# US 2026/0226212 A1 · Bottlebrush Poly(alpha olefin) Networks

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0226212 A1
- Document ID: US20260226212A1
- Status: Published application
- Kind: A1
- Application number: 19/460,719
- Filed: 2026-01-27
- Published: 2026-08-06
- Earliest claimed: 2025-02-03
- Applicants: ExxonMobil Technology and Engineering Company
- Inventors: Carlos R. Lopez-Barron; Tzu-Pin Lin
- Web page: https://patentgrep.com/patent/US20260226212A1

## CPC

- C08F 210/18: with non-conjugated dienes, e.g. EPT rubbers
- C08F 4/76: selected from titanium, zirconium, hafnium, vanadium, niobium or tantalum
- C08J 3/247: {Heating methods}
- C08K 3/06: Sulfur
- C08K 5/14: Peroxides
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F 2500/36: Terpolymer with exactly three olefinic monomers
- C08J 2323/24: having ten or more carbon atoms
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Embodiments of the present disclosure generally relate to polymer compositions and methods to prepare polymer compositions. In one or more embodiments, a method for preparing a poly(alpha olefin) terpolymer is provided and includes introducing ethylene, one or more linear α-olefin monomers, one or more non-conjugated diene monomers, and a catalyst system to a first reactor to form a reaction mixture, the catalyst system represented by Formula (V), polymerizing the reaction mixture to form a linear polymer, and vulcanizing the polymer mixture to form a polymer composition containing the poly(alpha olefin) terpolymer. In other embodiments, a polymer composition is provided and includes a poly(alpha olefin) terpolymer prepared from a reaction product of: ethylene, one or more linear α-olefin monomers containing an unsubstituted C2 to C40 alpha olefins, and one or more non-conjugated diene monomers, wherein the poly(alpha olefin) terpolymer has a complex modulus of about 1 kPa to about 100 kPa.

## Claims

### Claim 1

A method for preparing a poly(alpha olefin) terpolymer, the method comprising:
introducing ethylene, one or more linear α-olefin monomers, one or more non-conjugated diene monomers, and a catalyst system to a first reactor to form a reaction mixture, the catalyst system represented by Formula (V):
wherein:
M is a group 4 metal;
J is N, O, S, or P;
p is 1 when J is N or P, and is 0 when J is O or S;
each R2, R3, R4, and R7 is independently hydrogen, or a C1-C50 substituted or unsubstituted hydrocarbyl, halocarbyl, silylcarbyl, or germylcarbyl;
R′ is a C1-C100 substituted or unsubstituted hydrocarbyl, halocarbyl, silylcarbyl, substituted hydrocarbyl rings, unsubstituted hydrocarbyl rings, substituted heterocyclic rings, or unsubstituted heterocyclic rings each having 5, 6, 7, or 8 ring atoms;
T is (CR8R9)x, SiR8R9 or GeR8R9 where x is 1 or 2, each R8 and R9 is independently selected from hydrogen or substituted or unsubstituted hydrocarbyl, halocarbyl, silylcarbyl, and germylcarbyl and R8 and R9 may optionally be bonded together to form a ring structure;
y is 0 or 1;
each X is C1-C100 alkyl; and
each Ra, Rb, and Rc is independently C1-C10 alkyl or hydrogen;
polymerizing the reaction mixture to form a linear polymer; and
vulcanizing the polymer mixture to form a polymer composition comprising the poly(alpha olefin) terpolymer.

### Claim 2 (depends on 1)

The method of claim 1, one or more linear α-olefin monomers are substituted or unsubstituted C2 to C40 alpha olefins.

### Claim 3 (depends on 2)

The method of claim 2, wherein the one or more α-olefin monomers are unsubstituted C10 to C18 alpha olefins.

### Claim 4 (depends on 3)

The method of claim 3, wherein the wherein the one or more α-olefin monomers are decene or 1-octadecene.

### Claim 5 (depends on 1)

The method of claim 1, wherein the one or more non-conjugated diene monomers are substituted or unsubstituted C2 to C40 olefins.

### Claim 6 (depends on 5)

The method of claim 5, wherein the one or more non-conjugated diene monomers are selected from the group consisting of 2-ethylidene-5-norborene, 5-vinyl-2-norbornene, norbornadiene,
and any combination thereof.

### Claim 7 (depends on 5)

The method of claim 5, wherein the one or more non-conjugated diene monomers are 2-ethylidene-5-norborene.

### Claim 8 (depends on 1)

The method of claim 1, wherein vulcanizing the polymer mixture comprises performing a chemical curing process or a UV curing process.

### Claim 9 (depends on 8)

The method of claim 8, wherein vulcanizing comprises the chemical curing process, and wherein performing the chemical curing process comprises introducing a crosslinking agent to the linear polymer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the crosslinking agent comprises an organic peroxide or sulfur.

### Claim 11 (depends on 8)

The method of claim 8, wherein vulcanizing comprises the UV curing process, and wherein performing the UV curing process comprises introducing a photo-initiator to the linear polymer and exposing the linear polymer to a UV light source comprising a wavelength of about 100 nm to about 500 nm.

### Claim 12

A polymer composition, the polymer composition comprising a poly(alpha olefin) terpolymer prepared from a reaction product of:
ethylene,
one or more linear α-olefin monomers comprising an unsubstituted C2 to C40 alpha olefins,
and one or more non-conjugated diene monomers selected from the group consisting of 2-ethylidene-5-norborene, 5-vinyl-2-norbornene, norbornadiene,
and any combination thereof,
wherein the poly(alpha olefin) terpolymer comprises a complex modulus of about 1 kPa to about 100 kPa.

### Claim 13 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises a non-conjugated diene content of less than 10 wt %.

### Claim 14 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises an elastic modulus of about 1 kPa to about 2 MPa.

### Claim 15 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises a tensile strength in a range from about 30 kPa to about 140 kPa, a strain at break in a range from about 200% to about 1,200%, and a permanent set in a range from about 1% to about 5%.

### Claim 16 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises a compressive strength in a range from about 1 MPa to about 1.6 MPa, a compressive set at compressive strains of less than 80% ranging about 1% to about 10%, and a hysteresis loss energy of less than 1 kJ/m3.

### Claim 17 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises a melting temperature of about 20° C. to about 130° C., and a latent heat of about 3 J/g to about 200 J/g.

### Claim 18 (depends on 17)

The polymer composition of claim 17, wherein the poly(alpha olefin) terpolymer comprises a melting temperature of about 15° C. to about 35° C., and a latent heat of less than 100 J/g.

### Claim 19 (depends on 12)

The polymer composition of claim 12, wherein the poly(alpha olefin) terpolymer comprises a storage modulus of about 1 Pa to about 100 kPa, and a maximum stress of about 0.1 kPa to about 1,000 kPa.

### Claim 20 (depends on 12)

The polymer composition of claim 12, wherein the one or more non-conjugated diene monomers comprise 2-ethylidene-5-norborene, and the poly(alpha olefin) terpolymer is represented by Formula (XI):
wherein each of k, l, m, and n is independently an integer of greater than 1.