), the cosolvent is water, and the salt solution comprises zinc sulfate.

### Claim 22 (depends on 21)

The method of claim 21, wherein the toughened hydrogel has a tensile strength of at least 1.5 MPa, a toughness of at least 4.5 MJ/m3, and an ionic conductivity of at least 4.7 mS/cm at −20° C.

### Claim 23 (depends on 21)

The method of claim 21, wherein the toughened hydrogel is anti-freezing at a temperature lower than or equal to −20° C.

### Claim 24 (depends on 21)

The method of claim 21, wherein the battery is a zinc polyaniline battery, and the battery is dendrite-free after at least 3000 cycles from 25° C. to −20° C.

### Claim 25 (depends on 15)

The method of claim 15, wherein the solute is selected from the group consisting of PNIPAM, PVA and PNTBAM-co-PAM, the solvent is DMSO, the cosolvent is water, and the salt solution comprises potassium acetate and zinc acetate.

### Claim 26 (depends on 25)

The method of claim 25, wherein the toughened hydrogel has a tensile strength of at least 15 MPa, a toughness of at least 84 MJ/m3, a Young's modulus of at least 8 MPa, and an ionic conductivity of at least 50 mS/cm at 20° C.

### Claim 27 (depends on 15)

The method of claim 15, wherein the toughened hydrogel is anti-freezing at a temperature lower than or equal to −80° C.

### Claim 28 (depends on 15)

The method of claim 15, wherein the battery is a zinc polyaniline battery, and the battery is dendrite-free after at least 30,000 cycles from 25° C. to −20° C., and the battery has a reversible capacity of 50 mA h g−1 after 1,000 cycles at 25° C., and a reversible capacity of 57 mA h g−1 after 30,000 cycles at −20° C.