Preparation of Maple Wood for CTMP Production
AssigneeBillerud Aktiebolag (publ)
InventorsThomas Lindstedt, Thomas Granfeldt, Per Engstrand
Life of this patent
Estimating the term…
Abstract
There is provided a method of preparing chemithermomechanical CTMP from maple wood, said method comprising the steps of: a) providing maple wood chips having an average length below 20 mm, such as below 19 mm; b) washing the maple wood chips with water; c) steaming the washed maple wood chips for a period of at least 15 minutes to obtain pre-steamed chips; d) impregnating the pre-steamed chips to obtain impregnated chips; e) heating the impregnated chips to obtain pre-treated chips; and f) defibration of the pre-treated chips.
Claims20
A method of preparing chemithermomechanical pulp (CTMP) from maple wood, said method comprising the steps of:
- a) providing maple wood chips having an average length below 20 mm;
- b) washing the maple wood chips with water;
- c) steaming the washed maple wood chips for a period of at least 15 minutes to obtain pre-steamed chips;
- d) impregnating the pre-steamed chips to obtain impregnated chips;
- e) heating the impregnated chips to obtain pre-treated chips;
- and
- f) defibration of the pre-treated chips.
The method of clam 16, wherein the softwood is spruce.
Dependencies are inferred from the claim text.