# US 2026/0215176 A1 · Method of manufacturing epitaxial substrate and epitaxial substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0215176 A1
- Document ID: US20260215176A1
- Status: Published application
- Kind: A1
- Application number: 19/142,596
- Filed: 2023-12-01
- Published: 2026-07-23
- Earliest claimed: 2022-12-28
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Applicants: Shin-Etsu Handotai Co., Ltd.
- Inventors: Kazunori HAGIMOTO; Keitaro TSUCHIYA; Ippei KUBONO
- Web page: https://patentgrep.com/patent/US20260215176A1

## CPC

- H10P 14/3216: {Nitrides}
- C30B 23/025: {characterised by the substrate}
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 29/403: {AIII-nitrides}
- C30B 29/68: Crystals with laminate structure, e.g. "superlattices"
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/29: {characterised by the substrates}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2924: {Structures}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3238: {being insulating materials}
- H10P 14/3416: {Nitrides}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 90/00: Preparation of wafers not covered by a single main group of this subclass, e.g. wafer reinforcement
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A method of manufacturing an epitaxial substrate, wherein: a single-crystal Si substrate with a thickness equal to or greater than 1,500 μm is used, resistivity of the substrate and a ratio “a” (thickness of substrate/thickness of a group-III nitride epitaxial layer) are parameters, an epitaxial growth of the epitaxial layer on the substrate and measurement about a warp of the obtained epitaxial substrate are performed while parameters are changed, and correlation between ratio “a” and the warp is obtained for each value of resistivity; manufacturing parameters with which an absolute value of the warp becomes equal to or smaller than 50 μm are determined based on the correlation; and the epitaxial layer is caused to grow on the substrate using the determined parameters. Accordingly, an epitaxial substrate wherein withstand voltage characteristics are high and |warp|≤50 μm is achieved and a method of manufacturing such a substrate are provided.

## Claims

### Claim 1

A method of manufacturing an epitaxial substrate including a single-crystal Si substrate and a group-III nitride epitaxial layer on the single-crystal Si substrate, the method comprising:
a correlation acquisition step in which a single-crystal Si substrate with a thickness equal to or greater than 1,500 μm is used, resistivity of the single-crystal Si substrate and a ratio “a” between a thickness of the single-crystal Si substrate and a thickness of the group-III nitride epitaxial layer (the thickness of the single-crystal Si substrate/the thickness of the group-III nitride epitaxial layer) are set as parameters, an epitaxial growth of the group-III nitride epitaxial layer on the single-crystal Si substrate and measurement about a warp of the obtained epitaxial substrate are performed while the parameters are changed, and a correlation between the ratio “a” and the warp of the epitaxial substrate is obtained for each value of the resistivity of the single-crystal Si substrate;
a manufacturing parameter determination step of determining the resistivity of the single-crystal Si substrate and the ratio “a”, with which an absolute value of the warp of the epitaxial substrate becomes equal to or smaller than 50 μm based on the correlation; and
an epitaxial substrate manufacturing step of epitaxially growing the group-III nitride epitaxial layer on the single-crystal Si substrate by using the determined manufacturing parameters.

### Claim 2

An epitaxial substrate including a single-crystal Si substrate and a group-III nitride epitaxial layer on the single-crystal Si substrate, the epitaxial substrate having a diameter equal to or shorter than 150 mm, wherein
a thickness of the single-crystal Si substrate is equal to or greater than 1,500 μm, a thickness of the group-III nitride epitaxial layer is thicker than 7 μm, and
when a ratio between the thickness of the single-crystal Si substrate and the thickness of the group-III nitride epitaxial layer (the thickness of the single-crystal Si substrate/the thickness of the group-III nitride epitaxial layer) is set as “a”, at least one of the following (A) to (C) is satisfied:
(A) resistivity of the single-crystal Si substrate is equal to or lower than 2 mΩcm and the ratio “a” is equal to or higher than 125;
(B) resistivity of the single-crystal Si substrate is equal to or lower than 3 mΩcm and the ratio “a” is equal to or higher than 135; and
(C) resistivity of the single-crystal Si substrate is equal to or lower than 5 mΩcm and the ratio “a” is equal to or higher than 137.

### Claim 3 (depends on 2)

The epitaxial substrate according to claim 2, wherein
the single-crystal Si substrate is a single-crystal Si substrate with an oxygen concentration of 11 to 18 ppma (JEIDA).