# US 2026/0218377 A1 · Method of forming metal silicide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0218377 A1
- Document ID: US20260218377A1
- Status: Published application
- Kind: A1
- Application number: 19/459,112
- Filed: 2026-01-26
- Published: 2026-07-30
- Earliest claimed: 2025-01-29
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Jonathan Bakke; Wei Li; Sisi Wang
- Web page: https://patentgrep.com/patent/US20260218377A1

## CPC

- C23C 16/42: Silicides
- C23C 16/0245: {by etching with a plasma}
- C23C 16/45534: {Use of auxiliary reactants other than used for contributing to the composition of the main film, e.g. catalysts, activators or scavengers}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/56: After-treatment
- H10D 64/0112: {using conductive layers comprising silicides}
- H10P 14/414: {of metal-silicide materials}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods of forming a transition metal silicide are disclosed. Exemplary methods include selectively forming a transition metal silicide on a first surface relative to a second surface. The step of forming the transition metal silicide can include providing a catalyst. Additionally or alternatively, exemplary methods can include a cleaning and/or surface treatment step prior to forming the transition metal silicide. Methods described herein may be particularly useful in forming structures suitable for NMOS devices.

## Claims

### Claim 1

A method of forming a structure, the method comprising:
providing a substrate, comprising a semiconductor surface, within a reaction chamber of a reactor; and
forming a transition metal silicide layer on the semiconductor surface using a cyclical deposition process, the cyclical deposition process comprising the steps of:
providing a pulse of a transition metal precursor to the reaction chamber;
providing a pulse of a silicon precursor to the reaction chamber; and
providing a catalyst to the reaction chamber.

### Claim 2 (depends on 1)

The method of claim 1, wherein, a cycle of the cyclical deposition process comprises performing the steps in the following order:
A) providing the pulse of the transition metal precursor to the reaction chamber;
B) providing the pulse of the silicon precursor to the reaction chamber; and
C) providing the catalyst to the reaction chamber.

### Claim 3 (depends on 1)

The method of claim 1, wherein the silicon precursor comprises one or more of a silane or a halogen-substituted silane.

### Claim 4 (depends on 1)

The method of claim 1, wherein the transition metal precursor comprises one or more transition metals selected from the group consisting of Nb, Ti, Mo, Hf, Pd, Mo, Ni, V, Cr, Zr, and/or Pt.

### Claim 5 (depends on 1)

The method of claim 1, wherein the catalyst comprises one or more group 13 elements and/or one or more of La, Mg, Sc, or Y.

### Claim 6 (depends on 1)

The method of claim 1, further comprising a degas step prior to the step of forming the transition metal silicide layer.

### Claim 7 (depends on 1)

The method of claim 1, further comprising a clean step prior to the step of forming the transition metal silicide layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the clean step comprises providing activated species formed using a fluorine-containing gas and activated species formed using a hydrogen-containing gas to the reaction chamber.

### Claim 9 (depends on 7)

The method of claim 7, wherein the clean step is performed within a first process module of a reactor system and the forming a transition metal silicide layer step is performed within a second module of the reactor system.

### Claim 10 (depends on 1)

The method of claim 1, further comprising depositing a metal layer overlying the transition metal silicide layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the metal layer comprises a transition metal layer or a transition metal nitride layer.

### Claim 12 (depends on 10)

The method of claim 10, wherein the metal layer comprises molybdenum, titanium nitride, or titanium.

### Claim 13 (depends on 1)

The method of claim 1, wherein the structure comprises an NMOS structure.

### Claim 14 (depends on 1)

The method of claim 1, wherein the substrate comprises a gap, and wherein the transition metal silicide layer is formed within the gap.

### Claim 15 (depends on 1)

The method of claim 1, wherein the semiconductor surface comprises one or more of Si:P or SiGe:B.

### Claim 16 (depends on 1)

The method of claim 1, wherein providing the catalyst comprises a soak process.

### Claim 17 (depends on 16)

The method of claim 16, wherein a flowrate of gas from the reaction chamber to a vacuum source during the soak period is less than a flowrate of gas from the reaction chamber to the vacuum source during forming a transition metal silicide layer step.

### Claim 18 (depends on 1)

The method of claim 1, wherein a temperature of a substrate support during forming a transition metal silicide layer is greater than 400 °C.

### Claim 19

A method of forming a structure, the method comprising:
providing a substrate, comprising a semiconductor surface, within a reaction chamber of a reactor;
performing a plasma treatment; and
forming a transition metal silicide layer on the semiconductor surface using a cyclical deposition process, the cyclical deposition process comprising the steps of:
providing a pulse of a transition metal precursor to the reaction chamber;
providing a pulse of a silicon precursor to the reaction chamber; and
optionally providing a catalyst to the reaction chamber.

### Claim 20 (depends on 1)

A system comprising:
a cleaning module;
a deposition module; and
a controller configured to:
cause the system to move a substrate from the clean module to the deposition module; and
perform the method of claim 1 within the deposition module.