# US 2026/0218343 A1 · Non-oriented electrical steel sheet and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0218343 A1
- Document ID: US20260218343A1
- Status: Published application
- Kind: A1
- Application number: 19/130,039
- Filed: 2023-12-13
- Published: 2026-07-30
- Earliest claimed: 2022-12-21
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Se-Il Lee
- Web page: https://patentgrep.com/patent/US20260218343A1

## CPC

- C22C 38/02: containing silicon
- C21D 1/26: Methods of annealing
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/008: {containing Si}
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/008: {containing tin}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/18: containing chromium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The present invention relates to a non-oriented electrical steel sheet and a manufacturing method therefor. An aspect of the present invention is to provide: a non-oriented electrical steel sheet in which an iron loss in a direction perpendicular to a rolling direction at high frequency is less than that in the rolling direction; and a manufacturing method therefor.

## Claims

### Claim 1

A non-oriented electrical steel sheet, comprising:
by weight %, Si: 1.5 to 6.5%, Al: 0.0005 to 3.5%, Mn: 0.01 to 3.0%, Cr: 0.005 to 5.0%, S: 0.0005 to 0.03%, and a balance of Fe and inevitable impurities,
wherein a Goss orientation fraction in a region from a surface to 1/10t (t: thickness of the steel sheet) in a thickness direction is 3 area % or less, and
wherein a Goss orientation fraction in an entire region in the thickness direction is 5 area % or less.

### Claim 2 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet further includes one or more of P: 0.005 to 0.08% and Sn: 0.01 to 0.2%.

### Claim 3 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet further includes one or more of C: 0.005% or less (excluding 0%), N: 0.005% or less (excluding 0%), O: 0.005% or less (excluding 0%) and Ti: 0.01% or less (excluding 0%).

### Claim 4 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet further includes one or more of Mo: 0.1% or less (excluding 0%), B: 0.0050% or less (excluding 0%), V: 0.050% or less (excluding 0%), Ca: 0.010% or less (excluding 0%), Nb: 0.0050% or less (excluding 0%) and Mg: 0.0050% or less (excluding 0%).

### Claim 5 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet further includes one or more of Sb: 0.1% or less (excluding 0%), Ni: 0.05% or less (excluding 0%), Cu: 0.005 to 0.2% and Zn: 0.01% or less (excluding 0%).

### Claim 6 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet further includes 0.20% or less (excluding 0%) of one or more of Bi, Pb, Ge and As individually or in combination.

### Claim 7 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet has an iron loss (W10/600C) of 28 W/kg or lower, an iron loss (W10/800C) of 43 W/kg or lower, and an iron loss (W10/1200C) of 75 W/kg or lower.

### Claim 8 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet has an iron loss (W10/600L) of 30 W/kg or lower, an iron loss (W10/800L) of 48 W/kg or lower, and an iron loss (W10/1200L) of 85 W/kg or lower.

### Claim 9 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet has an iron loss (W15/600C) of 65 W/kg or lower, an iron loss (W15/800C) of 95 W/kg or lower, and an iron loss (W15/1200C) of 175 W/kg or lower.

### Claim 10 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet has an iron loss (W15/600L) of 75 W/kg or lower, an iron loss (W15/800L) of 105 W/kg or lower, and an iron loss (W15/1200L) of 190 W/kg or lower.

### Claim 11 (depends on 1)

The non-oriented electrical steel sheet of claim 1, wherein the non-oriented electrical steel sheet satisfies relational expression 1 as below:
iron loss (W10/600C)+iron loss (W10/800C)+iron loss (W10/1200C)<iron loss (W10/600L)+iron loss (W10/800L)+iron loss (W10/1200L). [Relational expression 1]

### Claim 12

A method of manufacturing a non-oriented electrical steel sheet, the method comprising:
heating a slab including, by weight %, Si: 1.5 to 6.5%, Al: 0.0005 to 3.5%, Mn: 0.01 to 3.0%, Cr: 0.005 to 5.0%, S: 0.0005 to 0.03%, and a balance of Fe and inevitable impurities at 1050 to 1220° C.;
finishing hot-rolling the slab and obtaining a hot-rolled sheet;
hot-rolled sheet annealing the hot-rolled sheet for 30 to 300 seconds at 850 to 1150° C.;
cold-rolling the hot-rolled sheet annealed hot-rolled sheet and obtaining a cold-rolled sheet;
heating the cold-rolled sheet; and
final annealing the heated cold-rolled sheet,
wherein, in the cold-rolling, [Relational expression 2] is satisfied,
wherein, in the heating, a heating rate in a temperature range of 300 to 500° C. is 5 to 150° C./s, and
wherein, in the final annealing, a gas atmosphere includes, by volume %, hydrogen: 15 to 99.99%, oxygen: 0.0001 to 0.0030%, and a remainder of inert gas.

### Claim at position 13

13-17. (canceled)

### Claim 18 (depends on 12)

The method of claim 12, wherein the finishing hot-rolling is performed at 700 to 1050° C.

### Claim 19 (depends on 12)

The method of claim 12, wherein the cold-rolling is performed with a cold reduction ratio of 35 to 98%.

### Claim 20 (depends on 12)

The method of claim 12, wherein, in the cold rolling, a maximum rolling rate in one or more of first pass and second pass is 3 m/s or higher.

### Claim 21 (depends on 12)

The method of claim 12, wherein the final annealing is performed for 10 to 500 seconds at 600 to 1150° C.