# US 2026/0216932 A1 · Molding Material, Method For Producing Molding Material, Molded Article, And Method For Producing Molded Article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0216932 A1
- Document ID: US20260216932A1
- Status: Published application
- Kind: A1
- Application number: 19/462,277
- Filed: 2026-01-28
- Published: 2026-07-30
- Earliest claimed: 2025-01-29
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Masaaki AOTA; Tomohiro FUJITA
- Web page: https://patentgrep.com/patent/US20260216932A1

## CPC

- B29C 45/0001: {characterised by the choice of material}
- B29B 7/82: Heating or cooling
- B29C 45/0005: {using fibre reinforcements}
- B29C 45/0013: {using fillers dispersed in the moulding material, e.g. metal particles}
- B29K 2021/003: {Thermoplastic elastomers}
- B29K 2105/251: {Particles, powder or granules (expandable particles B29K2105/046)}
- B29K 2201/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as reinforcement
- B29K 2475/00: Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof,} as filler
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The molding material of the present disclosure contains organic fibers that do not melt at 200° C., a thermoplastic resin that melts at 200° C. or lower, and thermosetting polyurethane particles. The content of the thermosetting polyurethane particles in the molding material is preferably 10.0% by mass or more and 40.0% by mass or less. The content of the thermoplastic resin in the molding material is preferably 20.0% by mass or more and 75.0% by mass or less.

## Claims

### Claim 1

A molding material comprising:
organic fibers that do not melt at 200°C;
a thermoplastic resin that melts at 200°C or lower; and
thermosetting polyurethane particles.

### Claim 2 (depends on 1)

The molding material according to claim 1, wherein a content of the thermosetting polyurethane particles is 10.0% by mass or more and 40.0% by mass or less.

### Claim 3 (depends on 1)

The molding material according to claim 1, wherein a content of the thermoplastic resin is 20.0% by mass or more and 75.0% by mass or less.

### Claim 4 (depends on 1)

The molding material according to claim 1, wherein a content of the organic fibers is 10.0% by mass or more and 55.0% by mass or less.

### Claim 5 (depends on 1)

The molding material according to claim 1, wherein an average particle size of the thermosetting polyurethane particles is 2.0 mm or less.

### Claim 6 (depends on 1)

The molding material according to claim 1, wherein the organic fibers are at least one kind selected from the group consisting of cellulose fibers and fibers made of a thermoplastic resin.

### Claim 7 (depends on 1)

The molding material according to claim 1, wherein the organic fibers are a defibrated product of a fabric.

### Claim 8

A method for producing a molding material, the method comprising a heating and kneading step of kneading organic fibers that do not melt at 200°C, a thermoplastic resin that melts at 200°C or lower, and thermosetting polyurethane particles while heating such that the thermoplastic resin melts and the thermosetting polyurethane particles do not melt.

### Claim 9 (depends on 8)

The method for producing a molding material according to claim 8, wherein a heating temperature in the heating and kneading step is 150° C. or higher and 200° C. or lower.

### Claim 10 (depends on 1)

A molded article comprising the molding material according to claim 1.

### Claim 11 (depends on 1)

A method for producing a molded article, the method comprising a molding step of molding the molding material according to claim 1 while heating to a temperature at which the thermoplastic resin melts and the thermosetting polyurethane particles do not melt.

### Claim 12 (depends on 11)

The method for producing a molded article according to claim 11, wherein a heating temperature in the molding step is 160° C. or higher and 200° C. or lower.

### Claim 13

A method for producing a molded article, the method comprising:
a heating and kneading step of kneading organic fibers that do not melt at 200°C, a thermoplastic resin that melts at 200°C or lower, and thermosetting polyurethane particles while heating such that the thermoplastic resin melts and the thermosetting polyurethane particles do not melt to obtain a molding material containing the organic fibers, the thermoplastic resin, and the thermosetting polyurethane particles; and
a molding step of molding the molding material while heating to a temperature at which the thermoplastic resin melts and the thermosetting polyurethane particles do not melt, wherein
a content of the thermosetting polyurethane particles in the molding material is 10.0% by mass or more and 40.0% by mass or less,
a content of the thermoplastic resin in the molding material is 20.0% by mass or more and 75.0% by mass or less,
a content of the organic fibers in the molding material is 10.0% by mass or more and 55.0% by mass or less,
the organic fibers are at least one kind selected from the group consisting of cellulose fibers and fibers made of a thermoplastic resin,
the organic fibers are a defibrated product of a fabric,
a heating temperature in the heating and kneading step is 150° C. or higher and 200° C. or lower, and
a heating temperature in the molding step is 160° C. or higher and 200° C. or lower.