# US 2026/0213158 A1 · Composite material for electrodes, electricity storage device, and method of manufacturing composite material for electrodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0213158 A1
- Document ID: US20260213158A1
- Status: Published application
- Kind: A1
- Application number: 19/158,153
- Filed: 2023-11-07
- Published: 2026-07-23
- Earliest claimed: 2023-03-01
- Assignees: Tohoku University
- Applicants: Tohoku University
- Inventors: Yuta NAKAYASU; Masaru WATANABE; Shu SOKABE
- Web page: https://patentgrep.com/patent/US20260213158A1

## CPC

- H01M 4/137: Electrodes based on electro-active polymers
- H01G 11/30: characterised by their material
- H01G 11/42: Powders or particles, e.g. composition thereof
- H01M 4/1399: of electrodes based on electro-active polymers
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/60: of organic compounds
- H01M 4/608: {containing heterocyclic rings}
- H01M 4/625: {Carbon or graphite}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A composite material for electrodes and an electricity storage device having a large support amount of an organic active material, and a method of manufacturing a composite material for electrodes capable of increasing support amount of organic active material. The composite material for electrodes has a porous carbon material and an organic active material supported within pores of porous carbon material. The organic active material is included in 28 wt % or more relative to total weight of porous carbon and organic active material. A porous carbon and an organic active material are maintained for a predetermined time in supercritical carbon dioxide between 70° C. to 170° C. and 20 MPa to 30 MPa, or between 90° C. to 170° C. and 13 MPa to 20 MPa impregnate organic active material within pores of porous carbon material, thereby manufacturing a composite material for electrodes having organic active material supported within pores of porous carbon material.

## Claims

### Claim 1

A composite material for electrodes, comprising:
a porous carbon material, and
an organic active material supported within pores of the porous carbon material,
wherein the organic active material is included in an amount of 28 wt % or more relative to the total weight of the porous carbon material and the organic active material.

### Claim 2 (depends on 1)

The composite material for electrodes according to claim 1, wherein the organic active material is included in an amount of 35 wt % or more relative to the total weight of the porous carbon material and the organic active material.

### Claim 3 (depends on 1)

The composite material for electrodes according to claim 1, wherein the organic active material is supported within the pores so as to occupy 70% or more of pore volume with a diameter of 1 to 1.5 nm among the pores of the porous carbon material.

### Claim 4 (depends on 1)

The composite material for electrodes according to claim 1, wherein the organic active material is supported within the pores so as to occupy 80% or more of the pore volume with a diameter of 1 to 1.5 nm among the pores of the porous carbon material.

### Claim 5 (depends on 3)

The composite material for electrodes according to claim 3, wherein the organic active material is supported within the pores so as to occupy 60% or more of the pore volume with a diameter of less than 1 nm among the pores of the porous carbon material.

### Claim 6 (depends on 3)

The composite material for electrodes according to claim 3, wherein the organic active material is supported within the pores so as to occupy 80% or more of the pore volume with a diameter of less than 1 nm among the pores of the porous carbon material.

### Claim 7 (depends on 1)

The composite material for electrodes according to claim 1, wherein the organic active material comprises a quinone compound, croconic acid, or metal phthalocyanine.

### Claim 8 (depends on 1)

The composite material for electrodes according to claim 1, wherein the porous carbon material consists of activated charcoal.

### Claim 9 (depends on 1)

An electricity storage device, having an electrode material comprising the composite material for electrodes according to claim 1.

### Claim 10

A method of manufacturing a composite material for electrodes, the method comprising: maintaining a porous carbon material and an organic active material for a predetermined time in supercritical carbon dioxide at 70° C. or more to 170° C. or less and 10 MPa or more to 30 MPa or less, or 90° C. or more to 170° C. or less and 10 MPa or more to 20 MPa or less to impregnate the organic active material within pores of the porous carbon material, thereby manufacturing the composite material for electrodes having the organic active material supported within the pores of the porous carbon material.

### Claim 11 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the composite material for electrodes for use as positive electrodes is manufactured using the supercritical carbon dioxide at 70° C. or more to 90° C. or less and 10 MPa or more to 30 MPa or less, or 90° C. or more to 130° C. or less and 10 MPa or more to 20 MPa or less.

### Claim 12 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the composite material for electrodes for use as negative electrodes is manufactured using the supercritical carbon dioxide at 130° C. or more to 170° C. or less and 10 MPa or more to 30 MPa or less.

### Claim 13 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the predetermined time is 3 hours or more.

### Claim 14 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the predetermined time is 20 hours or more.

### Claim 15 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein a polar solvent as an entrainer is added to the supercritical carbon dioxide and maintained for the predetermined time, thereby manufacturing the composite material for electrodes.

### Claim 16 (depends on 12)

The method of manufacturing a composite material for electrodes according to claim 12, wherein the predetermined time is 60 hours or more, and the composite material for electrodes for use as negative electrodes is manufactured.

### Claim 17 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the organic active material comprises a quinone compound, croconic acid, or metal phthalocyanine.

### Claim 18 (depends on 10)

The method of manufacturing a composite material for electrodes according to claim 10, wherein the porous carbon material consists of activated charcoal.