# US 2026/0225283 A1 · Highly-insulated ingot mold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0225283 A1
- Document ID: US20260225283A1
- Status: Published application
- Kind: A1
- Application number: 19/634,300
- Filed: 2026-03-31
- Published: 2026-08-06
- Earliest claimed: 2021-08-27
- Assignees: HarbisonWalker International Holdings, Inc.
- Applicants: HarbisonWalker International Holdings, Inc.
- Inventors: Donald ABRINO
- Web page: https://patentgrep.com/patent/US20260225283A1

## CPC

- B28B 7/36: Linings or coatings, {e.g. removable, absorbent linings, permanent anti-stick coatings; Linings becoming a non-permanent layer of the moulded article}(lubricating surfaces of moulds, cores or mandrels B28B7/38)
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- B22C 1/00: Compositions of refractory mould or core materials; Grain structures thereof (refractory materials in general C04B35/00); Chemical or physical features in the formation or manufacture of moulds
- B22C 1/02: characterised by additives for special purposes, e.g. indicators, breakdown additives
- B22C 9/02: Sand moulds or like moulds for shaped castings
- C04B 35/653: Processes involving a melting step
- F27B 14/10: Crucibles
- F27D 1/0006: {Linings or walls formed from bricks or layers with a particular composition or specific characteristics}
- C04B 2237/36: Non-oxidic
- C04B 2237/363: Carbon
- C04B 2237/365: Silicon carbide
- C04B 2237/366: Aluminium nitride
- C04B 2237/368: Silicon nitride
- C04B 2237/586: by joining layers or articles of the same composition but having different densities
- C04B 2237/704: of one or more of the ceramic layers or articles
- C04B 2237/84: Joining of a first substrate with a second substrate at least partially inside the first substrate, where the bonding area is at the inside of the first substrate, e.g. one tube inside another tube
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

An ingot mold for curing fused and melted material is provided. The ingot mold includes a steel box, an insulation material layer lining an inner surface of the steel box, a foamed carbon layer formed inward of the insulation material layer, and a graphite block layer formed inward of the foamed carbon layer and positioned to contact the fused and melted material. The insulation material layer includes a non-oxide based insulation material having a service temperature of at least about 3000°F. A combined thermal resistance of the insulation material layer and the foamed carbon layer is greater than a thermal resistance of the graphite block layer.

## Claims

### Claim 1

An ingot mold for curing fused and melted material, comprising:
a steel box;
an insulation material layer lining an inner surface of the steel box, the insulation material layer comprising a non-oxide based insulation material having a service temperature of at least about 3000°F;
a foamed carbon layer formed inward of the insulation material layer; and
a graphite block layer formed inward of the foamed carbon layer and positioned to contact the fused and melted material,
wherein a combined thermal resistance of the insulation material layer and the foamed carbon layer is greater than a thermal resistance of the graphite block layer.

### Claim 2 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material has a service temperature of at least about 3300°F.

### Claim 3 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material has a service temperature of at least about 3500°F.

### Claim 4 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material has a thermal conductivity less than about 10 W/m·K at temperatures of about 3600°F or greater.

### Claim 5 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material has a porosity greater than about 40%.

### Claim 6 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material is selected from the group consisting of carbon-based materials, carbide-based materials, nitride-based materials, and combinations thereof.

### Claim 7 (depends on 6)

The ingot mold of claim 6, wherein the non-oxide based insulation material is selected from the group consisting of graphite foams, carbon foams, carbon aerogels, carbon felt, carbon fiber mats, silicon carbide foams, porous boron carbide, silicon nitride, aluminum nitride, hexagonal boron nitride, and combinations thereof.

### Claim 8 (depends on 1)

The ingot mold of claim 1, wherein the insulation material layer has a thickness from about 0.5 inches to about 6 inches.

### Claim 9 (depends on 1)

The ingot mold of claim 1, wherein the foamed carbon layer has a thickness from about 0.5 inches to about 18 inches.

### Claim 10 (depends on 1)

The ingot mold of claim 1, wherein the graphite block layer has a thickness from about 0.5 inches to about 6 inches.

### Claim 11 (depends on 1)

The ingot mold of claim 1, wherein the non-oxide based insulation material comprises a first foamed carbon layer and the foamed carbon layer formed inward thereof comprises a second foamed carbon layer.

### Claim 12 (depends on 11)

The ingot mold of claim 11, wherein the first and second foamed carbon layers differ in density, porosity, or thermal conductivity.

### Claim 13 (depends on 1)

The ingot mold of claim 1, further comprising:
a lid, comprising:
a steel frame;
a lid insulation material layer lining an inner surface of the steel frame;
a lid foamed carbon layer formed inward of the lid insulation material layer; and
a lid graphite block layer formed inward of the lid foamed carbon layer.

### Claim 14

An ingot mold for curing fused and melted material, comprising:
a steel box;
a non-oxide based insulation material layer;
a foamed carbon layer; and
a graphite block layer positioned to contact the fused and melted material,
wherein the ingot mold reduces heat flux to less than about 25% of a heat flux of a standard practice ingot mold lined solely with dense graphite blocks.

### Claim 15 (depends on 14)

The ingot mold of claim 14, wherein the ingot mold reduces heat flux to less than about 15% of the standard practice ingot mold.

### Claim 16 (depends on 14)

The ingot mold of claim 14, wherein the ingot mold reduces heat flux to less than about 10% of the standard practice ingot mold.

### Claim 17 (depends on 14)

The ingot mold of claim 14, wherein the fused and melted material cast into the mold remains within a crystal growth temperature range for at least about 12 hours following casting.

### Claim 18

A method of producing a fused cast ingot having increased crystal size, the method comprising:
pouring fused and melted material into an ingot mold, the ingot mold including a steel box, a non-oxide based insulation material layer, a foamed carbon layer, and a graphite block layer; and
allowing the material to cool within the ingot mold,
wherein the material remains within a crystal growth temperature range for at least about 12 hours following casting.

### Claim 19 (depends on 18)

The method of claim 18, wherein the material remains within the crystal growth temperature range for between about 18 hours and about 36 hours.

### Claim 20 (depends on 18)

The method of claim 18, wherein the fused and melted material is selected from the group consisting of MgO, alpha alumina, beta alumina, calcia, chromia, silica, zirconia, silicon carbide, and combinations thereof.

### Claim 21

An ingot mold for curing fused and melted material, comprising:
a steel box;
a non-oxide based insulation material layer lining an inner surface of the steel box;
a foamed carbon layer formed inward of the insulation material layer; and
a graphite block layer formed inward of the foamed carbon layer and positioned to contact the fused and melted material,
wherein the non-oxide based insulation material has a service temperature of at least about 3000°F,
wherein a combined thermal resistance of the insulation material layer and the foamed carbon layer is greater than a thermal resistance of the graphite block layer, and
wherein the ingot mold reduces heat flux to less than about 25% of a heat flux of a standard practice ingot mold lined solely with dense graphite blocks.

### Claim 22 (depends on 21)

The ingot mold of claim 21, wherein the fused and melted material cast into the mold remains within a crystal growth temperature range for at least about 12 hours following casting.