# US 2026/0221436 A1 · Positive Electrode Active Material, Method For Preparing The Same, And Positive Electrode And Lithium Secondary Battery Which Include The Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0221436 A1
- Document ID: US20260221436A1
- Status: Published application
- Kind: A1
- Application number: 19/141,968
- Filed: 2023-12-20
- Published: 2026-07-30
- Earliest claimed: 2022-12-22
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution. Ltd.
- Inventors: Jin Tae Hwang; Eun Sol Lho; Su Yeon Oh; Byung Chun Park; Sang Min Park; Sang Wook Lee; Seul Ki Kim; Hyeong II Kim
- Web page: https://patentgrep.com/patent/US20260221436A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/80: Compounds containing nickel, with or without oxygen or hydrogen, and containing one or more other elements (C01G53/02, C01G53/06 - C01G53/40 take precedence)
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/90: Other crystal-structural characteristics not specified above
- C01P 2004/03: obtained by SEM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material includes: (1) lithium nickel-based transition metal oxide particles in which a mole ratio of nickel in the total transition metals is 80 mol % or greater; and (2) a coating layer formed on a surface of the lithium nickel-based transition metal oxide particles. The lithium nickel-based transition metal oxide particles are in the form of a single particle consisting of one single nodule or a quasi-single particle, which is a composite of up to 30 nodules. The coating layer includes cobalt and aluminum, and the aluminum is contained in an amount of 0.1 mol. to 0.5 mol. with respect to 100 moles of the lithium nickel-based transition metal oxide. A method of preparing the positive electrode active material, a positive electrode including the positive electrode active material, and a lithium secondary battery including the positive electrode.

## Claims

### Claim 1

A positive electrode active material comprising:
lithium nickel-based transition metal oxide particles in which a mole ratio of is 80 mol % or greater of a total transition metal content of the lithium nickel-based transition metal oxide particles; and
a coating layer formed on a surface of the lithium nickel-based transition metal oxide particles, wherein
the lithium nickel-based transition metal oxide particles are in the form of a single particle consisting of one single nodule or a quasi-single particle, which is a composite of up to 30 nodules, and wherein
the coating layer comprises cobalt and aluminum, and
the aluminum is contained in an amount of from 0.1 mol. to 0.5 mol. with respect to 100 moles of the lithium nickel-based transition metal oxide.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein the cobalt is contained in an amount of from 0.5 mol. to 5.0 mol. with respect to 100 moles of the lithium nickel-based transition metal oxide.

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein a mole ratio of nickel is 90 mol % or greater of a total transition metal content of the lithium nickel-based transition metal oxide particles.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the coating layer is discontinuously distributed on the surface of the lithium nickel-based transition metal oxide particles.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein the positive electrode active material has a peak in a 2θrange of from 37° to 38° on an XRD graph.

### Claim 6 (depends on 1)

The positive electrode active material of claim 1, wherein the positive electrode active material has a peak in a 2θrange of from 45° to 46° on an XRD graph.

### Claim 7 (depends on 1)

The positive electrode active material of claim 1, wherein the nodule or nodules of the positive electrode active material have an average particle diameter of from 1.0 μm to 9.0 μm.

### Claim 8 (depends on 1)

The positive electrode active material of claim 1, wherein the positive electrode active material has a D50 of from 4.0 μm to 9.0 μm.

### Claim 9

A method for preparing a positive electrode active material, the method comprising:
mixing a transition metal precursor containing nickel, cobalt, and manganese with a lithium raw material to form a mixture, and subjecting the mixture to primary firing to form a lithium nickel-based transition metal oxide; and
mixing the lithium nickel-based transition metal oxide with cobalt and aluminum to form another mixture, and subjecting the mixture to secondary firing to form a positive electrode active material comprising a coating layer;
wherein in the lithium nickel-based transition metal oxide, a mole ratio of nickel is 80 mol % or greater of a total transition metal content of the lithium nickel-based transition metal oxide,
the lithium nickel-based transition metal oxide is a single particle consisting of one single nodule or a quasi-single particle, which is a composite of up to 30 nodules, and
when mixing the lithium nickel-based transition metal oxide with cobalt and aluminum, a mole ratio of aluminum to the lithium nickel-based transition metal oxide is from 0.001 to 0.005.

### Claim 10 (depends on 9)

The method of claim 9, wherein the secondary firing is performed at a temperature of from 660° C. to 720° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the coating layer is discontinuously distributed on a surface of the lithium nickel-based transition metal oxide particles.

### Claim 12 (depends on 9)

The method of claim 9, wherein the primary firing performed at a temperature of from 800° C. to 890° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein the lithium nickel-based transition metal oxide is not washed prior to mixing it with cobalt and aluminum.

### Claim 14 (depends on 1)

A positive electrode comprising the positive electrode active material of claim 1.

### Claim 15 (depends on 14)

A lithium secondary battery comprising the positive electrode of claim 14.